arXiv 1301.3030cond-mat.mtrl-sci
收藏

Ge(Bi,Sb)_4Te_7单晶生长及热电性能研究

Single-Crystal Growth and Thermoelectric Properties of Ge(Bi,Sb)4Te7

Fabian von Rohr, Andreas Schilling, Robert J. Cava

摘要:

本文报道了10 ~ 300 K温度范围内的热电性能以及n型和p型GeBi_4 Te_7、GeSb_4 Te_7和Ge(Bi_(1-x)Sb_x)_4 Te_7固溶体单晶的生长。采用改进的Bridgman法生长了GeBi 4 Te 7单晶,并通过Sb替代Bi实现了p型行为。Ge(Bi 1-xSbx)4 Te 7固溶体的热电势范围为-117 muVK^-1至+160 muVK^-1。随着Sb含量的增加,从n型到p型的交叉是连续的,并且在x = 0.15处观察到。在所测试的n型和p型样品中,最高的热电效率分别为ZnT = 0.11和ZpT = 0.20。对于该合金系统中的最佳n-p耦合,在室温下的复合优值为ZnpT = 0.17。

英文摘要:

The thermoelectric properties between 10 and 300 K and the growth of single crystals of n-type and p-type GeBi4Te7, GeSb4Te7, and the Ge(Bi1-xSbx)4Te7 solid solution are reported. Single crystals were grown by the modified Bridgman method, and p-type behavior was achieved by the substitution of Bi by Sb in GeBi4Te7. The thermopower in the Ge(Bi1-xSbx)4Te7 solid solution ranges from -117 muVK^-1 to +160 muVK^-1. The crossover from n-type to p-type is continuous with increasing Sb content and is observed at x = 0.15. The highest thermoelectric efficiencies among the tested n-type and p-type samples are ZnT = 0.11 and ZpT = 0.20, respectively. For an optimal n-p couple in this alloy system the composite figure of merit is ZnpT = 0.17 at room temperature.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑