arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2401.08320cond-mat.mtrl-sci
收藏

用于动态核极化的多孔硅纳米颗粒的可控合成与表征

Controlled synthesis and characterization of porous silicon nanoparticles for dynamic nuclear polarization

Gevin von Witte, Aaron Himmler, Viivi Hyppönen, Jiri Jäntti, Mohammed M. Albannay, Jani O. Moilanen, Matthias Ernst, Vesa-Pekka Lehto, Joakim Riikonen, Sebastia… 展开作者

Gevin von Witte, Aaron Himmler, Viivi Hyppönen, Jiri Jäntti, Mohammed M. Albannay, Jani O. Moilanen, Matthias Ernst, Vesa-Pekka Lehto, Joakim Riikonen, Sebastian Kozerke, Mikko I. Kettunen, Konstantin Tamarov

AI总结:

本文通过可控金属辅助刻蚀与热氧化制备不同掺杂的多孔硅纳米颗粒,揭示其DNP极化建立和衰减速率主要由$P_b$中心相关自旋扩散势垒决定,并实现75分钟弛豫与约6%核极化。

摘要:

硅纳米颗粒(NPs)作为一种超极化磁共振成像(MRI)造影剂已得到积极开发,其成像窗口接近一小时。然而,由于对与高效超极化建立和长极化衰减相对应的结构性质认识不足,NPs的开发进展受到阻碍。在本工作中,我们研究了单晶多孔硅(PSi)NPs的动态核极化(DNP),这些颗粒具有明确的掺杂密度,范围从名义上未掺杂到高浓度硼或磷掺杂。为开发此类PSi NPs,我们对电子级硅粉进行低负载金属辅助催化刻蚀,随后进行热氧化,以在Si/SiO$_2$界面形成悬挂键,即$P_b$中心。$P_b$中心是DNP所需未配对电子自旋的内禀来源。可控的制备和氧化程序使我们能够彻底研究磁场、温度和掺杂对DNP过程的影响。我们认为,在约10至60 nm之间,建立和衰减速率常数与硅晶体尺寸无关。相反,这些速率受到跨越核自旋扩散势垒的极化转移限制,该势垒由$P_b$中心中心$^{29}$Si核的大超精细位移决定。随后,对于低掺杂和中等掺杂硅,这种与尺寸无关的速率仅受到掺杂程度的微弱影响,尽管要实现最高极化需要轻微掺杂。因此,我们发现低硼掺杂PSi NPs的室温弛豫达到$75 \pm 3$分钟,并且在6.7 T和1.4 K下极化时,核极化水平超过约6%。因此,我们的研究为进一步开发硅NPs作为超极化造影剂奠定了坚实基础。

英文摘要:

Si nanoparticles (NPs) have been actively developed as a hyperpolarized magnetic resonance imaging (MRI) contrast agent with an imaging window close to one hour. However, the progress in the development of NPs has been hampered by the incomplete understanding of their structural properties that correspond to efficient hyperpolarization buildup and long polarization decays. In this work we study dynamic nuclear polarization (DNP) of single crystal porous Si (PSi) NPs with defined doping densities ranging from nominally undoped to highly doped with boron or phosphorus. To develop such PSi NPs we perform low-load metal-assisted catalytic etching for electronic grade Si powder followed by thermal oxidation to form the dangling bonds in the Si/SiO$_2$ interface, the $P_b$ centers. $P_b$ centers are the endogenous source of the unpaired electron spins necessary for DNP. The controlled fabrication and oxidation procedures allow us to thoroughly investigate the impact of the magnetic field, temperature and doping on the DNP process. We argue that the buildup and decay rate constants are independent of size of Si crystals between approximately 10 and 60 nm. Instead, the rates are limited by the polarization transfer across the nuclear spin diffusion barrier determined by the large hyperfine shift of the central $^{29}$Si nuclei of the $P_b$ centers. The size-independent rates are then weakly affected by the doping degree for low and moderately doped Si although slight doping is required to achieve the highest polarization. Thus, we find the room temperature relaxation of low boron doped PSi NPs reaching $75 \pm 3$ minutes and nuclear polarization levels exceeding $\sim 6$ % when polarized at 6.7 T and 1.4 K. Our study thus establishes solid grounds for further development of Si NPs as hyperpolarized contrast agents.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑