arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1811.10482cond-mat.mtrl-sciphysics.chem-ph
收藏

β-Ta薄膜电子结构的X射线光电子能谱学和第一性原理计算

Electronic Structure of Beta-Ta Films from X-ray Photoelectron Spectroscopy and First-principles Calculations

Martin Magnuson, Grzegorz Greczynski, Fredrik Eriksson, Lars Hultman, Hans Högberg

摘要:

用4f芯能级和价带X射线光电子能谱学研究了001取向的β-Ta薄膜(空间群P421 m)的电子结构和化学键,并与α-Ta体相进行了比较。对于β相,4f 7/2峰位于21.91 eV处,4f 5/2位于23.81 eV处,其比α-Ta参考的相应4f峰高0.16 eV。我们认为,这种化学位移源于电子屏蔽,较高的电阻率或应变的β-钽膜。此外,在价带的底部的5d-5s状态被移动了0.75 eV的更高的结合能在β-Ta相比,α-Ta。这是由于最近邻的数量较低,在β-Ta中为4个,而在α-Ta相中为8个。本文讨论了β-Ta和α-Ta的电子结构、价带的谱线形状和Ta 4f,5 p芯能级的能级位置的差异,并与计算的β-Ta和α-Ta的态进行了比较。特别地,根据Mott定律,β-Ta(0.557态/eV/原子)相对于α-Ta(1.032态/eV/原子)的费米能级处的较低数目的态应当降低金属中的电导率并且通过价带中的电荷重新分布来影响稳定性。这在实验上得到了膜的电阻率测量值的支持,该膜的电阻率测量值为约170微欧姆-厘米,而α-Ta块体的电阻率测量值为约13.1微欧姆-厘米。

英文摘要:

The electronic structure and chemical bonding of Beta-Ta synthesized as a thin 001-oriented film (space group P421m) is investigated by 4f core level and valence band X-ray photoelectron spectroscopy and compared to alfa-Ta bulk. For the Beta-phase, the 4f7/2 peak is located at 21.91 eV and with the 4f5/2 at 23.81 eV which is 0.16 eV higher compared to the corresponding 4f peaks of the alfa-Ta reference. We suggest that this chemical shift originates from electron screening, higher resistivity or strain in the Beta-Ta film. Furthermore, the 5d-5s states at the bottom of the valence band are shifted by 0.75 eV towards higher binding energy in Beta-Ta compared to alfa-Ta. This is a consequence of the lower number of nearest neighbors with four in Beta-Ta compared to eight in the alfa-Ta phase. The difference in the electronic structures, spectral line shapes of the valence band and the energy positions of the Ta 4f, 5p core-levels of Beta-Ta versus alfa-Ta are discussed in relation to calculated states of Beta-Ta and alfa-Ta. In particular, the lower number of states at the Fermi level of Beta-Ta (0.557 states/eV/atom) versus alfa-Ta (1.032 states/eV/atom) that according to Mott's law should decrease the conductivity in metals and affect the stability by charge redistribution in the valence band. This is experimentally supported from resistivity measurements of the film yielding a value of ~170 micro-Ohm-cm in comparison to alfa-Ta bulk with a reported value of ~13.1 micro-Ohm-cm.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑