Next generation batteries based on lithium (Li) metal anodes have been plagued by the dendritic electrodeposition of Li metal on the anode during cycling, resulting in short circuit and capacity loss. Suppression of dendritic growth through the use of solid electrolytes has emerged as one of the most promising strategies for enabling the use of Li metal anodes. We perform a computational screening of over 12,000 inorganic solids based on their ability to suppress dendrite initiation in contact with Li metal anode. Properties for mechanically isotropic and anisotropic interfaces that can be used in stability criteria for determining the propensity of dendrite initiation are usually obtained from computationally expensive first-principles methods. In order to obtain a large dataset for screening, we use machine learning models to predict the mechanical properties of several new solid electrolytes. We train a convolutional neural network on the shear and bulk moduli purely on structural features of the material. We use AdaBoost, Lasso and Bayesian ridge regression to train the elastic constants, where the choice of the model depended on the size of the training data and the noise that it can handle. Our models give us direct interpretability by revealing the dominant structural features affecting the elastic constants. The stiffness is found to increase with a decrease in volume per atom, increase in minimum anion-anion separation, and increase in sublattice (all but Li) packing fraction. Cross-validation/test performance suggests our models generalize well. We predict over 20 mechanically anisotropic interfaces between Li metal and 6 solid electrolytes which can be used to suppress dendrite growth. Our screened candidates are generally soft and highly anisotropic, and present opportunities for simultaneously obtaining dendrite suppression and high ionic conductivity in solid electrolytes.
Rechargeable lithium metal batteries have been widely investigated recently, driven by the global trend for the electrification of transportation. Understanding the dynamics of lithium metal electrodeposition is crucial to design safe and reliable lithium metal anodes. In this study, we developed a grand potential-based phase-field model to investigate the effect of a static gas bubble, which forms due to the complicated internal side reactions, on the dynamics of the dendrite growth during electrodeposition. It is observed that with the presence of a gas bubble, the dendrite growth is largely…
Dendrite formation during electrodeposition while charging lithium metal batteries compromises their safety. While high shear modulus solid-ion conductors (SICs) have been prioritized to resolve pressure-driven instabilities that lead to dendrite propagation and cell shorting, it is unclear whether these or alternatives are needed to guide uniform lithium electrodeposition, which is intrinsically density-driven. Here, we show that SICs can be designed within a universal chemomechanical paradigm to access either pressure-driven dendrite-blocking or density-driven dendrite-suppressing properties…
Effective passivation of lithium metal surfaces, and prevention of battery-shorting lithium dendrite growth, are critical for implementing lithium-metal-anodes for batteries with increased power densities. Nanoscale surface heterogeneities can be "hot spots" where anode passivation breaks down. Motivated by the observation of lithium dendrites in pores and grain boundaries in all-solid batteries, we examine lithium metal surfaces covered with Li(2)O and/or LiF thin films with grain boundaries in them. Electronic structure calculations show that, at >0.25 V computed equilibrium overpotential, L…
Most next-generation Li-ion battery chemistries require a functioning lithium metal (Li) anode. However, its application in secondary batteries has been inhibited because of uncontrollable dendrite growth during cycling. Mechanical suppression of dendrite growth through solid polymer electrolytes (SPE) or through robust separators has shown the most potential for alleviating this problem. Studies of the mechanical behavior of Li at any length scale and temperature are virtually non-existent because of its extreme reactivity, which renders sample preparation, transfer, microstructure characteri…
This work presents an ab initio exploration of fundamental mechanisms with direct relevance to dendrite formation at lithium-electrolyte interfaces. Specifically, we explore surface diffusion barriers and solvated surface energies of typical solid-electrolyte interphase layers of lithium metal electrodes. Our results indicate that surface diffusion is an important mechanism for understanding the recently observed dendrite suppression from lithium-halide passivating layers, which were motivated by our previous work. Our results uncover possible mechanisms underlying a new pathway for mitigating…
Dendrite growth is a long-standing challenge that has limited the applications of rechargeable lithium metal electrodes. Here, we developed a grand potential based nonlinear phase-field model to study the electrodeposition of lithium as relevant for a lithium metal anode, using open-source software package MOOSE. The dynamic morphological evolution under large/small overpotential is studied in 2-dimensions, revealing important dendrite growth/stable deposition patterns. The corresponding temporal-spatial distributions of ion concentration, overpotential and driving force are studied, which dem…
We generalize the conditions for stable electrodeposition at isotropic solid-solid interfaces using a kinetic model which incorporates the effects of stresses and surface tension at the interface. We develop a stability diagram that shows two regimes of stability: previously known pressure-driven mechanism and a new density-driven stability mechanism that is governed by the relative density of metal in the two phases. We show that inorganic solids and solid polymers generally do not lead to stable electrodeposition, and provide design guidelines for achieving stable electrodeposition.
Conditional spinodal decomposition in Li-Mg anodes for lithium metal batteries
Max Planck Institute for Sustainable Materials(马克斯·普朗克可持续材料研究所);Aeronautics Institute of Technology(航空技术学院);Université de Picardie Jules Verne(亚眠儒勒·凡尔纳大学);University Grenoble Alpes, CNRS, Grenoble INP, SIMAP(格勒诺布尔阿尔卑斯大学,法国国家科学研究中心,格勒诺布尔理工学院,SIMAP);Thermo-Calc Software AB(Thermo-Calc软件有限公司);Federal University of São Carlos(圣卡洛斯联邦大学);Korea University(高丽大学);Univ Rouen Normandie, CNRS, INSA Rouen Normandie, Groupe de Physique des Matériaux, UMR 6634(鲁昂诺曼底大学,法国国家科学研究中心,鲁昂诺曼底国立应用科学学院,材料物理研究组)
Lithium metal cells are key towards achieving high specific energy and energy density for electrification of transportation and aviation. Anode-free cells are the limiting case of lithium metal cells involving no excess lithium and the highest possible specific energy. In addition, anode-free cells are easier, cheaper and safer as they avoid handling and manufacturing of lithium metal foils. Issues related to dendrite growth and poor cycling are magnified in anode-free cells due to lack of excess lithium. Electrolyte and current collector surface play a crucial role in affecting the cycling pe…
All solid state Li-ion batteries employing metallic lithium as an anode offer higher energy densities while also being safer than conventional liquid electrolyte based Li-ion batteries. However, the growth of tiny filaments of lithium (dendrites) across the solid state electrolyte layer leads to premature shorting of cells and limits their practical viability. The microscopic mechanisms that lead to lithium dendrite growth in solid state cells are still unclear. Using garnet based lithium ion conductor as a model solid state electrolyte, we show that interfacial void growth during lithium diss…
Magnesium (Mg) metal has been widely explored as an anode material for Mg-ion batteries (MIBs) owing to its large specific capacity and dendrite-free operation. However critical challenges, such as the formation of passivation layers during battery operation and anode-electrolyte-cathode incompatibilities, limit the practical application of Mg-metal anodes for MIBs. Motivated by the promise of group XIV elements (namely Si, Ge and Sn) as anodes for lithium- and sodium-ion batteries, here we conduct systematic first principles calculations to explore the thermodynamics and kinetics of group XIV…
Solid-state batteries (SSBs) can offer a paradigm shift in battery safety and energy density. Yet, the promise hinges on the ability to integrate high-performance electrodes with state-of-the-art solid electrolytes. For example, lithium (Li) metal, the most energy-dense anode candidate, suffers from severe interfacial chemomechanical issues that lead to cell failure. Li alloys of In/Sn are attractive alternatives, but their exploration has mostly been limited to the low capacity(low Li content)and In rich Li$_x$In (x$\leq$0.5). Here, the fundamental electro-chemo-mechanical behavior of Li-In a…
Multi-valent (MV) battery architectures based on pairing a Mg metal anode with a high-voltage ($\sim$ 3 V) intercalation cathode offer a realistic design pathway toward significantly surpassing the energy storage performance of traditional Li-ion based batteries, but there are currently only few electrolyte systems that support reversible Mg deposition. Using both static first-principles calculations and $ab\; initio$ molecular dynamics, we perform a comprehensive adsorption study of several salt and solvent species at the interface of Mg metal with an electrolyte of Mg$^{2+}$ and Cl$^-$ disso…
The properties of rechargeable lithium-ion batteries are determined by the electrochemical and kinetic properties of their constituent materials as well as by their underlying microstructure. Microstructural design can be leveraged to achieve a leap in performance and durability. Here we investigate a porous electrode structure, as a strategy to increase the surface area, and provide structural stability for Li-metal anodes. The porous architecture consists of a mixed electron/ion conductor that function as a scaffold for lithium metal deposition. A new finite element model was developed to si…
Li metal is an ideal anode material for use in state-of-the-art secondary batteries. However, Li-dendrite growth is a safety concern and results in low coulombic efficiency, which significantly restricts the commercial application of Li secondary batteries. Unfortunately, the Li deposition (growth) mechanism is poorly understood on the atomic scale. Here, we used machine learning to construct a Li potential model with quantum-mechanical computational accuracy. Molecular dynamics simulations in this study with this model revealed two self-healing mechanisms in a large Li-metal system, viz. surf…
Controlling nanostructure from molecular, crystal lattice to the electrode level remains as arts in practice, where nucleation and growth of the crystals still require more fundamental understanding and precise control to shape the microstructure of metal deposits and their properties. This is vital to achieve dendrite-free Li metal anodes with high electrochemical reversibility for practical high-energy rechargeable Li batteries. Here, cryogenic-transmission electron microscopy was used to capture the dynamic growth and atomic structure of Li metal deposits at the early nucleation stage, in w…
Density functional theory and ab initio molecular dynamics simulations are applied to investigate the migration of Mn(II) ions to above-surface sites on spinel Li(x)Mn(2)O(4) (001) surfaces, the subsequent Mn dissolution into the organic liquid electrolyte, and the detrimental effects on graphite anode solid electrolyte interphase (SEI) passivating films after Mn(II) ions diffuse through the separator. The dissolution mechanism proves complex, the much-quoted Hunter disproportionation of Mn(III) to form Mn(II) is far from sufficient. Key steps that facilitate Mn(II) loss include concerted liqu…
An Ultrathin Laterally Conductive Mesh Interphase Enables Spatially Extended Zinc Deposition for Aqueous Zinc Batteries
University of Chemistry and Technology Prague(布拉格化工大学);Technische Universität Dresden(德累斯顿工业大学);Center for Advancing Electronics Dresden (cfaed)(德累斯顿先进电子中心);Faculty of Chemistry and Food Chemistry, Technische Universität Dresden(德累斯顿工业大学化学与食品化学学院);Max Planck Institute of Microstructure Physics(马克斯·普朗克微观结构物理研究所);Chair of Analytical Chemistry, Faculty of Chemistry and Biochemistry, Ruhr- University Bochum(鲁尔大学波鸿分校化学与生物化学学院分析化学系)
All-solid-state batteries are expected to enable batteries with high energy density with the use of lithium metal anodes. Although solid electrolytes are believed to be mechanically strong enough to prevent lithium dendrites from propagating, various reports today still show cell failure due to lithium dendritic growth at room temperature. While cell parameters such as current density, electrolyte porosity and interfacial properties have been investigated, mechanical properties of lithium metal and the role of applied stack pressure on the shorting behavior is still poorly understood. Here, we…
The most promising solid electrolytes for all-solid-state Li batteries are oxide and sulfide ceramics. Current ceramic solid electrolytes are brittle and lack the toughness to withstand the mechanical stresses of repeated charge and discharge cycles. Solid electrolytes are susceptible to crack propagation due to dendrite growth from Li metal anodes and to debonding processes at the cathode/electrolyte interface due to cyclic variations in the cathode lattice parameters. In this perspective, we argue that solutions to the mechanics challenges of all-solid-state batteries can be borrowed from th…
Influence of Electrode Thickness and Electrolyte Composition on SEI Formation and Cycle Stability in Binder-Free Hard Carbon Anodes for Na-Ion Batteries
Université de Haute-Alsace(阿尔萨斯大学);Institut de Science des Matériaux de Mulhouse (IS2M)(穆尔豪斯材料科学研究所);CNRS UMR 7361(法国国家科学研究中心联合研究实验室7361);Université de Strasbourg(斯特拉斯堡大学);Réseau sur le Stockage Electrochimique de l’Energie (RS2E)(电化学储能网络);CNRS FR3459(法国国家科学研究中心自由研究基金3459)
本研究探讨了硬碳自支撑电极厚度、大孔率及电解液添加剂对钠离子电池SEI形成和循环稳定性的影响,发现FEC添加剂可改善稳定性,实现高达93%的初始库仑效率和328 mAh g-1的可逆容量。