球磨法制备$La_{0.67}Ca_{0.33}MnO_3$(D = Ca,Sr,Ba)锰氧化物的结构和磁性

Structural and magnetic properties of $La_{0.67}Ca_{0.33}MnO_3$ (D = Ca, Sr, Ba) manganites prepared by Ball milling

Sami Mahmood, Haneen Badran, Eman Al-Hwaitat, Ibrahim Bsoul, Rola bqaeen

摘要:

在这项研究中,我们报告了$La_{0.67}Ca_{0.33}MnO_3$(LCMO),$La_{0.67}Ba_{0.33}MnO_3$(LBMO)和$La_{0.67}Sr_{0.33}MnO_3$(LSMO)钙钛矿的合成和表征。采用球磨技术制备了钙钛矿样品的前驱体粉末。将所得粉末压制成圆盘,随后在1000 ℃下烧结2小时。采用X射线衍射(XRD)和扫描电子显微镜(SEM)对样品的结构进行了表征,采用振动样品磁强计(VSM)对样品的磁性能进行了研究。LCMO样品的XRD图谱显示具有Pnma空间群的纯钙钛矿相,而LSMO样品的XRD图谱显示具有R3 c $^-$空间群的纯钙钛矿相。然而,LBMO样品的XRD图谱表明存在具有R3 c $^-$对称性的主要钙钛矿相以及次要$BaMnO_3$相。当在1100 ℃的较高温度下烧结LBMO时,该第二相消失。等温磁性测量和热磁曲线表明,LCMO在室温下是顺磁性的。然而,LSMO在室温下表现出软铁磁行为,Tc = 380 K,Ms = 50.9 emu/g。1000 ℃烧结的LBMO样品在室温下表现出软铁磁性,居里温度Tc = 343 K,饱和磁化强度Ms = 30.7 emu/g。LBMO化合物的较高烧结温度导致饱和磁化强度显著增加,在1100 ℃烧结的样品的饱和磁化强度达到50.8emu/g。

英文摘要:

In this research, we report on the synthesis and characterization of $La_{0.67}Ca_{0.33}MnO_3$ (LCMO), $La_{0.67}Ba_{0.33}MnO_3$ (LBMO), and $La_{0.67}Sr_{0.33}MnO_3$ (LSMO) perovskites. Precursor powders for the perovskite samples were prepared using ball mailing technique. The resulting powder was pressed into disks which were subsequently sintered at 1000 C for 2h. The structural characteristics of the prepared samples were investigated using X-ray diffraction (XRD) and scanning electron microscope (SEM), and the magnetic properties were investigated using vibrating sample magnetometry (VSM). XRD pattern of LCMO sample revealed a pure perovskite phase with Pnma space group, while the pattern of LSMO sample revealed a pure perovskite with R3c$^-$ space group. XRD pattern of LBMO sample, however, demonstrated the presence of a major perovskite phase with R3c$^-$ symmetry, together with a secondary $BaMnO_3$ phase. This secondary phase disappeared upon sintering LBMO at a higher temperature of 1100 C. Isothermal magnetic measurements and thermomagnetic curves revealed that LCMO was paramagnetic at room temperature. However, LSMO exhibited soft ferromagnetic behavior at room temperature, with Tc = 380 K and Ms = 50.9 emu/g. Also, LBMO sample sintered at 1000 C exhibited soft ferromagnetic behavior at room temperature, with Curie temperature Tc = 343 K and a rather low saturation magnetization of Ms = 30.7 emu/g. The higher sintering temperature of LBMO compound resulted in a significant increase of the saturation magnetization to 50.8 emu/g for the sample sintered at 1100 C.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑