溅射用烧结BFO靶材
Sintering BFO targets for sputtering
摘要:
在$880^OC$中通过快速烧结制备陶瓷$BiFeO_{3}$样品。检查了两种组合物。一种$56/44\ Bi_{2}O_{3}/Fe_{2}O_{3}\ mole\%$组合物和一种$56Bi_{2}O_{3}\cdot44Fe_{2}O_{3}+6.5wt\%\,NaCl$组合物。将样品在不同时间热处理至多$8$分钟,并使用XRD测量和分析来检查相含量作为时间的函数。已经证明,使用两种组合物,在$3.5$分钟后获得最大的$BiFeO_{3}$相含量。在前者中,材料的大约$50\%$转化为$BiFeO_{3}$,而在后者中为$98.5\%$。
英文摘要:
Ceramic $BiFeO_{3}$ samples were prepared by rapid sintering at $880^OC$. Two compositions were examined. A $56/44\ Bi_{2}O_{3}/Fe_{2}O_{3}\ mole\%$ composition and a $56Bi_{2}O_{3}\cdot44Fe_{2}O_{3}+6.5wt\%\,NaCl$ composition. The samples were heat treated at different times up to $8$ minutes and the phase content was examined as a function of the time using XRD measurements and analysis. It was demonstrated that using both compositions, maximum $BiFeO_{3}$ phase content is obtained after $3.5$ minutes. In the former approximately $50\%$ of the material transformed to $BiFeO_{3}$ while in the latter $98.5\%$.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。