In rechargeable batteries, electron transport properties of inorganics in the solid-electrolyte interphase (SEI) critically determine the safety, lifespan and capacity loss of batteries. However, the electron transport properties of heterogeneous interfaces among different solid inorganics in SEI have not been studied experimentally or theoretically yet, although such heterogeneous interfaces exist inevitably. Here, by employing non-equilibrium Green's function (NEGF) method, we theoretically evaluated the atomic-scale electron transport properties under bias voltage for LiF/Li2O interfaces and single-component layers of them, since LiF and Li2O are common stable inorganics in the SEI. We reveal that heterogeneous interfaces orthogonal to the external electric-field direction greatly impede electron transport in SEI, whereas heterogeneous parallel-orientated interfaces enhance it. Structural disorders induced by densely distributed interfaces can severely interfere with electron transport. For each component, single-crystal LiF is highly effective to block electron transport, with a critical thickness of 2.9 nm, much smaller than that of Li2O (19.0 nm). This study sheds a new light into direct and quantitative understanding of the electron transport properties of heterogeneous interfaces in SEI, which holds promise for the advancement of a new generation of high-performance batteries.
Measuring the buried interphase between solid electrolytes and lithium metal using neutrons
Oak Ridge National Laboratory(橡树岭国家实验室);Brookhaven National Laboratory(布鲁克海文国家实验室);Technical University Munich(慕尼黑工业大学);Czech Academy of Sciences(捷克科学院)
Identification of Solid-Electrolyte Interphase Species by Joint Characterization of Li-ion Battery Chemistry by Mass Spectrometry and Electro-Chemical Reaction Networks
Bakar Institute of Digital Materials for the Planet, University of California at Berkeley(加州大学伯克利分校巴克数字材料星球研究所);Lawrence Berkeley National Laboratory(劳伦斯伯克利国家实验室);Department of Materials Science and Engineering, University of California at Berkeley(加州大学伯克利分校材料科学与工程系);Université de Rouen Normandie, INSA Rouen Normandie, Université de Caen Normandie, ENSICAEN, CNRS, Institut CARMeN UMR 6064(鲁昂诺曼底大学、鲁昂国立应用科学学院、卡昂诺曼底大学、ENSICAEN、法国国家科学研究中心CARMeN联合研究所);TotalEnergies OneTech, TotalEnergies Research & Technology Gonfreville(道达尔能源OneTech、道达尔能源贡夫勒维尔研究与技术部);Saft, Corporate Research(萨博公司企业研究部);International Joint Laboratory-Complex Matrices Molecular Characterization (iC2MC)(国际联合实验室-复杂基体分子表征);TotalEnergies OneTech Belgium(道达尔能源OneTech比利时);TotalEnergies EP Research & Technology(道达尔能源勘探与生产研究与技术部);Universite de Pau et des Pays de l’Adour, CNRS, IPREM(波城与阿杜尔地区大学、法国国家科学研究中心IPREM)
Interfacial Effects on Solid Electrolyte Interphase in Lithium-ion Batteries
界面处钝化层的存在是实现现代锂离子(Li离子)电池的主要因素。它们的特性决定了电池的循环寿命、性能和安全性。一种特殊情况是固体电解质中间相(SEI),一种由于电解质的不稳定性和随后在阳极表面的分解而形成的异质多组分膜。SEI充当阻碍电解质进一步分解的钝化层,这对库仑效率是有害的。在这项工作中,我们使用第一性原理模拟研究氟化锂(LiF)和碳酸锂(Li $_2$ CO $_3$)之间的界面的动力学和电子特性,这两种常见的SEI组件存在于具有有机液体电解质的锂离子电池中。我们发现,这些组件之间的一致的接口,限制在他们每个人的应变低于3%。我们发现,界面引起的弗伦克尔缺陷的形成能量的大幅度增加,产生Li空位的LiF和Li晶体中的Li $_2$ CO $_3$负责运输。另一方面,Li间隙跳跃势垒从体Li $_2$ CO $_3$中的$0.3$ eV降低到所考虑的界面结构中的$0.10$或$0.22$ eV,表明界面的有利作用。在异质SEI中控制这两种效应对于在SEI中保持快速离子传输是至关重要的。我们进一步进行了Car-Parrinello分子动力学模拟,以探讨在我们的界面结构,这揭示了增强的界面附近的锂离子扩散的锂离子传导。了解多相SEI的界面特性是实现下一代电池的重要前沿。
Flexible, solid electrolyte-based lithium battery composed of LiFePO4 cathode and Li4Ti5O10 anode for applications in smart textiles
在这里,我们报告制造的灵活和可拉伸的电池组成的应变自由LiFePO 4阴极,Li 4 Ti 5 O 10阳极和固体聚环氧乙烷(PEO)电解质作为隔膜层。该电池是从智能纺织品应用的角度开发的。该电池以固体热塑性电解质为关键使能元件,可挤压或拉伸成纤维或细条,直接与智能纺织品制造中使用的编织工艺兼容。本文首先详细介绍了材料的选择,电极和隔膜层的制造和表征。然后组装电池并对其进行表征,最后,将由几个长条制成的大型电池样品编织成织物,用导电线连接,并进行表征。在本文中,我们详细研究了电池设计的两个实际方面:第一是以导电碳和聚合物粘合剂材料的优化比例制备阴极/阳极材料的复合材料,第二是电池性能,包括循环,可逆性和阴极/阳极材料的相容性。最后,当铸造电极和隔膜层时,我们主要关注使用水溶液代替有机溶剂,以使制造过程环境友好。
Machine-Learning-Guided Insights into Solid-Electrolyte Interphase Conductivity: Are Amorphous Lithium Fluorophosphates the Key?
Bakar Institute of Digital Materials for the Planet, UC Berkeley(加州大学伯克利分校巴卡尔数字材料行星研究所);Materials Sciences Division, Lawrence Berkeley National Laboratory(劳伦斯伯克利国家实验室材料科学部);Department of Materials Science and Engineering, National University of Singapore(新加坡国立大学材料科学与工程系)
An Ultrathin Laterally Conductive Mesh Interphase Enables Spatially Extended Zinc Deposition for Aqueous Zinc Batteries
University of Chemistry and Technology Prague(布拉格化工大学);Technische Universität Dresden(德累斯顿工业大学);Center for Advancing Electronics Dresden (cfaed)(德累斯顿先进电子中心);Faculty of Chemistry and Food Chemistry, Technische Universität Dresden(德累斯顿工业大学化学与食品化学学院);Max Planck Institute of Microstructure Physics(马克斯·普朗克微观结构物理研究所);Chair of Analytical Chemistry, Faculty of Chemistry and Biochemistry, Ruhr- University Bochum(鲁尔大学波鸿分校化学与生物化学学院分析化学系)
Favorable Interfacial Chemomechanics Enables Stable Cycling of High Li-Content Li-In/Sn Anodes in Sulfide Electrolyte Based Solid-State Batteries
固态电池(SSB)可以在电池安全性和能量密度方面提供范式转变。然而,这一前景取决于将高性能电极与最先进的固体电解质集成的能力。例如,锂(Li)金属,最高能量密度的阳极候选者,遭受导致电池故障的严重界面化学机械问题。In/Sn的Li合金是有吸引力的替代品,但它们的开发主要限于低容量(低Li含量)和富In的Li $_x$ In(x $\leq$ 0.5)。在这里,基本的电化学机械行为的Li-In和Li-Sn合金的不同Li化学计量是解开硫化物电解质为基础的SSB。通过控制合成和制造技术开发的金属间化合物电极显示出令人印象深刻的(电)化学稳定性,其中Li $_6$ PS $_5$ Cl作为固体电解质,并且在电化学Li插入/脱嵌期间在最佳堆叠压力下保持近乎完美的界面接触。通过计算和电化学研究的结合,揭示了它们在锂迁移势垒随组成的有趣变化及其对观察到的锂循环过电位的影响。合金的稳定界面化学力学允许在相对高的电流密度(1 mA cm $^{-2}$)和容量(1 mAh cm $^{-2}$)下的长期无枝晶Li循环(>1000 h),如对于Li $_{13}$ In $_3$和Li $_{17}$ Sn $_4$所证明的,与低Li含量类似物相比,从容量和成本考虑,这是更期望的。这些认识对锂离子电池用高容量Li-In/Sn合金阳极的开发具有指导意义。
Influence of Electrode Thickness and Electrolyte Composition on SEI Formation and Cycle Stability in Binder-Free Hard Carbon Anodes for Na-Ion Batteries
Université de Haute-Alsace(阿尔萨斯大学);Institut de Science des Matériaux de Mulhouse (IS2M)(穆尔豪斯材料科学研究所);CNRS UMR 7361(法国国家科学研究中心联合研究实验室7361);Université de Strasbourg(斯特拉斯堡大学);Réseau sur le Stockage Electrochimique de l’Energie (RS2E)(电化学储能网络);CNRS FR3459(法国国家科学研究中心自由研究基金3459)
本研究探讨了硬碳自支撑电极厚度、大孔率及电解液添加剂对钠离子电池SEI形成和循环稳定性的影响,发现FEC添加剂可改善稳定性,实现高达93%的初始库仑效率和328 mAh g-1的可逆容量。
An Effective Strategy to Enable Argyrodite Sulfides as Superb Solid-State Electrolytes: Safeguarding Remarkable Ionic Conductivity and Interfacial Stability with Electrodes