arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2304.08002cond-mat.mtrl-sci
收藏

离子辅助磁控溅射沉积含11B4C的Ni/Ti多层膜中子光学器件中埋藏界面形貌的掠入射小角散射研究

Morphology of buried interfaces in ion-assisted magnetron sputter deposited 11B4C-containing Ni/Ti multilayer neutron optics investigated by grazing incidence small angle scattering

Sjoerd Broekhuijsen, Naureen Ghafoor, Matthias Schwartzkopf, Anton Zubayer, Jens Birch, Fredrik Eriksson

AI总结:

本研究通过掠入射小角散射发现,添加26.0 at.% 11B4C并结合高通量调制离子辅助可显著改善Ni/Ti多层膜界面形貌,使平均界面宽度降至2.7 Å,优于商用器件。

摘要:

多层膜中子光学器件需要精确控制界面形貌以实现最佳性能。在本工作中,我们研究了不同生长条件对Ni/Ti基多层膜界面形貌的影响,重点在于掺入低中子吸收的11B4C以及采用不同的离子辅助方案。利用掠入射小角X射线散射探测埋藏界面的结构和形貌细节,结果表明,随着11B4C含量的增加,层间相关性增强,界面形成丘状结构。在生长过程中施加高通量离子辅助可以减少丘状形成,但会导致界面混合,而采用高通量调制离子辅助方案,即初始缓冲层在低离子能量下生长、顶层在较高离子能量下生长,则可以防止混合。最佳条件为添加26.0 at.%的11B4C并结合高通量调制离子辅助。在此条件下生长了周期为48.2 Å、共100周期的多层膜,对中子反射率和X射线反射率数据的联合拟合显示,平均界面宽度仅为2.7 Å,较当前最先进的商用Ni/Ti多层膜有显著改善。总体而言,我们的研究表明,在生长过程中添加11B4C并采用高通量调制离子辅助可以显著改善Ni/Ti多层膜的界面形貌,从而提升中子光学器件的性能。

英文摘要:

Multilayer neutron optics require precise control of interface morphology for optimal performance. In this work, we investigate the effects of different growth conditions on the interface morphology of Ni/Ti based multilayers, with a focus on incorporating low-neutron-absorbing 11B4C and using different ion assistance schemes. Grazing incidence small angle X-ray scattering was used to probe the structural and morphological details of buried interfaces, revealing that the layers become more strongly correlated and the interfaces form mounds with increasing amounts of 11B4C. Applying high flux ion assistance during growth can reduce mound formation but lead to interface mixing, while a high flux modulated ion assistance scheme with an initial buffer layer grown at low ion energy and the top layer at higher ion energy prevents intermixing. The optimal condition was found to be adding 26.0 at.% 11B4C combined with high flux modulated ion assistance. A multilayer with a period of 48.2 Å and 100 periods was grown under these conditions, and coupled fitting to neutron and X-ray reflectivity data revealed an average interface width of only 2.7 Å, a significant improvement over the current state-of-the-art commercial Ni/Ti multilayers. Overall, our study demonstrates that the addition of 11B4C and the use of high flux modulated ion assistance during growth can significantly improve the interface morphology of Ni/Ti multilayers, leading to improved neutron optics performance.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑