Composite cathode coatings made of a high energy density layered oxide (Li1.2Ni0.15Mn0.55Co0.1O2, theoretical capacity ~377 mAh/g), polyvinylidene fluoride (PVdF) binder, and electron-conduction additives, were bonded to an elastic substrate. An electrochemical cell, built by pairing the cathode with a capacity-matched graphite anode, was electrochemically cycled and the real-time average stress evolution in the cathode coating was measured using a substrate-curvature technique. Features in the stress evolution profile showed correlations with phase changes in the oxide, thus yielding data complementary to in situ XRD studies on this material. The stress evolution showed a complex variation with lithium concentration suggesting that the volume changes associated with phase transformations in the oxide are not monotonically varying functions of lithium concentration. The peak tensile stress in the cathode during oxide delithiation was approximately 1.5 MPa and the peak compressive stress during oxide lithiation was about 6 MPa. Stress evolution in the anode coating was also measured separately using the same technique. The measured stresses are used to estimate the internal pressures that develop in a cylindrical lithium-ion cell with jelly-roll electrodes.
Impact of Surface Chemistry of Silicon Nanoparticles on the Structural and Electrochemical Properties of Si/Ni3.4Sn4 Com-posite Anode for Li-Ion Batteries
Film strains enhance the reversible cycling of intercalation electrodes
电池电极中化学机械降解的关键原因是它们在充电/放电循环期间经历突然的相变。这种相变伴随着晶格失配应变,晶格失配应变使微裂纹成核,诱导断裂,并且在极端情况下使插层电极非晶化。在这项工作中,我们提出了一种策略,以防止化学机械降解的嵌入电极:我们表明,通过工程合适的薄膜应变,我们可以调节薄膜嵌入电极的相变和规避大的体积变化。我们使用理论和实验的结合来测试这种策略:我们首先分析得出薄膜应变对薄膜插层电极的电化学响应的影响,然后将我们的分析模型应用于一个有代表性的例子(具有多个相变的LixV 2 O 5)。然后我们用实验来检验我们的理论预测。具体来说,我们电化学循环薄膜V2 O 5电极与不同的膜应变和测量它们的结构,电压和应力响应。我们的研究结果表明,拉伸膜应变降低了薄膜V2 O 5电极中相变的电压,并促进其在更宽的电压窗口内的可逆循环,而不会发生化学机械降解。这些结果表明,薄膜应变工程是一种替代的方法,以防止化学机械降解嵌入电极。除了薄膜电极之外,我们的研究结果也适用于研究基于颗粒的电极和阴极颗粒上形成的薄表面层中的应力诱导相变。
Insights on the volume variation of LiCoxMn2-xO4 electrode upon cycling: a correlative operando XRD and XAS study
Sorbonne Université, CNRS, Physicochimie des Electrolytes et Nanosystèmes interfaciaux (PHENIX)(索邦大学,法国国家科学研究中心,电解质与界面纳米系统物理化学);Sorbonne Université, CNRS, Laboratoire de Chimie de la Matière Condensée de Paris (LCMCP)(索邦大学,法国国家科学研究中心,巴黎凝聚态物质化学实验室);Réseau sur le Stockage Electrochimique de l’Energie (RS2E), FR CNRS 3459(电化学储能研究网络(RS2E),FR CNRS 3459)
BaMF$_4$ (M = Mn, Co, Ni): New Electrode Materials for Hybrid Supercapacitor with Layered Polar Structure
为了追求基于具有氧化还原反应或吸附/脱附效应的法拉第电荷转移的超级电容器的高电化学性能,电解质离子到电极材料中的嵌入效率是具有额外体积贡献的超过纯表面容量的关键先决条件。在这里,我们报告了层状钡过渡金属氟化物,BaMF_4(M = Mn,Co,Ni)是一系列新的电极材料应用于标准的三电极配置。得益于电解质离子的有效浸润,这些材料具有显著的比电容。电化学表征表明,BaMF 4电极在循环伏安图中既表现出电容行为,又表现出法拉第氧化还原反应,并具有良好的充放电循环储电能力和循环稳定性。特别是BaCoF_4在电流密度为0.6 A g ~(-1)时,其比电容最高,达到360 F g ~(-1),即使其颗粒尺寸远远超过纳米级。此外,第一性原理计算揭示了可能的潜在机制。
Favorable Interfacial Chemomechanics Enables Stable Cycling of High Li-Content Li-In/Sn Anodes in Sulfide Electrolyte Based Solid-State Batteries
固态电池(SSB)可以在电池安全性和能量密度方面提供范式转变。然而,这一前景取决于将高性能电极与最先进的固体电解质集成的能力。例如,锂(Li)金属,最高能量密度的阳极候选者,遭受导致电池故障的严重界面化学机械问题。In/Sn的Li合金是有吸引力的替代品,但它们的开发主要限于低容量(低Li含量)和富In的Li $_x$ In(x $\leq$ 0.5)。在这里,基本的电化学机械行为的Li-In和Li-Sn合金的不同Li化学计量是解开硫化物电解质为基础的SSB。通过控制合成和制造技术开发的金属间化合物电极显示出令人印象深刻的(电)化学稳定性,其中Li $_6$ PS $_5$ Cl作为固体电解质,并且在电化学Li插入/脱嵌期间在最佳堆叠压力下保持近乎完美的界面接触。通过计算和电化学研究的结合,揭示了它们在锂迁移势垒随组成的有趣变化及其对观察到的锂循环过电位的影响。合金的稳定界面化学力学允许在相对高的电流密度(1 mA cm $^{-2}$)和容量(1 mAh cm $^{-2}$)下的长期无枝晶Li循环(>1000 h),如对于Li $_{13}$ In $_3$和Li $_{17}$ Sn $_4$所证明的,与低Li含量类似物相比,从容量和成本考虑,这是更期望的。这些认识对锂离子电池用高容量Li-In/Sn合金阳极的开发具有指导意义。
Operando Characterization of Volume Changes in Lithium-Ion Battery Electrodes during Cycling using Isotope Multilayers
Clausthal University of Technology(克莱斯特大学);Clausthal Center for Materials Technology(克莱斯特材料技术中心);Center for Neutron and Muon Sciences, Paul Scherer Institute(保罗谢勒研究所中子与缪子科学中心)
Electrochemical properties of Na$_{0.66}$V$_4$O$_{10}$ nanostructures as cathode material in rechargeable batteries for energy storage applications
我们报道了Na $_{0.66}$ V $_4$ O $_{10}$纳米结构作为可充电电池阴极材料的电化学性能。室温X射线衍射图的Rietveld精修显示具有C2/m空间群的单斜相。所制备的半电池的循环伏安曲线在~3.1和2.6~V处呈现氧化还原峰,这是由于V $^{5+/4+}$之间的两相转变反应,并且可以归属于Na离子的单步脱嵌/嵌入。我们观察到良好的循环稳定性,在电流密度为3和50 mA g $^{-1}$下,放电比容量(相对于Na $^+$ /Na测量)分别在80($\pm$ 2)和30($\pm$ 2)mAh g $^{-1}$之间。还用Li阳极测试了Na $_{0.66}$ V $_4$ O $_{10}$电极的电化学性能,其显示出比Na更高的容量,但衰减更快。利用密度泛函理论,我们计算了Na空位的形成能;在材料的本体中为3.37~eV,在(100)表面上为2.52~eV,这强调了纳米结构的重要性。
Investigations on the improved cycling stability of Kazakhstanite phase Fe-V-O layered oxide by using superconcentrated electrolytes: Generalized solubility limit approach (Part I)
Unraveling the storage mechanism of Na$_{3}$V$_{2-x}$Ni$_x$(PO$_4$)$_2$F$_3$/C cathodes for sodium-ion batteries through electrochemical, {\it operando} X-ray diffraction and microscopy studies
Indian Institute of Technology Delhi(印度理工学院德里分校);National Yang Ming Chiao Tung University(国立阳明交通大学);Chung Yuan Christian University(中原大学)
本研究结合 EIS、GITT、CV、operando XRD 与原位同步辐射 TXM,揭示 Ni 掺杂 Na₃V₂(PO₄)₂F₃/C 正极的储钠机制、扩散动力学及长循环稳定性。
Performance Classification and Remaining Useful Life Prediction of Lithium Batteries Using Machine Learning and Early Cycle Electrochemical Impedance Spectroscopy Measurements
Quantifying Phase Transformations in Alloying Anodes via In-Situ Liquid Cell Hard X-ray Spectroscopy and Cryogenic Microscopy
Imperial College London(帝国理工学院);Diamond Light Source(钻石光源);Max-Planck Institute for Sustainable Materials(马克斯·普朗克可持续材料研究所);Univ Rouen Normandie, CNRS, INSA Rouen Normandie, Groupe de Physique des Matériaux, UMR 6634(鲁昂诺曼底大学、法国国家科学研究中心、鲁昂诺曼底国立应用科学学院、材料物理研究组)
Mixed Polyanionic NaFe$_{1.6}$V$_{0.4}$(PO$_{4}$)(SO$_{4}$)$_{2}$@CNT Cathode for Sodium-ion Batteries: Electrochemical Diffusion Kinetics and Distribution of Relaxation Time Analysis at Different Temperatures
Nanostructuring Strategies for Silicon-based Anodes in Lithium-ion Batteries: Tuning Areal Silicon Loading, SEI Formation/Irreversible Capacity Loss, Rate Capability Retention and Electrode Durability
硅是锂离子电池最有前途的负极材料之一。硅在循环时承受体积变化,这导致随后的粉化和容量衰减。这些缺点导致寿命差,并阻碍了硅阳极的商业化。在这项工作中,基于硅纳米颗粒(SiNPs)锚定在垂直排列的碳纳米管(VACNTs)与定义的间距,以适应体积变化的混合纳米结构阳极合成的商业宏观集流体。实现具有良好稳定性和优异电化学性能的电极仍然是一个挑战。因此,我们在本文中通过在固定的VACNT毯状物长度下改变硅沉积时间来调节SiNP体积,或者通过在固定的SiNP体积下改变VACNT长度来调节活性硅面积负载。SiNP的低面积负载改善了循环期间的容量稳定性,但由于形成了固体电解质界面(SEI)层而引发了大的不可逆容量损失。相比之下,较高的面积负载电极减少了所形成的SEI的量,但是在随后的循环期间负面地影响电极的容量稳定性。通过增加VACNTs毯状物长度而不损害循环稳定性来实现硅的更高重量容量和更高面积负载质量。该混合纳米结构电极显示出优异的稳定性,在2000次循环后可逆容量为1330 mAh g-1。
Thermal conductivity of intercalation, conversion, and alloying lithium-ion battery electrode materials as function of their state of charge
在插入和取出锂时,对于电化学能量储存重要的材料可以经历热导率($Λ$)和弹性模量($\it M$)的变化。这些变化是由于演化的固有的热载流子寿命和原子间的键合强度与电极材料的结构转变具有不同程度的可逆性。利用原位时域热反射技术和皮秒声学技术,系统研究了电极材料在循环过程中的转化、嵌入和合金化过程中的$Λ$和$\it M$。插层V $_{2}$ O $_{5}$和TiO $_{2}$表现出非单调可逆$Λ$和$\it M$切换高达1.8倍($Λ$)和1.5倍($\it M$)作为锂含量的函数。在第一次锂化时,转化的Fe $_{2}$ O $_{3}$和NiO在$Λ$和$\it M$中经历不可逆衰变。合金化Sb显示出$Λ$在脱锂状态(18 W m $^{-1}$ K $^{-1}$)和锂化状态(<1 W m $^{-1}$ K $^{-1}$)之间的最大和部分可逆的数量级的量值切换。不可逆的$Λ$归因于循环过程中大量体积变化导致的结构降解和粉碎。这些发现为电池设计的重要性循环过程中电极材料的热和机械性能演变提供了新的理解,并且还指出了形成具有热切换性能的材料的途径。
Competing redox and material redistribution during electrode ageing
Stanford University(斯坦福大学);Lawrence Berkeley National Laboratory(劳伦斯伯克利国家实验室);University of California, Los Angeles(加州大学洛杉矶分校);SLAC National Accelerator Laboratory(SLAC国家加速器实验室);University of California, Berkeley(加州大学伯克利分校)