Cycling efficiency and rate capability of porous copper-coated, amorphous silicon thin-film negative electrodes are compared to equivalent silicon thin-film electrodes in lithium-ion batteries. The presence of a copper layer coated on the active material plays a beneficial role in increasing the cycling efficiency and the rate capability of silicon thin-film electrodes. Between 3C and C/8 discharge rates, the available cell energy decreased by 8% and 18% for 40 nm copper-coated silicon and equivalent silicon thin-film electrodes, respectively. Copper-coated silicon thin-film electrodes also show higher cycling efficiency, resulting in lower capacity fade, than equivalent silicon thin-film electrodes. We believe that copper appears to act as a glue that binds the electrode together and prevents the electronic isolation of silicon particles, thereby decreasing capacity loss. Rate capability decreases significantly at higher copper-coating thicknesses as the silicon active-material is not accessed, suggesting that the thickness and porosity of the copper coating need to be optimized for enhanced capacity retention and rate capability in this system.
Impact of Surface Chemistry of Silicon Nanoparticles on the Structural and Electrochemical Properties of Si/Ni3.4Sn4 Com-posite Anode for Li-Ion Batteries
Favorable Interfacial Chemomechanics Enables Stable Cycling of High Li-Content Li-In/Sn Anodes in Sulfide Electrolyte Based Solid-State Batteries
固态电池(SSB)可以在电池安全性和能量密度方面提供范式转变。然而,这一前景取决于将高性能电极与最先进的固体电解质集成的能力。例如,锂(Li)金属,最高能量密度的阳极候选者,遭受导致电池故障的严重界面化学机械问题。In/Sn的Li合金是有吸引力的替代品,但它们的开发主要限于低容量(低Li含量)和富In的Li $_x$ In(x $\leq$ 0.5)。在这里,基本的电化学机械行为的Li-In和Li-Sn合金的不同Li化学计量是解开硫化物电解质为基础的SSB。通过控制合成和制造技术开发的金属间化合物电极显示出令人印象深刻的(电)化学稳定性,其中Li $_6$ PS $_5$ Cl作为固体电解质,并且在电化学Li插入/脱嵌期间在最佳堆叠压力下保持近乎完美的界面接触。通过计算和电化学研究的结合,揭示了它们在锂迁移势垒随组成的有趣变化及其对观察到的锂循环过电位的影响。合金的稳定界面化学力学允许在相对高的电流密度(1 mA cm $^{-2}$)和容量(1 mAh cm $^{-2}$)下的长期无枝晶Li循环(>1000 h),如对于Li $_{13}$ In $_3$和Li $_{17}$ Sn $_4$所证明的,与低Li含量类似物相比,从容量和成本考虑,这是更期望的。这些认识对锂离子电池用高容量Li-In/Sn合金阳极的开发具有指导意义。
Theoretical Studies on Sodium Storage Mechanism in Hard Carbon Anodes of Sodium-Ion Batteries: Molecular Simulations Based on Machine Learning Force Fields
Nanostructuring Strategies for Silicon-based Anodes in Lithium-ion Batteries: Tuning Areal Silicon Loading, SEI Formation/Irreversible Capacity Loss, Rate Capability Retention and Electrode Durability
硅是锂离子电池最有前途的负极材料之一。硅在循环时承受体积变化,这导致随后的粉化和容量衰减。这些缺点导致寿命差,并阻碍了硅阳极的商业化。在这项工作中,基于硅纳米颗粒(SiNPs)锚定在垂直排列的碳纳米管(VACNTs)与定义的间距,以适应体积变化的混合纳米结构阳极合成的商业宏观集流体。实现具有良好稳定性和优异电化学性能的电极仍然是一个挑战。因此,我们在本文中通过在固定的VACNT毯状物长度下改变硅沉积时间来调节SiNP体积,或者通过在固定的SiNP体积下改变VACNT长度来调节活性硅面积负载。SiNP的低面积负载改善了循环期间的容量稳定性,但由于形成了固体电解质界面(SEI)层而引发了大的不可逆容量损失。相比之下,较高的面积负载电极减少了所形成的SEI的量,但是在随后的循环期间负面地影响电极的容量稳定性。通过增加VACNTs毯状物长度而不损害循环稳定性来实现硅的更高重量容量和更高面积负载质量。该混合纳米结构电极显示出优异的稳定性,在2000次循环后可逆容量为1330 mAh g-1。
The Intercalation Chemistry of the Disordered RockSalt Li3V2O5 Anode from Cluster Expansions and Machine Learning Interatomic Potentials
无序岩盐Li 3V 2 O 5由于其理想的低电压、高倍率性能和优异的循环稳定性而成为锂离子二次电池负极材料的理想选择。在此,我们提出了一个全面的研究DRX-Li 3V 2 O 5阳极的嵌入化学使用密度泛函理论计算结合机器学习集群扩展和原子间势。基于蒙特卡罗模拟和拟合的团簇膨胀模型,预测了室温下无序Li 3V 2 O 5阳极的电压分布,与实验结果吻合良好。与之前的DFT结果相比,我们发现在充电过程中Li离子主要嵌入四面体位置,而八面体位置的Li和V离子大多数保持稳定。此外,用拟合的矩张量势进行的MD模拟将DRX-Li 3V 2 O 5的快速充电能力归因于Li+通过四面体-八面体-四面体途径的容易扩散性。我们进一步建议调整Li:V比作为在该系统中权衡增加的锂化容量和降低的阳极电压的手段。这项工作为高性能DRX-Li 3V 2 O 5阳极提供了深入的见解,并为发现其他无序阳极材料铺平了道路。
Mn3O4-Graphene Hybrid as a High Capacity Anode Material for Lithium Ion Batteries
我们开发了两步溶液相反应以在还原氧化石墨烯(RGO)片上形成用于锂离子电池应用的Mn 3 O 4纳米颗粒的杂化材料。相对于溶液中的自由颗粒生长,在RGO片上选择性生长的Mn 3 O 4纳米颗粒允许电绝缘Mn 3 O 4纳米颗粒通过下面的导电石墨烯网络连接到集电器。在RGO上形成的Mn 3 O 4纳米颗粒显示出高达~ 900 mAh/g的高比容量,接近其理论容量,具有良好的倍率性能和循环稳定性,这归因于石墨烯基底与其上生长的Mn 3 O 4纳米颗粒之间的密切相互作用。Mn 3 O 4/RGO杂化材料有望成为高容量、低成本、环境友好的锂离子电池负极材料。我们的石墨烯生长方法应该为基于高绝缘材料的电池电极的设计和合成提供一种新技术。
The intriguing mechanism of phosphorus anodes for sodium ion batteries revealed by operando pair distribution function and X-ray diffraction computed tomography
Eliminating solvents and polymers in high-performance Si anodes by gas-phase assembly of nanowire fabrics
开发可持续的电池电极制造方法对于诸如硅的合金型活性物质尤其紧迫,其通常需要额外的能量密集型和基于溶剂的处理以用缓冲基质来增强它们。本工作介绍了一种新的方法来制造硅阳极作为连续的,坚韧的织物的任意厚度,没有加工溶剂,聚合物粘合剂,碳添加剂,或任何增强基体。阳极由直接从气相中的悬浮液组装的长Si纳米线的网状结构组成,在气相中它们通过浮动催化剂化学气相沉积生长。高于75重量%的高Si含量在纺织品状网络结构中,导致高性能的电极性质。对于所生产的所有厚度,它们的重量容量在C/20下为2330 mAh g-1,在C/20下达到9.3 mAh cm-2以上的面积容量,在1C下达到3.4 mAh cm-2(具有3.4 mg cm-2)。额定数据的分析给出了一个高的传输系数(6.6x10-12 m2 s-1),由于一个高的面外电导率(0.6 S m-1)和短的固态扩散长度。Si在延长的循环后保持细长元件的网状结构,保持导电性并导致在C/5下100次循环后80%的容量保持率和在C/2下500次循环后约60%的容量保持率。当与NMC 111阴极集成时,证明了480 Wh kg-1的全电池重量能量密度。
Flexible, solid electrolyte-based lithium battery composed of LiFePO4 cathode and Li4Ti5O10 anode for applications in smart textiles
在这里,我们报告制造的灵活和可拉伸的电池组成的应变自由LiFePO 4阴极,Li 4 Ti 5 O 10阳极和固体聚环氧乙烷(PEO)电解质作为隔膜层。该电池是从智能纺织品应用的角度开发的。该电池以固体热塑性电解质为关键使能元件,可挤压或拉伸成纤维或细条,直接与智能纺织品制造中使用的编织工艺兼容。本文首先详细介绍了材料的选择,电极和隔膜层的制造和表征。然后组装电池并对其进行表征,最后,将由几个长条制成的大型电池样品编织成织物,用导电线连接,并进行表征。在本文中,我们详细研究了电池设计的两个实际方面:第一是以导电碳和聚合物粘合剂材料的优化比例制备阴极/阳极材料的复合材料,第二是电池性能,包括循环,可逆性和阴极/阳极材料的相容性。最后,当铸造电极和隔膜层时,我们主要关注使用水溶液代替有机溶剂,以使制造过程环境友好。
Operando monitoring of single-particle kinetic state-of-charge heterogeneities and cracking in high-rate Li-ion anodes
近年来,对能够存储更多能量、更快充电和更长使用寿命的电池技术的需求迅速上升,这主要是由交通运输电气化和电网规模储能系统的推动。这导致了许多有前途的新型高倍率锂离子电池电极材料的开发。为了合理化和改善材料性能,至关重要的是要了解在实际电池运行过程中发生的纳米到中尺度的基本离子嵌入和降解机制。在这里,我们应用一个简单的实验室为基础的operando光学散射显微镜的方法来研究微米级棒的高速率阳极材料Nb $_{14}$ W $_3$ O $_{44}$在循环过程中的速率高达30 C。我们直接可视化杆的伸长,通过与系综X射线衍射的比较,使我们能够确定单个粒子的荷电状态(SOC)。还观察到散射强度随SOC的连续变化,使得能够观察到单个颗粒内的非平衡动力学相分离。相场建模(由脉冲场梯度核磁共振和电化学实验提供信息)被用来验证这种分离的动力学起源,其起因于锂离子扩散系数对SOC的依赖性。最后,我们见证了这种颗粒内SOC异质性如何导致颗粒开裂;我们跟踪所得碎片的循环行为,并表明它们可能与电极电断开。这些结果表明,光学散射显微镜的权力,以跟踪快速的非平衡过程,往往发生在不到1分钟,这将是不可访问的既定表征技术。
Nanoscale imaging reveals critical plating and stripping mechanisms in anode-free lithium and sodium solid-state batteries
Autonomous University of Madrid (UAM)(马德里自治大学);Nicolás Cabrera University Institute of Materials Science (INC), UAM(尼古拉斯·卡布雷拉大学材料科学研究院(INC));ALBA Synchrotron Light Facility(阿尔巴同步辐射光源设施);Norwegian University of Science and Technology (NTNU)(挪威科技大学);Fraunhofer Institute for Ceramic Technologies and Systems (IKTS)(弗劳恩霍夫陶瓷技术和系统研究所);Instituto de Ciencia de Materiales de Madrid, Consejo Superior de Investigaciones Científicas (CSIC)(马德里材料科学研究所,西班牙国家研究委员会);National Institute of Advanced Industrial Science and Technology (AIST), Research Institute for Energy Efficient Technologies(国立先进工业科学技术研究院,能源效率技术研究所);Condensed Matter Physics Center (IFIMAC), UAM(凝聚态物理中心(IFIMAC))
Theoretical prediction of MoN2 monolayer as a high capacity electrode material for metal ion batteries
近年来合成的二维(2D)材料MoN 2具有环境友好、易提纯、热稳定性高等优点,在清洁能源和可再生能源领域显示出巨大的应用潜力。本文通过第一性原理计算表明,单层MoN_2有望成为金属离子电池的高容量电极材料。首先,通过声子色散和剥离能的计算,证实了MoN 2单层膜的结构稳定性,并且在实验中可以从其体相剥离。其次,所有研究的金属原子(Li,Na和K)可以吸附在MoN 2单层,与原始和掺杂的MoN 2是金属。第三,金属原子在MoN 2上具有中等/低的迁移势垒,这确保了作为电池电极的优异循环性能。此外,计算的平均电压表明,MoN 2单层适合作为锂离子电池的阴极和钠离子和钾离子电池的阳极。最重要的是,作为锂离子电池的阴极,MoN 2具有可比的平均电压,但比通常的商业阴极材料大1-2倍的容量(432 mA h g-1);作为钠离子电池的阳极,MoN 2的理论容量(864 mA h g-1)比典型的2D阳极材料如MoS 2和大多数MXene大2-5倍。最后,我们还提供了其他过渡金属二氮化物材料的容量估计。我们的工作表明,过渡金属二氮化物MoN 2是一种有吸引力的高存储容量的二维电极材料。
Influence of Electrode Thickness and Electrolyte Composition on SEI Formation and Cycle Stability in Binder-Free Hard Carbon Anodes for Na-Ion Batteries
Université de Haute-Alsace(阿尔萨斯大学);Institut de Science des Matériaux de Mulhouse (IS2M)(穆尔豪斯材料科学研究所);CNRS UMR 7361(法国国家科学研究中心联合研究实验室7361);Université de Strasbourg(斯特拉斯堡大学);Réseau sur le Stockage Electrochimique de l’Energie (RS2E)(电化学储能网络);CNRS FR3459(法国国家科学研究中心自由研究基金3459)
本研究探讨了硬碳自支撑电极厚度、大孔率及电解液添加剂对钠离子电池SEI形成和循环稳定性的影响,发现FEC添加剂可改善稳定性,实现高达93%的初始库仑效率和328 mAh g-1的可逆容量。
An Effective Strategy to Enable Argyrodite Sulfides as Superb Solid-State Electrolytes: Safeguarding Remarkable Ionic Conductivity and Interfacial Stability with Electrodes