通过溶胶-凝胶法结合喷雾沉积与近红外烧结原位烧结制备NASICON(Na$_3$Zr$_2$(SiO$_4$)$_2$PO$_4$)陶瓷薄膜的新方法

New approach for obtaining ceramic NASICON (Na$_3$Zr$_2$ (SiO$_4$)$_2$PO$_4$) films sintered in situ by a sol-gel method, using spray deposition and Near-Infra Red Sintering

Rafael Marti Valls, Rebecca Griffin, Anne Sawhney, Celina Domingos-Dlofo, Tom Dunlop, Sam Reis, Peter J. Holliman, Jenny Baker

AI总结:

本研究提出一种结合溶胶-凝胶喷雾沉积与近红外超快烧结的新方法,首次在约1000℃高温下原位制备出NASICON陶瓷薄膜,大幅缩短了制造时间。

摘要:

本研究展示了一种在熔融石英基底上原位烧结的NASICON薄膜。该制备方法结合了喷雾涂覆的溶胶-凝胶溶液与近红外(NIR)超快烧结技术,大幅缩短了制造时间。这是首次在约1000$^\text{circ}$C的高温下实现近红外烧结陶瓷的演示。

英文摘要:

In this work we demonstrate a NASICON film sintered in situ onto a fused silica substrate. This production method drastically reduces the manufacturing time by combining the use of a spray-coated sol-gel solution and near-infrared (NIR) ultrafast sintering technology. The first demonstration of NIR sintered ceramics at high temperatures (~1000$^\circ$C).