超导前体相SmFeAsO负热膨胀的证据

Evidence for negative thermal expansion in the superconducting precursor phase SmFeAsO

H. D. Zhou, P. M. Sarte, B. S. Conner, L. Balicas, C. R. Wiebe, X. H. Chen, T. Wu, G. Wu, R. H. Liu, H. Chen, D. F. Fang

摘要:

用高分辨粉末X射线散射研究了SmFeAsO $_{1-x}$ F $_x$(0 $\leq x \leq$ 0.10)系列掺氟稀土铁氧铌酸盐。与以前的研究一致,在T $\rm{_{S}}$ ~=~130~K时,母体化合物SmFeAsO表现出四方晶到正交晶的结构畸变,这种畸变被超导圆顶内0.10深处的$x \simeq$迅速抑制。在120 K时,晶胞对称性的改变伴随着以前未报道的磁弹性畸变.热膨胀系数$α_{V}$的温度依赖性揭示了SmFeAsO的丰富的相图:(i)在125 K的全球最小值对应于由泵浦探测飞秒光谱测量的自旋密度波不稳定性的开口,而(ii)在110 K的全球最大值对应于由磁性X射线散射测量的Sm和Fe亚晶格的磁有序。在比T $\rm{_{N}}$低得多的温度下,SmFeAsO表现出明显的负热膨胀,约为-40~ppm~ $\cdot$ ~K $^{-1}$,这与其他稀土氧铌酸盐如PrFeAsO和锕系氧铌酸盐NpFeAsO的行为相反,后者的$α<$ 0的起始只出现在磁有序附近.相关的电阻率和晶胞参数的温度和掺杂的依赖性,这一功能,我们解释的负热膨胀作为指示可能的凝结的巡回电子伴随着SDW间隙的开放,符合运输测量。

英文摘要:

The fluorine-doped rare-earth iron oxypnictide series SmFeAsO$_{1-x}$F$_x$ (0 $\leq x \leq$ 0.10) was investigated with high resolution powder x-ray scattering. In agreement with previous studies, the parent compound SmFeAsO exhibits a tetragonal-to-orthorhombic structural distortion at T$\rm{_{S}}$~=~130~K which is rapidly suppressed by $x \simeq$ 0.10 deep within the superconducting dome. The change in unit cell symmetry is followed by a previously unreported magnetoelastic distortion at 120~K. The temperature dependence of the thermal expansion coefficient $α_{V}$ reveals a rich phase diagram for SmFeAsO: (i) a global minimum at 125 K corresponds to the opening of a spin-density wave instability as measured by pump-probe femtosecond spectroscopy whilst (ii) a global maximum at 110 K corresponds to magnetic ordering of the Sm and Fe sublattices as measured by magnetic x-ray scattering. At much lower temperatures than T$\rm{_{N}}$, SmFeAsO exhibits a significant negative thermal expansion on the order of -40~ppm~$\cdot$~K$^{-1}$ in contrast to the behavior of other rare-earth oxypnictides such as PrFeAsO and the actinide oxypnictide NpFeAsO where the onset of $α<$ 0 only appears in the vicinity of magnetic ordering. Correlating this feature with the temperature and doping dependence of the resistivity and the unit cell parameters, we interpret the negative thermal expansion as being indicative of the possible condensation of itinerant electrons accompanying the opening of a SDW gap, consistent with transport measurements.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑