摘要:

采用放电等离子烧结(SPS)方法制备了磷钇矿结构陶瓷。通过溶胶-凝胶法获得磷酸盐Y $_{0.95}$ Gd $_{0.05}$ PO $_4$(YPO $_4$:Gd)。将合成的纳米粉末收集在尺寸为10-50 mkm的大团聚体中。陶瓷具有细晶粒显微结构和高相对密度(98.67%)。SPS过程的总时间约为18分钟。高密度烧结陶瓷YPO $_4$:Gd与磷钇矿结构的照射与$^{+26}$离子(E = 167 MeV)的能量密度的$1\times10^{12}$ - $3\times 10^{13}$ cm $^{-2}$。在最大能量密度下未实现完全非晶化。随着注量的增加,观察到的非晶层的深度的一个微不足道的增加。根据掠入射XRD(GIXRD)的结果,随着能量密度从$1\times10^{12}$ - $3\times 10^{13}$ cm $^{-2}$增加,观察到非晶结构的体积分数从20%增加到70%。在恢复退火(700 $^\circ$ C,18小时)后,XRD峰200 YPO $_4$:Gd的强度达到初始强度I 0的~80%的值。

英文摘要:

The paper reports on the preparation of xenotime-structured ceramics by the Spark Plasma Sintering (SPS) method. Phosphates Y$_{0.95}$Gd$_{0.05}$PO$_4$ (YPO$_4$:Gd) were obtained by the sol-gel method. The synthesized nanopowders are collected in large agglomerates 10-50 mkm in size. Ceramics has a fine-grained microstructure and a high relative density (98.67%). The total time of the SPS process was approximately 18 min. High-density sintered ceramics YPO$_4$:Gd with a xenotime structure were irradiated with Xe$^{+26}$ ions (E = 167 MeV) to fluences of $1\times10^{12}$-$3\times 10^{13}$ cm$^{-2}$. Complete amorphization at maximum fluence was not achieved. As the fluence increases, an insignificant increase in the depth of the amorphous layer is observed. According to the results of grazing incidence XRD (GIXRD), with an increase in fluence from $1\times10^{12}$-$3\times 10^{13}$ cm$^{-2}$, an increase in the volume fraction of the amorphous structure from 20 to 70% is observed. The intensity of XRD peak 200 YPO$_4$:Gd after recovery annealing (700$^\circ$C, 18 h) reached a value of ~80% of the initial intensity I0.