可控生长的氧化钇氢化物薄膜的光致变色性:通过HiPIMS和脉冲-直流磁溅射制备

Growth-controlled photochromism in yttrium oxyhydride thin films deposited by HiPIMS and pulsed-DC magnetron sputtering

University of Latvia(拉脱维亚大学);University of Helsinki(赫尔辛基大学);KTH Royal Institute of Technology(皇家理工学院)

M. Zubkins, E. Letko, E. Strods, V. Vibornijs, D. Moldarev, K. Sarakinos, K. Mizohata, K. Kundzins, J. Purans

AI总结:

本研究通过HiPIMS和脉冲-直流MS制备氧化钇氢化物薄膜,发现生长条件和微结构对光致变色性能有显著影响,脉冲-直流MS薄膜在光致变色对比度和带隙方面表现更优。

摘要:

本研究调查了通过反应性高功率脉冲磁溅射(HiPIMS)制备的含氧钇氢化物(YHO)薄膜的光致变色性,并将其光致变色、光学和结构特性与通过反应性脉冲直流磁溅射(脉冲-直流MS)制备的薄膜进行比较。光学发射光谱显示,与脉冲-直流MS中占主导的Ar+离子不同,HiPIMS放电以强烈的Y+发射为特征,表明高钇离子化和显著的自溅射回收。获得透明且光致变色薄膜所需的关键工作压力(Pc)对于HiPIMS(Pc≈1.0 Pa)比脉冲-直流MS(Pc≈0.5 Pa)更高。尽管在Pc附近沉积的薄膜表现出相似的太阳透射率(约72%)和晶格参数(5.38-5.39 Å),但脉冲-直流MS薄膜的相对光致变色对比度(34%)明显更高,而光学带隙(2.70 eV)比HiPIMS薄膜(9%对比度和2.94 eV)更低。这种差异部分归因于脉冲-直流MS薄膜中氧与氢原子比较低。在结构上,HiPIMS薄膜大多为多晶,具有随机的平面晶体学取向,而脉冲-直流MS薄膜表现出显著的<100>平面优先取向。这些结果表明,除了组成外,薄膜生长条件和微结构在决定YHO的光致变色性能方面起着关键作用。

英文摘要:

The present study investigates photochromic oxygen-containing yttrium hydride (YHO) thin films deposited by reactive high power impulse magnetron sputtering (HiPIMS) and compares their photochromic, optical, and structural properties with those of films synthesized by reactive pulsed direct current magnetron sputtering (pulsed-DCMS). Optical emission spectroscopy reveals that, unlike pulsed-DCMS where Ar$^{+}$ ions dominate, HiPIMS discharges are characterised by strong Y$^{+}$ emission, evidencing high yttrium ionisation and substantial self-sputter recycling. The critical working pressure (P$_c$) required to obtain transparent and photochromic films is higher for HiPIMS (Pc $\approx$ 1.0 Pa) than for pulsed-DCMS (Pc $\approx$ 0.5 Pa). Although films deposited near Pc exhibit similar solar transmittance (~72 %) and lattice parameters (5.38--5.39 Å), the pulsed-DCMS film shows a substantially higher relative photochromic contrast (34 %) and a lower optical band gap (2.70 eV) compared with the HiPIMS film (9 % contrast and 2.94 eV). This difference is partly attributed to a lower oxygen-to-hydrogen atomic ratio in the pulsed-DCMS film. Structurally, HiPIMS films are largely polycrystalline with random out-of-plane crystallographic orientation, whereas pulsed-DCMS films exhibit a pronounced <100> out-of-plane preferred orientation. These results demonstrate that, beyond composition, thin-film growth conditions and microstructure play a crucial role in governing the photochromic performance of YHO.