二步烧结法制备Ni4Nb2O9陶瓷及其相组成和显微结构

Fabrication, phase formation and microstructure of Ni4Nb2O9 ceramics by using two-stage sintering technique

Orawan Khamman, Jiraporn Jainumpone, Anucha Watcharapasorn, Supon Ananta

摘要:

采用两段烧结法制备高致密、高纯度的Ni_4Nb_2O_9陶瓷具有较低的烧成温度。采用X射线衍射(XRD)、阿基米德法和扫描电子显微镜(SEM)分别研究了烧结条件对陶瓷相形成、致密化和显微结构的影响。已经发现,根据烧结条件,铌酸盐NiNb 2 O 6的次要相倾向于与所需的Ni 4 Nb 2 O 9相一起形成。通过优化烧结条件,可得到单相正交相的Ni_4Nb_2O_9陶瓷。在950/1250 °C下复烧4 h,陶瓷的最大致密度为92%。在这两组烧结的Ni 4 Nb 2 O 9陶瓷中普遍发现具有更致密的角晶粒堆积的显微结构。但是,当样品在1050/1250 °C烧结时,晶粒形状不规则。两阶段烧结也被发现提高Ni 4 Nb 2 O 9陶瓷的铁电行为。

英文摘要:

The potential utilization of two-stage sintering for the production of highly dense and pure nickel diniobate (Ni4Nb2O9) ceramics with low firing temperature was demonstrated. Effects of designed sintering conditions on phase formation, densification and microstructure of the ceramics were characterized by X-ray diffraction (XRD), Archimedes method and scanning electron microscopy (SEM), respectively. It has been found that minor phase of columbite NiNb2O6 tended to form together with the desired Ni4Nb2O9 phase, depending on sintering conditions. The optimization of sintering conditions could lead to a single-phase Ni4Nb2O9 ceramics with orthorhombic structure. The ceramics doubly sintered at 950/1250 °C for 4 h exhibited maximum density value of 92%. Microstructures with denser angular grain-packing were generally found in both sets of the sintered Ni4Nb2O9 ceramics. However, the grains were irregular in shape when the samples are sintered at 1050/1250 °C. Two-stage sintering was also found to enhance ferroelectric behavior of Ni4Nb2O9 ceramic.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑