arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1612.04865cond-mat.mtrl-sciphysics.plasm-ph
收藏

Laser光照下多孔硅的结构、形貌和电学性能

Structural, Morphological and Electrical Properties of Porous Silicon Prepared Under Laser Illumination

Oday A. Al-Owaedi

摘要:

本文采用光电化学腐蚀方法在两种不同折射率(3.5)的n型硅晶片上制备了多孔硅(PSi)层 ohm.cm和0.02 ohm.cm)在24.5%浓度的氢氟酸(HF)中在不同的蚀刻时间(5至25分钟)下进行。辐照是使用2 W功率和810 nm波长的激光束实现的。利用X射线衍射(XRD)、扫描电子显微镜(SEM)和重量分析等技术研究了PSi层的形貌和结构特性。X射线衍射数据表明,随着刻蚀时间从5分钟增加到25分钟,PSi层的结构方面保持晶态,以及来自PSi层的X射线衍射角(θ B)(29度到26度)的减小和PSi结构的晶格参数值的增加,并且硅衬底的电阻率为0.02至3.5欧姆·厘米。随着刻蚀次数的增加和硅衬底电阻率的增加,纳米微晶的尺寸从20.72 nm减小到5.13 nm。SEM图像显示,孔宽度和PSi层厚度的值从孔壁厚度随刻蚀次数和衬底折射率的增加而变化,变化范围分别为0.5 ~ 6.25 μ m和6.7 ~ 47 μ m;孔壁厚度随刻蚀次数和衬底折射率的增加而变化,变化范围为1.25 ~ 0.03 μ m。随着蚀刻条件的变化,孔的孔形从圆柱形到矩形再到星形。随着刻蚀次数的增加和衬底电阻率的增加,多晶硅层的比表面积从7.43增加到235.35 m2/cm 3。

英文摘要:

Porous silicon (PSi) layers has been prepared in this work via photoelectrochemical (PEC) etching process of an n type silicon wafers of two resistivities (3.5 ohm.cm and 0.02 ohm.cm) in hydrofluoric (HF) acid of 24.5 precent concentration at different etching times (5 to 25 min). The irradiation has been achieved using laser beam of 2W power and 810 nm wavelength. We have studied the morphological and structural properties of PSi layers using the techniques of Xray Diffraction (XRD) and Scanning Electron Microscopy (SEM) and Gravimetric method. The Xray Diffraction data shows that the structure aspect of PSi layers remains crystalline as well as the decreasing of diffraction angle (thetaB) of Xray from PSi layers (29 to 26 degree) and increasing of the lattice parameter values of PSi structures with increasing of etching times from 5 to 25 min., and the resistivity of silicon substrates from 0.02 to 3.5 ohm.cm. The nanocrystallite size is decreasing from (20.72 to 5.13 nm) with increasing of etching times, and the resistivity of silicon substrates. The SEM images shows that the values of pore width and PSi layer thickness increases from (0.5 to 6.25 micrometer) and (6.7 to 47 micrometer) respectively with increasing of etching times and silicon substrates resistivities, while the values of the thickness of walls between pores has been varied from (1.25 to 0.03 micrometer) with increasing of etching times and silicon substrates resistivities. The pore shape of pores has been varied from Cylindrical to Rectangular and to Starful with varied of etching conditions. Further the measured specific surface area of PSi layers has been increased from (7.43 to 235.35 m2/cm3) with increasing of etching times and silicon substrates resistivities.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑