新超导体RO(1-x)F(x)FeAs的WDX分析及其对电子Phase Diagram的影响

WDX-Analysis of the New Superconductors RO(1-x)F(x)FeAs and Its Consequences on the Electronic Phase Diagram

Anke Köhler, Günter Behr

摘要:

在电子显微镜中通过波长色散X射线光谱(WDX)研究RO 1-xFxFeAs(0 < x < 0.25)(R = La、Sm、Gd)的多晶样品,以确定样品的组成,特别是氟含量。发现测量的氟含量可显著偏离初始重量。在镧系化合物LaO_(1-x)F_xFe_(As)中,主要在x > 0.05时有较好的一致性,而在x < 0.05时,氟几乎不进入样品。对于钐化合物,我们在所有氟浓度下测量的样品中的氟少于最初称重的一半。在绘制LaO 1-xFxFeAs和SmO 1-xFxFeAs的电子相图时考虑这些测量值。这导致与初始重量的图相比,两个图的图片更加一致。

英文摘要:

Polycrystalline samples of RO1-xFxFeAs (0 < x < 0.25) (R = La, Sm, Gd) were investigated by wavelength-dispersive X-ray spectroscopy (WDX) in the electron microscope to determine the composition of the samples, in particular the fluorine content. It was found that the measured fluorine content can deviate considerably from the initial weight. In the lanthanum compound LaO1-xFxFeAs, we found good agreement mainly for x > 0.05, but for x < 0.05 the fluorine hardly goes into the sample. For the samarium compound we measured less than half the fluorine in the sample as initially weighed at all fluorine concentrations. These measured values are taken into account when drawing the electronic phase diagrams of LaO1-xFxFeAs and SmO1-xFxFeAs. This leads to a more consistent picture of both of the diagrams in comparison to the plot of the initial weight.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑