Pr3Rh4Sn13-type、Yb3Co4Ge13和Yb3Co4Sn13化合物的热电性能

Thermoelectric properties of Pr3Rh4Sn13-type Yb3Co4Ge13 and Yb3Co4Sn13 compounds

A. V. Morozkin, V. Yu. Irkhin, V. N. Nikiforov

摘要:

报道了Yb_3Co_4Ge_(13)、Yb_3Co_4Sn_(13)、Yb_2CeCo_4Ge_(13)和Yb_2.3La_(0.7)Co_4Ge_(13)固溶体的晶体学数据和热电性能(240 ~ 380 K)。所有化合物的Seebeck系数、电阻和热导率在240 ~ 380 K范围内均随温度的升高而单调增加。Yb_3Co_4Sn_(13)的塞贝克系数S = 14 - 27 μV//K,Yb_3Co_4Ge_(13)的塞贝克系数S = -21 - -12 μV/K。Yb取代Yb_3Co_4Ge_(13)中的铈或镧使Seeebeck系数变为正值。Yb_3Co_4Sn_1_3具有Pr_3Rh_4Sn_1_3型化合物中最大的ZT参数。在240 ~ 380 K温度范围内,Yb 3Co 4Sn 13化合物的ZT参数从0.006增加到0.017。

英文摘要:

Crystallographic data and thermoelectric properties (from 240 K up to 380 K) of Yb3Co4Ge13, Yb3Co4Sn13 compounds and Yb2CeCo4Ge13 and Yb2.3La0.7Co4Ge13 solid solutions are reported. The Seebeck coefficients, electric resistance and thermal conductivity increase monotonically with increasing temperature from 240 to 380 K for all the compounds. The Seebeck coefficient is S = 14 - 27 μV//K for Yb3Co4Sn13, and S = -21 -- -12 μV/K for Yb3Co4Ge13. The substitution of Yb for cerium or lanthanum in Yb3Co4Ge13 shifts the Seeebeck coefficient to positive values. The Yb3Co4Sn13 has a maximal ZT parameter from available Pr3Rh4Sn13-type compounds. The ZT parameter of Yb3Co4Sn13 compound increases from 0.006 up to 0.017 with increasing temperature from 240 K to 380 K.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑