AI总结:

采用密度泛函理论计算了六方和立方GaN中堆垛层错的能量、原子和电子结构,发现I1型层错在六方相中最稳定,立方相中本征层错占主导,并揭示了层错附近的电荷再分布导致II型能带偏移。

摘要:

我们进行了密度泛函理论(DFT)计算,以表征GaN中堆垛层错的能量学、原子和电子结构,包括稳定的六方纤锌矿(wz)相和亚稳态立方闪锌矿(zb)相。在wz GaN中,(0001)面上的SF可分为三种本征堆垛层错(I1、I2和I3)和一种非本征堆垛层错(E)。在zb GaN中,SF沿(111)方向形成,分别产生一种本征、非本征和孪晶SF。根据计算的形成能,I1是wz GaN中最稳定的SF,与实验一致。对于zb GaN,本征堆垛层错是最主要的平面缺陷。为了表征堆垛层错对材料电子结构的影响,我们检查了能带密度。我们发现,wz GaN中价带顶附近的能带局域在堆垛层错的Ga极性侧(即垂直于SF的Ga-N键的Ga侧),而导带底附近的能带更多在N极性侧,尽管有些离域。我们在zb GaN中发现了相反的趋势;这种行为是由界面附近的电荷再分布引起的。我们还展示了堆垛层错的能带偏移,发现它们对局部条件非常敏感,但都可以描述为II型界面,堆垛层错的存在局部减小了带隙。

英文摘要:

We have performed density functional theory (DFT) calculations to characterize the energetics, and the atomic and electronic structure, of stacking faults in GaN, both in the stable hexagonal wurtzite (wz) phase and in the metastable cubic zincblende (zb) phase. In wz GaN, SFs on the (0001) planes can be divided into three different intrinsic stacking faults (I1, I2, and I3) and oneextrinsic stacking fault (E). In zb GaN, SFs form along (111) directions, giving one type each of intrinsic, extrinsic and twin SFs. Based on the calculated formation energy, I1 is the most stable SF of wz GaN in agreement with experiment. For zb GaN, the intrinsic stacking fault is the most dominant planar defect. To characterize the effect of the stacking faults on the electronic structure of the material, we examined the band density. We found that the bands near the valence band maximum in wz GaN are localised on the Ga-polar side of the stacking fault (i.e. on the Ga side of the Ga-N bonds perpendicular to the SF), with the bands near the conduction band minimum more on the N-polar side, though somewhat delocalised. We found the opposite trend in zb GaN; this behaviour is caused by a redistribution of charge near the interface. We also show the band offsets for the stacking faults, finding that they are very sensitive to local conditions, but can all be described as type II interfaces, with the presence of a stacking fault reducing the gap locally.