受添加剂FEC驱动的原位聚合提升硅负极的日历寿命 via 表面钝化增强
Aging-driven in situ polymerization of FEC additive boosts the calendar-life of silicon anodes via surface passivation enhancement
AI总结:
FEC添加剂通过原位聚合增强硅负极表面钝化,显著延长电池日历寿命。
摘要:
添加剂如FEC在延长硅负极日历寿命方面的作用仍不完全清楚。本文研究了高负载硅(80 wt%)在基准1.2 M LiPF6 EC-EMC电解质与添加10 wt% FEC的对比情况,持续数月。在8天老化后,FEC使硅-锂铁磷酸盐全电池的不可逆容量损失减少了13倍。无FEC的电池预计在约22天内容量降至初始值的80%,而有FEC的电池则可维持约279天。从回收电极中提取的对称Si-Si电池在无FEC时表现出更大的相间电阻增加,其中0 wt% FEC在2个月内电阻增加10.81欧姆,而10 wt% FEC仅增加3.37欧姆。对长期相间电阻的幂律建模发现,在无FEC的电池中存在混合的传输-反应增长行为,表明显著溶解,而添加10 wt% FEC的电池则表现出扩散控制的阻抗增长行为,表明表面钝化膜的稳定性。事后FTIR和XPS证实了SEI中聚碳酸酯的富集,该现象主要源于FEC在闲置老化期间的自聚合。当带有和不带有FEC的硅电极被回收并重新组装成使用相同电解质的全电池时,0 wt% FEC的首次循环库仑效率为71%,而10 wt% FEC的为97%。后续循环中,10 wt% FEC的库仑效率维持在99.7%以上,超过预老化前的98.8%。这种提高的库仑效率表明,由老化过程中形成的聚合物碎片提供的钝化效果优于电化学形成的SEI,后者未发现强聚合物FTIR信号。因此,FEC等添加剂在闲置老化期间的自聚合是一种原位机制,可用于进一步工程化以延长基于硅的电池寿命。
英文摘要:
The role of additives such as FEC in extending the calendar life of silicon anodes beyond the cycling benefits is still not fully understood. Herein, the calendar life of high-loading Si (80 wt%) using baseline 1.2 M LiPF6 in EC-EMC electrolyte versus adding 10 wt% FEC is investigated over months. Over 8 days of aging, FEC leads to a 13-fold reduction in irreversible capacity loss in Si-LiFePO4 full cells. Cells without FEC are projected to fall below 80% of their initial capacity within approx. 22 days versus approx. 279 days with FEC. Symmetric Si-Si cells from harvested electrodes show greater increase in interphase resistance without FEC, whereby an increase of 10.81 Ohms is measured for 0 wt% FEC vs. only 3.37 Ohms for 10 wt% FEC over 2 months. Power law modeling of this long-term interphase resistance finds mixed transport-reaction growth behavior in FEC-free cells, suggesting significant dissolution, whereas cells with 10 wt% FEC added display a diffusion-controlled impedance growth behavior, suggesting a robust surface passivation film. Post-mortem FTIR and XPS confirm polycarbonate enrichment of the SEI, which was discovered to predominantly emerge from FEC self-polymerization during the idle aging. When the Si electrodes aged with and without FEC are harvested and reassembled into full cells with the same electrolytes used at aging, the first-cycle coulombic efficiency is 71% for 0 wt% FEC versus 97% for 10 wt% FEC. Subsequent cycling maintains over 99.7% CE with 10 wt% FEC, surpassing the pre-aging CE of 98.8%. This elevated CE indicates better passivation provided by the polymer fragments formed during aging compared to electrochemically formed SEI where no strong polymer FTIR signal is found. The self-polymerization during idle aging with additives such as FEC is therefore an opportune in situ mechanism to further engineer in extending the life of Si-based batteries.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。