arXiv 1909.07197cond-mat.mtrl-sci
收藏

氪/三甲基硼气氛下反应磁控溅射钨靶

Reactive magnetron sputtering of tungsten target in krypton/trimethylboron atmosphere

Martin Magnuson, Lina Tengdelius, Fredrik Eriksson, Mattias Samuelsson, Esteban Broitman, Grzegorz Greczynski, Lars Hultman, Hans Högberg

摘要:

采用Kr/TMB等离子体反应溅射法在Si(100)基片上沉积了W-B-C薄膜。X射线光电子能谱学(XPS)定量分析表明,薄膜中W含量在~ 73 ~~ 93 at.%之间W.在用1 sccm TMB沉积的膜中检测到最高的金属含量。C和B浓度随着TMB流量的增加而增加,最大值为~18和~7原子%,而O含量几乎保持恒定在2- 3at.%。样品清洗后进行的化学键合结构分析显示C-W和B-W键合,没有检测到W-O键。在用5 sccm TMB和500 oC或用10 sccm TMB和300-600 oC薄膜生长薄膜期间,X射线衍射显示形成立方100取向的WC 1-x,其中可能存在B的固溶体。较低的流量和较低的生长温度分别有利于W和W2 C的生长。在700和800 oC的沉积导致由于与衬底反应而形成WSi 2。在900 oC时,XPS分析显示~96 at.%由于Si相互扩散,薄膜中的Si。扫描电子显微镜图像显示沉积的WC 1-x薄膜的细晶粒显微结构。纳米压痕给出的硬度值范围从~23到~31 GPa,在低于600 oC的温度下沉积的薄膜的弹性模量在~220到280 GPa之间。在较高的生长温度下,硬度降低3至4倍,在700-800 oC时形成WSi 2,在900 oC时形成富Si表面。

英文摘要:

W-B-C films were deposited on Si(100) substrates held at elevated temperature by reactive sputtering from a W target in Kr/trimethylboron (TMB) plasmas. Quantitative analysis by X-ray photoelectron spectroscopy (XPS) shows that the films are W-rich between ~ 73 and ~ 93 at.% W. The highest metal content is detected in the film deposited with 1 sccm TMB. The C and B concentrations increase with increasing TMB flow to a maximum of ~18 and ~7 at.%, respectively, while the O content remains nearly constant at 2-3 at.%. Chemical bonding structure analysis performed after samples sputter-cleaning reveals C-W and B-W bonding and no detectable W-O bonds. During film growth with 5 sccm TMB and 500 oC or with 10 sccm TMB and 300-600 oC thin film X-ray diffraction shows the formation of cubic 100-oriented WC1-x with a possible solid solution of B. Lower flows and lower growth temperatures favor growth of W and W2C, respectively. Depositions at 700 and 800 oC result in the formation of WSi2 due to a reaction with the substrate. At 900 oC, XPS analysis shows ~96 at.% Si in the film due to Si interdiffusion. Scanning electron microscopy images reveal a fine-grained microstructure for the deposited WC1-x films. Nanoindentation gives hardness values in the range from ~23 to ~31 GPa and reduced elastic moduli between ~220 and 280 GPa in the films deposited at temperatures lower than 600 oC. At higher growth temperatures the hardness decreases by a factor of 3 to 4 following the formation of WSi2 at 700-800 oC and Si-rich surface at 900 oC.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑