双交叉束PLD制备BiFeO3-BiCrO3薄膜及其结构与性能

Growth, Structure and Properties of BiFeO3-BiCrO3 Films obtained by Dual Cross Beam PLD

R. Nechache, C. Harnagea, L. Gunawan, L. -P. Carignan, C. Maunders, D. Menard, G. A. Botton, A. Pignolet

摘要:

最近通过脉冲激光沉积合成的外延Bi 2FeCrO 6薄膜的性质部分证实了理论预测(即,磁矩为2 μ B/分子式单位,0 K时的极化为~80 μ C/cm 2)。这种材料在室温下存在磁有序是一个意想不到的,但非常有前途的结果,需要进一步研究。由于磁性被认为是由Fe和Cr阳离子之间的交换相互作用引起的,因此磁性行为强烈依赖于它们的有序性和它们之间的距离。我们在这里提出了成功的合成外延Bi 2FexCryO 6(BFCO x/y)薄膜生长在SrTiO 3衬底上使用双交叉束脉冲激光沉积。薄膜的晶体结构取决于沉积条件而具有不同类型的(111)取向超结构。在室温下,BFCO(x/y)薄膜的铁电和磁滞的存在证明了其多铁性。Fe和Cr离子在薄膜中的氧化态仅为3+,并且宏观磁化强度与Fe/Cr比组成的差异只能是由于Cr 3+和Fe 3+阳离子的有序化,因此它们之间的交换相互作用的改变。

英文摘要:

The properties of epitaxial Bi2FeCrO6 thin films, recently synthesized by pulsed laser deposition, have partially confirmed the theoretical predictions (i.e. a magnetic moment of 2 muB per formula unit and a polarization of ~80 microC/cm2 at 0K). The existence of magnetic ordering at room temperature for this material is an unexpected but very promising result that needs to be further investigated. Since magnetism is assumed to arise from the exchange interaction between the Fe and Cr cations, the magnetic behaviour is strongly dependent on both their ordering and the distance between them. We present here the successful synthesis of epitaxial Bi2FexCryO6 (BFCO x/y) films grown on SrTiO3 substrates using dual crossed beam pulsed laser deposition. The crystal structure of the films has different types of (111)-oriented superstructures depending on the deposition conditions. The multiferroic character of BFCO (x/y) films is proven by the presence of both ferroelectric and magnetic hysteresis at room temperature. The oxidation state of Fe and Cr ions in the films is shown to be 3+ only and the difference in macroscopic magnetization with Fe/Cr ratio composition could only be due to ordering of the Cr3+ and Fe3+ cations therefore to the modification of the exchange interaction between them.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑