arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2512.16643physics.ins-dethep-ex
收藏

中子辐照二极管的长期退火行为的温度依赖性

Temperature dependence of the long-term annealing behavior of neutron irradiated diodes from 8-inch p-type silicon wafers

CERN(欧洲核子研究组织);Karlsruhe Institute of Technology(卡尔斯鲁厄理工学院);Heidelberg University(海德堡大学);Uppsala University(乌普萨拉大学);Al-Farabi Kazakh National University(阿尔法拉比哈萨克国立大学);An Najah National University(安纳贾赫国立大学);HAN University of Applied Sciences(汉应用科学大学)

Leena Diehl, Oliwia Kaluzinska, Marie Mühlnikel, Max Andersson, Natalya Gerassyova, Jenan Amer, Eva Sicking, Dana Groner, Jan Kieseler, Matteo Defranchis

AI总结:

研究中子辐照二极管在不同温度下的退火行为,利用电特性测量和电荷收集测量,提取退火时间常数,改进HL-LHC通量范围内的退火建模。

摘要:

为应对高亮度LHC期间集成亮度增加10倍导致的更高辐射水平,CMS探测器将用高粒度 calorimeter(HGCAL)概念取代当前的 calorimeter endcap(CE)。考虑到集成亮度为3ab⁻¹,CE的高辐射区域,预计通量在1×10¹⁴n_eq/cm²到1×10¹⁶n_eq/cm²之间,剂量最高达2MGy,将配备硅垫传感器。这包括整个电磁部分以及部分强子部分的CE。硅传感器是在8英寸p型晶圆上加工而成,厚度分别为300μm、200μm和120μm,并切割成六边形以充分利用整个晶圆面积和堆砌。每个主传感器上都搭载了多个小型测试结构(例如垫二极管),用于质量保证和辐射耐受性测试。为了研究辐射诱导的体损伤,这些二极管已通过JSI(约瑟夫·斯蒂芬研究所,斯洛文尼亚卢布尔雅那)的反应堆中子辐照至通量在5×10¹⁴n_eq/cm²到1.5×10¹⁶n_eq/cm²之间。本研究聚焦于不同温度(5.5°C至60°C)下体材料的等温退火行为,通过电特性测量和电荷收集测量进行研究。结果用于提取该材料和通量范围的退火时间常数,基于汉堡模型方法,以允许估计硅传感器在年底技术停机和长期HL-LHC停机期间的预期退火效应。所发现的退火参数将使HL-LHC通量范围内的p型硅探测器项目能够比现有汉堡模型更准确地建模退火行为。

英文摘要:

To face the higher levels of radiation due to the 10-fold increase in integrated luminosity during the High-Luminosity LHC, the CMS detector will replace the current Calorimeter Endcap (CE) using the High-Granularity Calorimeter (HGCAL) concept. The high-radiation regions of the the CE, where fluences between $1\cdot10^{14}~n_{eq}/cm^{2}$ and $1\cdot10^{16}~n_{eq}/cm^{2}$ and doses of up to 2\,MGy are expected considering an integrated luminosity of $3\,ab^{-1}$, will be equipped with silicon pad sensors. This includes the entire electromagnetic as well as parts of the hadronic section of the CE. The silicon sensors are processed on 8-inch p-type wafers with an active thickness of 300\,\textmu m, 200\,\textmu m and 120\,\textmu m and cut into hexagonal shapes for optimal use of the full wafer area and tiling. With each main sensor, several small test structures (e.g. pad diodes) are hosted on the wafers, used for quality assurance and radiation hardness tests. In order to investigate the radiation-induced bulk damage, these diodes have been irradiated with reactor neutrons at JSI (Jozef Stefan Institute, Ljubljana, Slovenia) to fluences between $5\cdot10^{14}~n_{eq}/cm^{2}$ and $1.5\cdot10^{16}~n_{eq}/cm^{2}$. This study focuses on the isothermal annealing behavior of the bulk material at different temperatures between 5.5°C and 60°C using electrical characterization and charge collection measurements. The results are used to extract the annealing time constants for this material and fluence range based on the Hamburg model approach to allow an estimation of the expected annealing effects in silicon sensors during the year-end technical stops and the long HL-LHC shutdowns. The annealing parameters found will make it possible to model the annealing behavior of p-type silicon detector projects at HL-LHC fluence ranges better than the existing Hamburg model.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑