We study the role of thermal magnons in the spin and heat transport across a normal-metal/insulating-ferromagnet interface, which is beyond an elastic electronic spin transfer. Using an interfacial exchange Hamiltonian, which couples spins of itinerant and localized orbitals, we calculate spin and energy currents for an arbitrary interfacial temperature difference and misalignment of spin accumulation in the normal metal relative to the ferromagnetic order. The magnonic contribution to spin current leads to a temperature-dependent torque on the magnetic order parameter; reciprocally, the coherent precession of the magnetization pumps spin current into the normal metal, the magnitude of which is affected by the presence of thermal magnons.
Detection of the interfacial exchange field at a ferromagnetic insulator-nonmagnetic metal interface with pure spin currents
在铁磁金属(NM)和铁磁绝缘体(FI)之间的界面处,自旋电流可以与磁化相互作用,导致自旋电流的调制。在这些FI-NM界面的界面交换场可以通过将该界面放置成与横向自旋阀(LSV)器件的自旋输运通道接触并观察额外的自旋弛豫过程来探测。研究了铁磁绝缘体EuS(EuS-LSV)和钇铁石榴石YPDMATHABMM Fe $_5$ O $_{12}$(YIG-LSV)附近的Cu自旋输运通道的横向自旋阀器件中的界面交换场.将自旋信号与在具有MgO或AlO $_x$覆盖的单晶硅/SiO $_2$衬底上制造的参考横向自旋阀器件进行比较。EuS-LSV和YIG-LSV中的非局域自旋阀信号分别低约4倍和6倍。自旋信号的抑制归因于由于界面自旋轨道场而在Cu-EuS(或Cu-YIG)界面处增强的表面自旋翻转概率。除了自旋信号的抑制外,我们还发现在$T \sim$ 30 K处的自旋信号中广泛观察到的低温峰在与EuS或YIG接触的情况下向更高的温度移动。不同注入器-检测器距离的自旋信号的温度依赖性揭示了在这些界面处的波动交换场导致额外的自旋退相干,其除了常规的自旋弛豫源之外还限制了自旋弛豫时间。结果表明,纯自旋电流随温度变化的测量方法可以用来探测铁磁绝缘体-铁磁金属界面的界面交换场。
Emergence of Unconventional Interfacial Magnetic Phenomenon in Topological Insulator-Based Magnetic Heterostructures
在拓扑绝缘体(TI)/磁性绝缘体(MI)异质结构中,TI的大自旋轨道耦合和界面处的反转对称性破缺可以在界面处促进非平面自旋织构,例如skyrmion。这在常规霍尔设置中被观察为拓扑霍尔效应。虽然已经在TI/MI的界面处观察到这种效应,其中MI观察到垂直磁各向异性,但在具有面内磁各向异性的界面MI中发展的非平凡自旋纹理被报道不足。在这项工作中,我们利用平面霍尔效应(PHE)研究了Bi $_2$ Te $_3$ /EuS异质结构。我们观察到的平面拓扑霍尔和自发平面霍尔功能的特点是在界面处的非平凡的面内自旋纹理。我们发现,后者是最小的电流和磁场方向平行对齐时,和最大的样品平面内,这可能归因于潜在的平面各向异性的自旋织构垂直对齐时。这些结果表明的重要性,PHE灵敏的检测和表征的非平凡的磁相,逃避了勘探的TI/MI接口。
Edge and Interfacial States in a 2D Topological Insulator:Bi(111) Bilayer on Bi$_{2}$Te$_{2}$Se
利用扫描隧道谱(STS)和第一性原理计算研究了二维拓扑绝缘体Bi(111)双层膜及其边缘的电子态.在解理的Bi $_{2}$ Te $_{2}$ Se晶体上外延生长了具有锯齿形边缘的有序双层膜和岛。计算表明,由于Bi和Bi $_{2}$ Te $_{2}$ Se之间的强相互作用,Bi双层膜的带隙关闭,形成了一个新的但很小的杂化带隙.尽管如此,拓扑性质的Bi双层和拓扑边缘状态被保存只有一个能量转移。边缘增强的局域态密度被STS清晰地识别和可视化,与计算结果吻合得很好。这可以是拓扑边缘态的符号,它对应于量子自旋霍尔态。Bi和Bi $_{2}$ Te $_{2}$ Se之间的界面态也在带隙区域内被识别。这种状态也表现出边缘调制,这是以前解释为拓扑边缘状态的证据[F。Yang等人,物理修订版信函109,016801(2012)]。
Electrically tunable interfacial thermal conduction via electronic structure engineering in ${Au}$/$Bi_{1-x}$$Sb_{x}$ topological insulators
The Ohio State University(俄亥俄州立大学);Korea Institute of Science and Technology (KIST)(韩国科学技术院);Korea Advanced Institute of Science and Technology (KAIST)(韩国科学技术院);Pohang University of Science and Technology (POSTECH)(浦项科技大学);Carnegie Mellon University(卡内基梅隆大学);E. O. Lawrence Berkeley National Laboratory(劳伦斯伯克利国家实验室)
Effects of Crystalline Disorder on Interfacial and Magnetic Properties of Sputtered Topological Insulator/Ferromagnet Heterostructures
由拓扑绝缘体和铁磁体组成的薄膜是高能效自旋电子学器件的理想选择。在这里,TI的晶体结构无序的界面和磁性能的溅射沉积的TI/FM,Bi 2 Te 3/Ni 80 Fe 20,异质结的影响进行了报道。发现Ni和少量Fe从Py扩散穿过界面并与Bi 2 Te 3反应。对于高度结晶的c轴取向的Bi 2 Te 3薄膜,吉尔伯特阻尼的巨大增强被观察到,伴随着有效的面外磁各向异性和增强的阻尼样自旋轨道扭矩(DL-SOT),可能是由于拓扑表面状态(TSS)的Bi 2 Te 3。此外,在低温下的磁滞回线测量中观察到自发交换偏置。这是由于扩散的Ni与Bi_2 Te_3反应形成的反铁磁拓扑界面层与FM,Ni_(80)Fe_(20)耦合。随着Bi_2Te_3无序度的增加,AFM界面层中的交换相互作用明显减弱。
Stabilizing Magnetic Bubble Domains in Epitaxial 2D Magnet/Topological Insulator Heterostructures through Interfacial Interactions
University of Southern California(南加州大学);University of South Florida(南佛罗里达大学);The Ohio State University(俄亥俄州立大学);Max Planck Institute for Solid State Research(马克斯·普朗克固体研究所);Helmholtz-Zentrum Berlin für Materialien und Energie(柏林赫尔姆霍兹材料能源中心)
Interaction of magnons with plasmons in a system of antiferromagnetic insulators coupled to a superconductor microwave cavity through the interfacial exchange interaction
A Molecular Approach for Engineering Interfacial Interactions in Magnetic-Topological Insulator Heterostructures
控制磁性/拓扑绝缘体异质结构中的界面相互作用是出现新的自旋相关电子现象的主要挑战。对于任何依赖邻近效应的异质结构的合理设计,理想情况下应该保留每个组件的整体属性,同时调整界面处的相互作用。然而,在大多数无机界面相互作用太强,因此扰动,甚至淬火,在界面的每一侧的磁矩和拓扑表面状态。在这里,我们表明,这些属性可以通过使用配体化学来调整磁性离子与表面状态的相互作用来保持。通过在Bi $_2$ Te $_3$薄膜的表面上沉积Co基卟啉和酞菁单层,形成了稳健的界面,其保留了未掺杂的拓扑表面状态以及二价Co离子的原始磁矩。所选择的配体允许我们在该弱相互作用范围内调节界面杂化。这些结果,这是在与Co酞菁的相互作用诱导的Bi $_2$ Se $_3$的第一个五重层的表面状态的观察到的抑制形成鲜明对比,证明了平面金属有机分子的能力,跨越从强到弱的限制的相互作用。
Interface Engineering Enabled Low Temperature Growth of Magnetic Insulator on Topological Insulator
在异质结构中结合拓扑绝缘体(TI)和磁性材料对于推进基于自旋的电子学至关重要。磁绝缘体(MI)可以使用自旋喷涂工艺沉积在TI上,这是一种独特的非真空低温生长工艺。TI具有在暴露于大气时氧化的高反应性表面,使得在TI上生长旋转喷雾铁氧体具有挑战性。在这项工作中,它被证明是一个薄的钛覆盖层上TI,然后在大气中氧化,以产生一个薄的TiOx界面层,保护TI表面,而不会显着损害自旋传输从磁性材料的整个TiOx的TI表面状态。首先,证明了在Bi 2 Te 3/TiOx/Ni 80 Fe 20异质结构中,TiOx提供了对磁性物质扩散的优异阻挡,但保持了大的自旋泵浦效应。第二,TiOx也被用作Bi 2 Te 3上的保护性覆盖层,随后是MI,NixZnyFe 2 O 4(NZFO)的旋转喷射生长。对于最薄的TiOx阻挡层,由于扩散,Bi_2Te_3/TiOx/NZFO样品具有AFM无序界面层。随着TiOx阻挡层厚度的增加,扩散减少,但仍保持强的界面自旋泵相互作用。这些实验结果表明,一种新的方法,低温生长的磁绝缘体上的TI使接口工程。
Persistent Interfacial Topological Hall Effect Demonstrating Electrical Readout of Topological Spin Structures in Insulators
University of Nebraska, Lincoln(内布拉斯加大学林肯分校);Fudan University(复旦大学);North Carolina State University(北卡罗来纳州立大学);Georgia Institute of Technology(佐治亚理工学院);Bryn Mawr College(布林茅尔学院);Argonne National Laboratory(阿贡国家实验室)
Spin Seebeck Effect in Normal-Metal--Chiral-Insulator Heterostructure
Key Laboratory of Advanced Optoelectronic Quantum Architecture and Measurement, Ministry of Education, Beijing Institute of Technology(北京理工大学);Graduate School of China Academy of Engineering Physics(中国工程物理研究院研究生院)