arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2108.00843cond-mat.mtrl-sciphysics.chem-ph
收藏

良好的界面化学力学使高锂含量Li-In/Sn阳极在基于硫化物电解质的固态电池中稳定循环

Favorable Interfacial Chemomechanics Enables Stable Cycling of High Li-Content Li-In/Sn Anodes in Sulfide Electrolyte Based Solid-State Batteries

Christian Hänsel, Baltej Singh, David Kiwic, Pieremanuele Canepa, Dipan Kundu

摘要:

固态电池(SSB)可以在电池安全性和能量密度方面提供范式转变。然而,这一前景取决于将高性能电极与最先进的固体电解质集成的能力。例如,锂(Li)金属,最高能量密度的阳极候选者,遭受导致电池故障的严重界面化学机械问题。In/Sn的Li合金是有吸引力的替代品,但它们的开发主要限于低容量(低Li含量)和富In的Li $_x$ In(x $\leq$ 0.5)。在这里,基本的电化学机械行为的Li-In和Li-Sn合金的不同Li化学计量是解开硫化物电解质为基础的SSB。通过控制合成和制造技术开发的金属间化合物电极显示出令人印象深刻的(电)化学稳定性,其中Li $_6$ PS $_5$ Cl作为固体电解质,并且在电化学Li插入/脱嵌期间在最佳堆叠压力下保持近乎完美的界面接触。通过计算和电化学研究的结合,揭示了它们在锂迁移势垒随组成的有趣变化及其对观察到的锂循环过电位的影响。合金的稳定界面化学力学允许在相对高的电流密度(1 mA cm $^{-2}$)和容量(1 mAh cm $^{-2}$)下的长期无枝晶Li循环(>1000 h),如对于Li $_{13}$ In $_3$和Li $_{17}$ Sn $_4$所证明的,与低Li含量类似物相比,从容量和成本考虑,这是更期望的。这些认识对锂离子电池用高容量Li-In/Sn合金阳极的开发具有指导意义。

英文摘要:

Solid-state batteries (SSBs) can offer a paradigm shift in battery safety and energy density. Yet, the promise hinges on the ability to integrate high-performance electrodes with state-of-the-art solid electrolytes. For example, lithium (Li) metal, the most energy-dense anode candidate, suffers from severe interfacial chemomechanical issues that lead to cell failure. Li alloys of In/Sn are attractive alternatives, but their exploration has mostly been limited to the low capacity(low Li content)and In rich Li$_x$In (x$\leq$0.5). Here, the fundamental electro-chemo-mechanical behavior of Li-In and Li-Sn alloys of varied Li stoichiometries is unravelled in sulfide electrolyte based SSBs. The intermetallic electrodes developed through a controlled synthesis and fabrication technique display impressive (electro)chemical stability with Li$_6$PS$_5$Cl as the solid electrolyte and maintain nearly perfect interfacial contact during the electrochemical Li insertion/deinsertion under an optimal stack pressure. Their intriguing variation in the Li migration barrier with composition and its influence on the observed Li cycling overpotential is revealed through combined computational and electrochemical studies. Stable interfacial chemomechanics of the alloys allow long-term dendrite free Li cycling (>1000 h) at relatively high current densities (1 mA cm$^{-2}$) and capacities (1 mAh cm$^{-2}$), as demonstrated for Li$_{13}$In$_3$ and Li$_{17}$Sn$_4$, which are more desirable from a capacity and cost consideration compared to the low Li content analogues. The presented understanding can guide the development of high-capacity Li-In/Sn alloy anodes for SSBs.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑