arXiv 1609.05431cond-mat.mtrl-sci
收藏

位错退火动力学及氢陷阱效应的原位衍射研究

Kinetics of dislocation annealing and the effect of trapped hydrogen, investigated with in-situ diffraction

T. A. Webb, C. J. Webb, C. V. Tapia-Bastidas, E. MacA. Gray

摘要:

原位粉末衍射被用来研究原型氢吸收剂Pd和LaNi 5中位错的退火。利用热诱导脱附探讨了位错与俘获氢之间的关系。发现Pd中的位错是由氢吸收在宽温度范围内退火引起的,并且尽管它们在低于250 $^\circ$ C时开始退火,但是需要远高于750 $^\circ$ C的温度来完全退火金属。结果表明,在较低温度下允许进一步的时间不会进一步退火金属。有人认为,这是由于位错缠结和钉扎,导致不同的钉扎缺陷需要不同的温度。结果发现,在LaNi 5中捕获的氢在很宽的温度范围内被释放,因此得出结论,氢被捕获在位错应变场和位错核以及空位中。氘释放和位错密度的直接比较显示没有相关性,与以前的间接比较。LaNi 5中的位错在低至150 $^\circ$ C的温度下退火,与先前的报告相反,先前的报告建议需要超过500 $^\circ$ C。这种较低的位错退火温度至少部分地解释了为什么低温老化会增加氢循环LaNi 5中的压力滞后。

英文摘要:

In-situ powder diffraction was used to study the annealing of dislocations in the archetypal hydrogen absorbers Pd and LaNi5. The relationship between dislocations and trapped hydrogen was explored using thermally induced desorption. It was found that the dislocations in Pd caused by hydrogen absorption anneal over a wide range of temperatures and that although they start to anneal below 250 $^\circ$C, temperatures well above 750 $^\circ$C are required to fully anneal the metal. It was shown that allowing further time at lower temperatures does not further anneal the metal. It is suggested that this is due to dislocation tangling and pinning, causing different temperatures to be required for different pinning defects. It was found that hydrogen trapped in LaNi5 is released in a wide range of temperatures and it was therefore concluded that hydrogen is trapped in the dislocation strain field and dislocation core as well as vacancies. The direct comparison of deuterium release and dislocation density showed no correlation, in agreement with previous indirect comparisons. Dislocations in LaNi5 were shown to anneal at temperatures as low as 150 $^\circ$C, in contrast to previous reports which suggested more than 500 $^\circ$C was required. This lower annealing temperature for dislocations at least partly explains why low temperature ageing increases the pressure hysteresis in hydrogen cycled LaNi5.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑