arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2605.16166cond-mat.mtrl-sci
收藏

快速大气压水蒸气沉积H:In2O3透明导电氧化物薄膜

Rapid Atmospheric Vapor Deposition of H:In2O3 Transparent Conducting Oxide Thin Films

University of Oxford(牛津大学);University of Surrey(萨里大学);National Taiwan University(台湾大学);University of Cambridge(剑桥大学);University of Manchester(曼彻斯特大学);Sungkyunkwan University(成均馆大学);Univ. Toulouse, CNRS, Toulouse INP, LGC(图卢兹大学,法国国家科学研究中心,图卢兹第三工业大学,化学实验室)
Xiaoyu Guo, Hae-Jun Seok, Eilidh L. Quinn, Matthew K Sharpe, Callum. D. McAleese, Yi-Teng Huang, Xinjuan Li, Kexue Li, Chia-Yu Chang, Yongjie Wang, John O'Sulli… 展开作者

Xiaoyu Guo, Hae-Jun Seok, Eilidh L. Quinn, Matthew K Sharpe, Callum. D. McAleese, Yi-Teng Huang, Xinjuan Li, Kexue Li, Chia-Yu Chang, Yongjie Wang, John O'Sullivan, Katie L. Moore, Caterina Ducati, Ruy Sebastian Bonilla, Han-Ki Kim, Abderrahime Sekkat, Robert L. Z. Hoye

AI总结:

本研究通过大气压化学气相沉积法快速制备低电阻高透光率的H:In2O3薄膜,其性能优于商业溅射InSnO,且在温和条件下实现高性能透明导电氧化物的高效制造。

摘要:

透明导电氧化物(TCOs)对光电子工业至关重要,但缺乏有效且经济的方法快速沉积低电阻、高透光率的薄膜而不损害敏感材料,包括新兴的软半导体如金属卤化物钙钛矿。本文使用大气压化学气相沉积(AP-CVD)合成H:In2O3薄膜,其表电阻为7.20±0.01 Ohm/sq(0.50±0.06 mOhm·cm电阻率),近红外透光率高达89%,超越商业溅射沉积的氧化铟锡。生长速率比原子层沉积(ALD)高40倍,AP-CVD薄膜在仅140°C的常压条件下即可完全加工。二次离子质谱和时间飞行弹性反冲探测分析与载流子浓度变化的比较表明,H掺杂来自氧化剂水。当氧化剂从O2改为H2O时,迁移率从40±10 cm²/Vs增加到160±30 cm²/Vs,归因于H掺杂剂钝化氧空位,这些空位作为载流子散射中心。本工作确立了AP-CVD作为快速、可扩展且经济的高性能TCOs制造方法,使用与热敏感材料兼容的温和生长条件。

英文摘要:

Transparent conducting oxides (TCOs) are essential for the optoelectronics industry, but there is a critical gap in cost-effective methods to rapidly deposit low sheet resistance, high transmittance films without damaging delicate materials, including emerging soft semiconductors like metal-halide perovskites. In this work, atmospheric pressure chemical vapor deposition (AP-CVD) is used to synthesise H:In2O3 films with 7.20+/-0.01 Ohm/sq sheet resistance (0.50+/-0.06 mOhm.cm resistivity) and transmittance up to 89% in the near-infrared (NIR), surpassing commercial sputter-deposited indium tin oxide. The growth rate is 40x higher than atomic layer deposition (ALD), and the AP-CVD films are fully processed under atmospheric conditions at only 140 C. Comparison of secondary ion mass spectrometry and time-of-flight elastic recoil detection analysis with changes in carrier concentration indicate that H dopants are introduced from the water oxidant. There is an increase in mobility form 40+/-10 cm2/Vs to 160+/-30 cm2/Vs when changing from O2 to H2O as the oxidant, which is attributed to H dopants passivating oxygen vacancies that act as carrier scattering centers. This work establishes AP-CVD as a promising method for manufacturing high figure-of-merit TCOs in a rapid, scalable and cost-effective manner, using mild growth conditions compatible with thermally-sensitive materials.