Mathematical models of capacity fade can reduce the time and cost of lithium-ion battery development and deployment, and growth of the solid-electrolyte interphase (SEI) is a major source of capacity fade. Experiments in Part I reveal nonlinear voltage dependence and strong charge-discharge asymmetry in SEI growth on carbon black negative electrodes, which is not captured by previous models. Here, we present a theoretical model for the electrochemical kinetics of SEI growth coupled to lithium intercalation, which accurately predicts experimental results with few adjustable parameters. The key hypothesis is that the initial SEI is a mixed ion-electron conductor, and its electronic conductivity varies approximately with the square of the local lithium concentration, consistent with hopping conduction of electrons along percolating networks. By including a lithium-ion concentration dependence for the electronic conductivity in the SEI, the bulk SEI thus modulates the overpotential and exchange current of the electrolyte reduction reaction. As a result, SEI growth is promoted during lithiation but suppressed during delithiation. This new insight establishes the fundamental electrochemistry of SEI growth kinetics. Our model improves upon existing models by introducing the effects of electrochemical SEI growth and its dependence on potential, current magnitude, and current direction in predicting capacity fade.
The role of the electrolysis and enzymatic hydrolysis in the enhancement of the electrochemical properties of 3D-printed carbon black/poly(lactic acid) structures
Efficient Electrocatalytic Reduction of CO2 by Nitrogen-Doped Nanoporous Carbon-Carbon Nanotube Membranes - A Step Towards the Electrochemical CO2 Refinery
Data-Augmented Machine Learning for Predicting Biomass-Derived Hard Carbon Anode Performance in Sodium-Ion Batteries
Shanghai Key Laboratory of Magnetic Resonance, School of Physics and Electronic Science, Institute of Magnetic Resonance and Molecular Imaging in Medicine, East China Normal University(华东师范大学);Siyuan Laboratory, Guangdong Provincial Engineering Technology Research Center of Vacuum Coating Technologies and New Energy Materials, Department of Physics, College of Physics & Optoelectronic Engineering, Jinan University(暨南大学)
Electron Paramagnetic Resonance Study of Radical Species on NaNbO3@CeO2-Modified Carbon Vulcan XC72 Gas Diffusion Electrode for Electrochemical Degradation of Paracetamol via Electro-Fenton
Centro de Ciências Naturais e Humanas, Universidade Federal do ABC(自然与人文科学中心,巴西联邦ABC大学);Centro de Engenharia, Modelagem e Ciências Sociais Aplicadas, Universidade Federal do ABC(工程、建模与应用社会科学中心,巴西联邦ABC大学)
Marcus-Hush-Chidsey Kinetics at Electrode-Electrolyte Interfaces
电极-电解质界面处的电化学动力学限制了包括燃料电池和蓄电池的装置的性能。虽然已经认识到超越Butler-Volmer动力学并将电极的电子态密度的影响纳入其中的重要性,但仍然缺乏将这些方面直接纳入电化学性能模型的统一框架。在这项工作中,我们明确占DFT计算的状态密度数值计算电化学反应速率的各种电极-电解质界面。我们首先示出了这两种情况下的实用程序,与Li金属电沉积和剥离在Li表面和Cu表面(无阳极配置)。反应速率的偏差是轻微的情况下,与平坦的状态密度,如锂,但由于非色散的d-带产生大的变化是显着的铜。最后,我们考虑了由LiF和Li $_2$ CO $_3$组成的固体电解质中间相(SEI)的半导体情况,并注意到界面处的费米能级的重要性,由那里发生的氧化还原反应钉扎。我们确定的不对称性反应速率的函数放电/充电自然在这种方法。本工作中使用的分析代码在Github上是开源的。
Revealing the interfacial kinetic mechanisms in high-entropy doped Na$_3$V$_2$(PO$_4$)$_3$ through electrochemical investigation and distribution of relaxation times
Nanostructuring Strategies for Silicon-based Anodes in Lithium-ion Batteries: Tuning Areal Silicon Loading, SEI Formation/Irreversible Capacity Loss, Rate Capability Retention and Electrode Durability
硅是锂离子电池最有前途的负极材料之一。硅在循环时承受体积变化,这导致随后的粉化和容量衰减。这些缺点导致寿命差,并阻碍了硅阳极的商业化。在这项工作中,基于硅纳米颗粒(SiNPs)锚定在垂直排列的碳纳米管(VACNTs)与定义的间距,以适应体积变化的混合纳米结构阳极合成的商业宏观集流体。实现具有良好稳定性和优异电化学性能的电极仍然是一个挑战。因此,我们在本文中通过在固定的VACNT毯状物长度下改变硅沉积时间来调节SiNP体积,或者通过在固定的SiNP体积下改变VACNT长度来调节活性硅面积负载。SiNP的低面积负载改善了循环期间的容量稳定性,但由于形成了固体电解质界面(SEI)层而引发了大的不可逆容量损失。相比之下,较高的面积负载电极减少了所形成的SEI的量,但是在随后的循环期间负面地影响电极的容量稳定性。通过增加VACNTs毯状物长度而不损害循环稳定性来实现硅的更高重量容量和更高面积负载质量。该混合纳米结构电极显示出优异的稳定性,在2000次循环后可逆容量为1330 mAh g-1。