氧化镓($β$-Ga$_2$O$_3$)在高温、高功率和传感电子学应用中展现出巨大潜力。然而,高温下长期稳定的欧姆接触金属化层面临着独特的热力学挑战。目前最常见的基于20 nm Ti的欧姆接触设计,由于非化学计量的Ti/Ga$_2$O$_3$界面反应和动力学上有利的Ti扩散过程的共同作用,已被反复证明在中等升温(300-400$^{\circ}$C)下即会失效。在此,我们利用具有自限制界面反应的超薄Ti层,展示了可在500-600$^{\circ}$C下稳定运行的Ga$_2$O$_3$器件欧姆接触。5nm Ti / 100nm Au接触堆叠中的超薄Ti层被设计为在形成欧姆接触时完全氧化,从而限制了热力学和动力学不稳定性。这种新型接触设计策略形成了一层外延导电锐钛矿型氧化钛界面层,实现了低电阻欧姆接触,该接触在真空($\leq$ 10$^{-4}$ Torr)中600$^{\circ}$C下长期连续运行(>500小时)以及在流动N$_2$中室温和550$^{\circ}$C之间反复热循环(15次)后均保持稳定。这种稳定的欧姆接触设计将推动高温器件的发展,使研究重点得以转向整流接触及其他界面层。
英文摘要:
Beta gallium oxide ($β$-Ga$_2$O$_3$) shows significant promise in the high-temperature, high-power, and sensing electronics applications. However, long-term stable metallization layers for Ohmic contacts at high temperature present unique thermodynamic challenges. The current most common Ohmic contact design based on 20 nm of Ti has been repeatedly demonstrated to fail at even moderately elevated temperatures (300-400$^{\circ}$C) due to a combination of non-stoichiometric Ti/Ga$_2$O$_3$ interfacial reactions and kinetically favored Ti diffusion processes. Here we demonstrate stable Ohmic contacts for Ga$_2$O$_3$ devices operating up to 500-600$^{\circ}$C using ultrathin Ti layers with a self-limiting interfacial reaction. The ultrathin Ti layer in the 5nm Ti / 100nm Au contact stack is designed to fully oxidize while forming an Ohmic contact, thereby limiting both thermodynamic and kinetic instability. This novel contact design strategy results in an epitaxial conductive anatase titanium oxide interface layer that enables low-resistance Ohmic contacts that are stable both under long-term continuous operation (>500 hours) at 600$^{\circ}$C in vacuum ($\leq$ 10$^{-4}$ Torr), as well as after repeated thermal cycling (15 times) between room temperature and 550$^{\circ}$C in flowing N$_2$. This stable Ohmic contact design will accelerate the development of high-temperature devices by enabling research focus to shift towards rectifying contacts and other interfacial layers.
On the importance of Ni-Au-Ga interdiffusion in the formation of a Ni-Au / p-GaN ohmic contact
Centre de Nanosciences et de Nanotechnologies, C2N, UMR 9001, CNRS, Université Paris-Saclay(纳米科学和纳米技术研究中心);CRHEA, UMR7073, CNRS, Université Côte d’Azur(高电阻率电子学中心);Institut d’Electronique, de Microélectronique et de Nanotechnologie, IEMN, UMR 8520, CNRS, Université de Lille(电子、微电子和纳米技术研究所);Georgia Tech CNRS, IRL 2958, GT-Europe(佐治亚理工学院-法国国家科学研究中心联合研究)
The influence of Bi2O3 glass powder in silver paste on the fabrication of ohmic contacts and its potential effectiveness in solar cells and integrated circuits on p-type silicon substrates
Physical mechanisms of ohmic contact and tunnel diode: A novel explanation in terms of impurity-photovoltaic-effect resulting from infrared self-emission at room-temperature
Institute of Semiconductors, Chinese Academy of Sciences(中国科学院半导体研究所)
Numerical analysis and simulation of lateral memristive devices: Schottky, ohmic, and multi-dimensional electrode models
Weierstrass Institute for Applied Analysis and Stochastics (WIAS)(魏尔斯特拉斯应用分析与随机性研究所);Univ. Lille, CNRS, Inria, UMR 8524 - Laboratoire Paul Painlevé(里尔大学、法国国家科学研究中心、法国国家信息与自动化研究所,UMR 8524 - 保罗·潘勒瓦实验室);Christian-Albrechts-Universität zu Kiel(基尔大学)