热还原对氧化石墨烯低温吸附~4He动力学及结构特征的影响

The effect of the thermal reduction on the kinetics of low temperature 4He sorption and the structural characteristics of graphene oxide

A. V. Dolbin, M. V. Khlistuck, V. B. Esel'son, V. G. Gavrilko, N. A. Vinnikov, R. M. Basnukaeva, A. I. Prokhvatilov, I. V. Legchenkova, V. V. Meleshko, W. K. Maser, A. M. Benito

摘要:

在1.5 - 20 K的温度区间内,研究了起始氧化石墨(GtO)和热还原氧化石墨烯样品(TRGO,Treduction = 200、300、500、700和900 C)对4He的吸附和随后的解吸的动力学。通过X射线衍射(XRD)技术研究了退火温度对样品结构特征的影响。当温度从20 K降低到11 - 12 K时,所有样品的4He吸附时间都增加,这是典型的热激活扩散条件下观察到的。低于5 K的4He吸附的GtO和TRGO-200样品的特征时间仅弱依赖于温度,这表明隧道机制的主导地位。在相同的区域(T <5 K)中,在较高温度(300、500、700和900 C)下还原的TRO的特征时间随着温度降低而增长,推测是由于在去除氧官能团(oFG)时在碳平面中产生的缺陷。4He扩散的活化能(Ea)的估计表明,在TRGO-200样品中,Ea值比母体GtO低2.9倍,这是由于插入在碳的层间空间中的水的蒸发导致的GtO剥离所致。在200 ℃以上处理的GtO样品的非单调依赖性Ea与T由两个过程之间的竞争确定-石墨碳结构的恢复,这增加了活化能,以及缺陷的产生,这通过打开额外的表面积和吸附方式来降低活化能。活化能对处理温度的依赖关系与GtO中的晶相含量随退火温度的升高而变化密切相关。

英文摘要:

The kinetics of the sorption and the subsequent desorption of 4He by the starting graphite oxide (GtO) and the thermally reduced graphene oxide samples (TRGO, Treduction = 200, 300, 500, 700 and 900 C) have been investigated in the temperature interval 1.5 - 20 K. The effect of the annealing temperature on the structural characteristics of the samples was examined by the X-ray diffraction (XRD) technique. On lowering the temperature from 20 K to 11-12 K, the time of 4He sorption increased for all the samples, which is typically observed under the condition of thermally activated diffusion. Below 5 K the characteristic times of 4He sorption by the GtO and TRGO-200 samples were only weakly dependent on temperature, suggesting the dominance of the tunnel mechanism. In the same region (T<5 K) the characteristic times of the TRGOs reduced at higher temperatures (300, 500, 700 and 900 C) were growing with lowering temperature, presumably due to the defects generated in the carbon planes on removing the oxygen functional groups (oFGs). The estimates of the activation energy (Ea) of 4He diffusion show that in the TRGO-200 sample the Ea value is 2.9 times lower as compared to the parent GtO, which is accounted for by GtO exfoliation due to evaporation of the water intercalated in the interlayer space of carbon. The nonmonotonic dependences Ea vs T for the GtO samples treated above 200 C are determined by a competition between two processes - the recovery of the graphite carbon structure, which increases the activation energy, and the generation of defects, which decreases the activation energy by opening additional surface areas and ways for sorption. The dependence of the activation energy on treatment temperature correlates well with the contents of the crystalline phase in GtO varying with a rise of the annealing temperature.