Atomically sharp epitaxial growth of Bi2Se3 films is achieved on Si (111) substrate with MBE (Molecular Beam Epitaxy). Two-step growth process is found to be a key to achieve interfacial-layer-free epitaxial Bi2Se3 films on Si substrates. With a single-step high temperature growth, second phase clusters are formed at an early stage. On the other hand, with low temperature growth, the film tends to be disordered even in the absence of a second phase. With a low temperature initial growth followed by a high temperature growth, second-phase-free atomically sharp interface is obtained between Bi2Se3 and Si substrate, as verified by RHEED (Reflection High Energy Electron Diffraction), TEM (Transmission Electron Microscopy) and XRD (X-Ray Diffraction). The lattice constant of Bi2Se3 is observed to relax to its bulk value during the first quintuple layer according to RHEED analysis, implying the absence of strain from the substrate. TEM shows a fully epitaxial structure of Bi2Se3 film down to the first quintuple layer without any second phase or an amorphous layer.
Epitaxial Ni/Cu Superlattice Nanowires with Atomically Sharp Interfaces for Spin Transport
Jožef Stefan Institute(约瑟夫·斯特凡研究所);Max-Planck-Institut für Nachhaltige Materialien(马克斯·普朗克可持续材料研究所);Institute of Nanoscience and Nanotechnology, Department of Physics, University of Kashan(卡尚大学物理系纳米科学与技术研究所);Department of Medical Equipment Technology Engineering, Al-Hadba University(阿尔哈德巴大学医疗设备技术工程系);Institut Jean Lamour – CNRS – Université de Lorraine(让·拉缪尔研究所 - 法国国家科学研究中心 - 洛林大学);Institut Universitaire de France (IUF)(法兰西学院);Jožef Stefan International Postgraduate School(约瑟夫·斯特凡国际研究生院)
Metal-induced gap states in epitaxial organic-insulator/metal interfaces
我们已经表明,在实验和理论上,金属诱导的间隙状态(MIGS)可以存在于外延生长的有机绝缘体/金属界面。实验是针对具有元素选择性近边X射线吸收精细结构(NEXAFS)的烷烃/Cu(001)进行的,其表现出指示MIGS的前峰。{ \it ab initio}电子结构计算支持MIGS的存在。当用Ni代替Cu衬底时,预测界面磁性(在界面处的自旋极化有机晶体)可能具有载流子掺杂。
Tuning metal-insulator transitions in epitaxial V$_2$O$_3$ thin films
采用直流反应磁控溅射法在$c$平面Al $_2$ O $_3$衬底上外延生长V $_2$ O $_3$薄膜。结果揭示了一个温度窗口,在大大低于以前报道的值,其中外延膜时,可以得到沉积在[0001]取向的表面。该薄膜显示金属-绝缘体的转变与高达四个数量级的电阻的变化,强烈依赖于在沉积过程中的O $_2$分压。虽然薄膜的电子性质显示出对薄膜沉积过程中存在的O $_2$的量的敏感性,但它们的晶体结构和原子级平坦的台阶结构的表面形态具有高达微米的尺寸被保持。的转变温度,以及金属-绝缘体转变的规模,相关的化学计量和局部应变的薄膜中的沉积参数可控。
Millimeter-Scale, Atomically Controlled 2D Topological Insulators Revealed by Multimodal Spectroscopy
The University of Chicago(芝加哥大学);Gachon university(嘉泉大学);Weizmann Institute of Science(魏茨曼科学研究所);Northwestern University(西北大学);University of Illinois Urbana-Champaign(伊利诺伊大学厄巴纳-香槟分校);University of Florida(佛罗里达大学);Pennsylvania State University(宾夕法尼亚州立大学);University of Maryland, College Park(马里兰大学帕克分校)
Transport properties of band engineered p-n heterostructures of epitaxial Bi$_2$Se$_3$/(Bi$_{1-x}$Sb$_x$)$_2$(Te$_{1-y}$Se$_y$)$_3$ topological insulators
在Bi基三维拓扑绝缘体材料中,寄生体掺杂的挑战仍然无处不在,特别是在通过分子束外延(MBE)制备样品时。在这里,我们提出了一种异质结构的外延BSTS生长的方法。薄的n型Bi $_2$ Se $_3$(BS)层被用作外延和静电种子,其显著地改善了样品性质的结晶和电子质量以及再现性。在具有p型(Bi $_{1-x}$ Sb $_x$)$_2$(Te $_{1-y}$ Se $_y$)$_3$(BSTS)的BS异质结构中,我们证明了仅通过调整相应层的厚度来调谐电子性质的固有带弯曲效应。弱反局域化的特点,在磁导的分析表明,随着BSTS厚度的增加,顶部和底部的导电层的分离。通过温度和门依赖的传输测量,我们表明,薄BS种子层可以完全耗尽内的异质结构,并证明通过背栅在整个样品厚度的带的静电调谐。
Study of polycrystalline bulk Sr$_3$OsO$_6$ double-perovskite insulator: comparison with 1000 K ferromagnetic epitaxial films
在高温高压(1200 $^\circ$ C,6 GPa)条件下,通过固相反应合成了有序双钙钛矿绝缘体SrPDMATHABMM OsO $_6$多晶。的合成使我们能够进行比较研究的散装形式的Sr $_3$ OsO $_6$朝向揭示1000 K铁磁性的驱动机制,这是最近发现的外延生长的Sr $_3$ OsO $_6$薄膜。与薄膜不同的是,块体主要是反铁磁性而不是铁磁性。因此,只有当Sr $_3$ OsO $_6$受到界面的影响时,才会出现强的铁磁有序.在低温下($<$ 17 K),比热容为39.6(9)× 10 $^{-3}$ J mol $^{-1}$ K $^{-2}$.这个值是非常高的,这表明在磁基态可能存在类似费米子的激发。虽然Sr $_3$ OsO $_6$的体相和薄膜相具有相同的晶格基和电绝缘状态,但它们的磁性却完全不同。
Si Intercalation Beneath Epitaxial Graphene: Modulating Mott States at the SiC(0001) Interface
Institute of Physics, Chemnitz University of Technology(开姆尼茨工业大学物理研究所);Center for Materials, Architectures and Integration of Nanomembranes (MAIN)(纳米膜材料、架构与集成中心)
Single-Crystalline Al/Ge Heterostructure with an Atomically Sharp Commensurate Interface
Beijing Academy of Quantum Information Sciences(北京量子信息科学研究院);Beijing National Laboratory for Condensed Matter Physics and Institute of Physics, Chinese Academy of Sciences(中国科学院物理研究所、凝聚态物理国家实验室);Peking University(北京大学)
Accurate prediction of optical transitions in epitaxial InGaAs/InAlAs asymmetric coupled quantum well structures
Centre de Nanosciences et de Nanotechnologies, CNRS - Université Paris-Saclay(纳米科学与技术中心,法国国家科学研究中心-巴黎萨克雷大学);III-V Lab(III-V 实验室);Laboratoire de Physique de l’École Normale Supérieure, ENS, Université, PSL, CNRS, Sorbonne Université, Université Paris Cité(巴黎高等师范学校物理实验室,巴黎文理研究大学,法国国家科学研究中心,索邦大学,巴黎西岱大学)
Atomically precise interfaces from non-stoichiometric deposition
复合氧化物异质结构显示出一些最化学突变的、原子精确的界面,这在通过并置不相容的基态来构造具有涌现性质的新界面相时是有利的。人们可能会认为,原子精确的界面从化学计量生长的结果,但在这里,我们表明,最精确的控制是获得非化学计量的生长,不同的表面能,可以通过表面活性剂样的效果进行补偿。对于精确生长的Sr $_{n+1}$ Ti $_n$ O $_{3n+1}$ Ruddlesden-Popper(RP)相,化学计量沉积导致的损失的第一RP岩盐双层,但生长与富锶的表面层恢复批量化学计量和有序的次表面RP结构。我们的研究结果极大地扩展了可以在外延异质结构中制备的材料,具有精确的界面控制-从仅仅$n=\infty$端成员(钙钛矿)到整个RP家族-使人们能够在更丰富的氧化物界面上探索新的量子现象。
Molecular Beam Epitaxial Growth of Bi2Te3 and Sb2Te3 Topological Insulators on GaAs (111) Substrates: A Potential Route to Fabricate Topological Insulator p-n Junction
采用固体源分子束外延技术在GaAs(111)衬底上外延生长了高质量的Bi 2 Te 3和Sb 2 Te 3拓扑绝缘体薄膜。用反射高能电子衍射、原子力显微镜、X射线衍射和高分辨透射电子显微镜研究了它们在邻位和非邻位GaAs(111)衬底上的生长和行为。发现非邻位GaAs(111)衬底比邻位GaAs(111)衬底更能获得高质量的Bi_2Te_3和Sb_2Te_3薄膜。霍尔和磁阻测量表明,p型Sb_2Te_3和n型Bi_2Te_3拓扑绝缘体薄膜可以直接生长在GaAs(111)衬底上,这为在同一衬底上制备拓扑绝缘体pn结提供了一条途径,与现有半导体光电子器件的制备工艺相兼容。
Epitaxial germanidation of full-Heusler Co2FeGe alloy thin films formed by rapid thermal annealing
采用快速热退火诱导锗化方法,在绝缘体上硅(SOI)衬底上外延生长Fe/Co/赝Ge(001)-on-insulator(GOI)多层膜,制备了全Heusler Co2 FeGe(CFG)合金薄膜。X射线衍射(XRD)分析结果表明,薄膜沿[001]方向外延生长,且具有面内外延结构,薄膜的面内外延关系为[100]|| GOI[100],虽然电影稍微包含纹理成分。强的(111)和(200)超晶格衍射强度表明,CFG薄膜具有高度有序的L21结构。薄膜的横截面高分辨率透射电子显微镜图像表明薄膜具有主要的外延和轻微的织构组分,这与XRD测量结果一致。外延元件直接生长在SOI衬底的BOX层上,而不形成任何界面层。