Ge virtual substrates for high efficiency III-V solar cells: applications, potential and challenges
Iván García, Manuel Hinojosa, Iván Lombardero, Luis Cifuentes, Ignacio Rey-Stolle, Carlos Algora, Huy Nguyen, Stuart Edwards, Aled Morgan, Andrew Johnson
发表信息:
Proceedings of the IEEE Photovoltaic Specialists Conference 2019
Virtual substrates based on thin Ge layers on Si by direct deposition have achieved high quality recently. Their application to high efficiency III-V solar cells is analyzed in this work. Replacing traditional Ge substrates with Ge/Si virtual substrates in standard lattice-matched and upright metamorphic GaInP/Ga(In)As/Ge solar cells is feasible according to our calculations using realistic parameters of state-of-the-art Ge solar cells but with thin bases (< 5um). The first experimental steps are tackled by implementing Ge single-junction and full GaInP/Ga(In)As/Ge triple-junction solar cells on medium quality Ge/Si virtual substrates with 5um thick Ge layers. The results show that the photocurrent in the Ge bottom cell is barely enough to achieve current matching with the upper subcells, but the overall performance is poor due to low voltages in the junctions. Moreover, observed cracks in the triple-junction structure point to the need to reduce the thickness of the Ge + III-V structure or using other advanced approaches to mitigate the thermal expansion coefficient mismatch effects, such as using embedded porous silicon. Next experimental work will pursue this objective and use more advanced Ge/Si virtual substrates available with lower threading dislocation densities and different Ge thicknesses.
Pulsed Laser Ejection of Single-Crystalline III-V Solar Cells From GaAs Substrates
与许多光电子产品一样,最高质量的III-V族太阳能电池最初是在GaAs衬底上的薄单晶多层膜。将这些器件层与它们的生长衬底分离能够实现更高性能的器件和晶片再利用,这两者对于III-V太阳能电池在陆地市场中的生存能力都是至关重要的。在这里,我们删除刚性结合,晶格匹配,16毫米$^2$ × 3.5 μ m厚的GaAs器件的GaAs基板使用10纳秒,非聚焦Nd:YAG激光脉冲。该脉冲在器件下方的较低带隙、晶格匹配的结晶层中被选择性地吸收,从而驱动准二维烧蚀事件,该烧蚀事件将结晶多层从衬底上剥离。在几分钟的选择性湿化学蚀刻和前接触沉积后,我们的冠军0.1 cm $^2$器件显示出(17.4 +/- 0.5)%的功率转换效率和1.07 V的开路电压,使用AM 1.5直接(1000 W m $^{-2}$),没有抗反射涂层。我们表明,性能是通过传统的基板溶解工艺生产的类似的太阳能电池。我们讨论了独特的工艺特点和机会,如每个激光脉冲分离晶圆大小的薄膜太阳能电池的潜力。
III-V antiphase boundaries are not generated by Si or Ge substrate step edges
Univ Rennes, INSA Rennes(雷恩大学,雷恩国立应用科学学院);CNRS, Institut FOTON – UMR 6082(法国国家科学研究中心,FOTON研究所);IES, University of Montpellier(蒙彼利埃大学,生态系统与可持续发展研究所);CNRS(法国国家科学研究中心);Univ Rennes, CNRS, IPR (Institut de Physique de Rennes)–UMR 6251(雷恩大学,法国国家科学研究中心,雷恩物理研究所);C2N, University of Paris Saclay(巴黎萨克雷大学,纳米科学中心);CNRS, UMR 9001(法国国家科学研究中心)
High-reflectance III-nitride distributed Bragg reflectors grown on Si substrates
在Si(111)衬底上生长了AlN/AlGaN超晶格分布布拉格反射器(DBR)。通过在Si衬底上直接生长DBR来实现Si上的第一高反射率III族氮化物DBR,以由于Si/AlN界面处的高折射率对比度而增强整体反射率。对于9 x DBR,96.8%的实测峰值反射率实际上超过了96.1%的理论值。AlN/AlGaN超晶格起到了补偿无裂纹500 nm GAN /7 x DBR / Si结构生长期间产生的大拉伸应变的额外目的。这一成就为在不透明Si衬底中制造无光吸收的高质量III族氮化物光电子器件提供了可能性。
Wurtzite III-nitride distributed Bragg reflectors on Si (100) substrates
首次在Si(100)衬底上制备了由AlN/GAN超晶格组成的分布布拉格反射器(DBR)。在此立方衬底上,采用表面法线指向[110]方向4°的Si(100)晶片,获得了单晶纤锌矿超晶格结构。这种取向不良引入了额外的外延约束,其阻止了双畴GAN表面以及立方GAN夹杂物的生长。在Si(100)上实现了无裂纹的600 nm GAN帽层/5 x AlN / GAN DBR结构。在Si(100)上实现纤锌矿III族氮化物DBR为将新型光学和光电子器件与已建立的Si微电子技术集成提供了可能性。
Heteroepitaxial Growth of PbSe on InP Substrates via Lattice-Matched III-V Buffer Layers
CREOL, The College of Optics and Photonics, University of Central Florida(中佛罗里达大学光学与光子学院);Department of Materials Science and Engineering, University of Central Florida(中佛罗里达大学材料科学与工程系)
Parasitic Bipolar Leakage in III-V FETs: Impact of Substrate Architecture
实验和理论表明,具有中到高In含量的基于InGaAs的全包围栅(GAA)FET不适合用于低泄漏的先进CMOS节点。其主要原因是由寄生双极效应(PBE)引起的大泄漏损失,这在GAA架构中被认为特别难以补救。实验证据的PBE在In 70 Ga 30 As GAA FET的演示,随着PBE行为的模拟为基础的分析。PBE的影响进行了研究,通过模拟替代器件架构,如体FinFET和绝缘体上FinFET。PBE被发现是不可忽略的,在所有标准的InGaAs FET设计。实用PBE指标的介绍和PBE抑制基板架构的设计阐明。最后,它的结论是,GAA架构是不适合低泄漏InGaAs FET的体FinFET是更适合的角色。
Ultrashort pulse action onto thin film on substrate: Qualitative model of shock propagation in substrate explaining phenomenon of fast growth of a hole with increase of absorbed energy