arXiv 1801.09676physics.app-phcond-mat.mtrl-sciphysics.chem-ph
收藏

固体电解质相间过电位的温度依赖性:第一部分。两个并联机构,一个相变

Temperature-Dependence of the Solid-Electrolyte Interphase Overpotential: Part I. Two Parallel Mechanisms, One Phase Transition

Michael Hess

摘要:

最近的研究表明,由碱金属离子通过内部致密固体电解质界面(SEI)的离子传导引起的过电位是强非线性的。提出了一个经验公式,将25 $^{\circ}$ C下恒电流循环(GS)和电化学阻抗谱(EIS)测量的电阻合并。在此,该分析被扩展到从-40 $^{\circ}$ C到+80 $^{\circ}$ C的电池的全温度范围,用于碳酸盐电解质中的Li、Na、K和Rb金属电极。发现了两种不同的输运机制:第一种在所有温度下都是传导碱金属离子的。第二种传输机制传导所有七种测量的Li离子电解质和四种Na离子电解质中的一种的离子,然而,仅高于某一临界温度$T_C$。在$T_C$观察到一个相变关闭更有效的传输机制,只留下一般的离子传导机制。根据碱金属离子、盐和溶剂,相关的过电位在低于$T_C$时迅速增加,并成为所有锂离子电解质在低温下恒电流操作期间的限制因素。通常,电流分析将由EIS测量的范围从最佳Li的26 $Ω$ cm $^2$到Rb电极的292 M $Ω$ cm $^2$的SEI电阻合并到其超过七个数量级的恒电流响应。对于测试的Li,所确定的临界温度在0-25 $^{\circ}$ C之间,对于Na电解质,所确定的临界温度在50 $^{\circ}$ C以上。

英文摘要:

It has been shown recently that the overpotential originating from ionic conduction of alkali-ions through the inner dense solid-electrolyte interphase (SEI) is strongly non-linear. An empirical equation was proposed to merge the measured resistances from both galvanostatic cycling (GS) and electrochemical impedance spectroscopy (EIS) at 25$^{\circ}$C. Here, this analysis is extended to the full temperature range of batteries from -40$^{\circ}$C to +80$^{\circ}$C for Li, Na, K and Rb-metal electrodes in carbonate electrolytes. Two different transport mechanisms are found. The first one conducts alkali-ions at all measured temperatures. The second transport mechanism conducts ions for all seven measured Li-ion electrolytes and one out of four Na-ion electrolytes, however, only above a certain critical temperature $T_C$. At $T_C$ a phase transition is observed switching-off the more efficient transport mechanism and leaving only the general ion conduction mechanism. The associated overpotentials increase rapidly below $T_C$ depending on alkali-ion, salt and solvent and become a limiting factor during galvanostatic operation of all Li-ion electrolytes at low temperature. In general, the current analysis merges the SEI resistances measured by EIS ranging from 26 $Ω$cm$^2$ for the best Li up to 292 M$Ω$cm$^2$ for Rb electrodes to its galvanostatic response over seven orders of magnitude. The determined critical temperatures are between 0-25$^{\circ}$C for the tested Li and above 50$^{\circ}$C for Na electrolytes.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑