Fe-Cr合金系800 K下的可熔性间隙

On the miscibility gap at 800 K in the Fe-Cr alloy system

Stanislaw M. Dubiel, Jan Zukrowski

摘要:

本文用穆斯堡尔效应谱研究了Fe_(73.7)Cr_(26.3)合金在800 K下的相分解动力学和相边界。的动力学被揭示,以及遵循约翰逊-梅尔-阿夫拉米-Kolgomarov方程证明的成核和生长机制的分解。Cr在Fe基体中的溶解极限被确定为17.3(6)at.% Fe在Cr基体中的含量为18.5(9)at.%。所得结果与各种理论预测进行了比较。

英文摘要:

Issues pertinent to the miscibility gap at 800K in a Fe73.7Cr26.3 alloy viz. the kinetics of the phase decomposition and borders of the latter were investigated by means of the Mössbauer-effect spectroscopy. The kinetics was revealed to well follow the Johnson-Mehl-Avrami-Kolgomarov equation testifying to a nucleation and growth mechanism underlying the decomposition. A solubility limit of Cr in the Fe matrix was determined to be 17.3(6) at.% and that of Fe in the Cr matrix was found as equal to 18.5(9) at.%. The results obtained have been compared with various theoretical predictions.