arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1503.05906cond-mat.mtrl-sci
收藏

LaAlO $_3$ / SrTiO $_3$界面生长诱导电子迁移率增强

Growth-induced electron mobility enhancement at the LaAlO$_3$/SrTiO$_3$ interface

A. Fête, C. Cancellieri, D. Li, D. Stornaiuolo, A. D. Caviglia, S. Gariglio, J. -M. Triscone

摘要:

研究了在不同生长温度下制备的LaAlO $_3$ /SrTiO $_3$界面二维电子液体的电子性质。我们观察到在650°C下制备的界面表现出最高的低温迁移率($\approx 10000 \textrm{ cm}^2/\textrm{Vs}$)和最低的片状载流子密度($\approx 5\times 10^{12} \textrm{ cm}^{-2}$)。这些样品表现出金属行为和Shubnikov-de Haas振荡的磁阻。在较高温度(800-900°C)下生长的样品显示出在$\approx 2-5 \times 10^{13} \textrm{ cm}^{-2}$范围内的载流子密度和在4K下的$\approx 1000 \textrm{ cm}^2/\textrm{Vs}$的迁移率。通过场效应将它们的载流子密度降低到$8\times 10^{12} \textrm{ cm}^{-2}$,使它们的迁移率降低到$\approx 50 \textrm{ cm}^2/\textrm{Vs}$,从而使电导达到弱局域化状态。

英文摘要:

We have studied the electronic properties of the 2D electron liquid present at the LaAlO$_3$/SrTiO$_3$ interface in series of samples prepared at different growth temperatures. We observe that interfaces fabricated at 650°C exhibit the highest low temperature mobility ($\approx 10000 \textrm{ cm}^2/\textrm{Vs}$) and the lowest sheet carrier density ($\approx 5\times 10^{12} \textrm{ cm}^{-2}$). These samples show metallic behavior and Shubnikov-de Haas oscillations in their magnetoresistance. Samples grown at higher temperatures (800-900°C) display carrier densities in the range of $\approx 2-5 \times 10^{13} \textrm{ cm}^{-2}$ and mobilities of $\approx 1000 \textrm{ cm}^2/\textrm{Vs}$ at 4K. Reducing their carrier density by field effect to $8\times 10^{12} \textrm{ cm}^{-2}$ lowers their mobilites to $\approx 50 \textrm{ cm}^2/\textrm{Vs}$ bringing the conductance to the weak-localization regime.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑