高质量原子级薄且原子级平整的Bi$_2$O$_2$Se薄膜的可控快速生长

Controllable and Fast Growth of High-Quality Atomically Thin and Atomically Flat Bi$_2$O$_2$Se Films

Yusen Feng, Pei Chen, Nian Li, Suzhe Liang, Ke Zhang, Minghui Xu, Yan Zhao, Jie Gong, Shu Zhang, Huaqian Leng, Yuanyuan Zhou, Yong Wang, Liang Qiao

AI总结:

本文系统研究脉冲激光沉积法快速可控生长原子级薄且平整的Bi$_2$O$_2$Se薄膜,提出四步生长机制并成功制备高质量外延薄膜。

摘要:

作为一种新型且有前景的二维材料,硒氧化铋(Bi$_2$O$_2$Se)因其高对称性、可调电子结构、超高电子迁移率等独特物理性质,已展现出克服多种电子器件应用中现有技术障碍的巨大潜力。然而,在精确控制下快速生长至几个原子层厚度的Bi$_2$O$_2$Se薄膜仍然是一个重大挑战。本工作系统研究了通过脉冲激光沉积(PLD)方法生长二维(2D)Bi$_2$O$_2$Se薄膜。通过控制温度、氧压、激光能量密度和激光发射频率,我们成功在SrTiO3的(001)表面上制备出原子级薄且平整的Bi$_2$O$_2$Se (001)薄膜。重要的是,我们为理解原子级薄且平整的Bi$_2$O$_2$Se薄膜的生长过程提供了一个基础且独特的视角,该生长过程主要可归纳为四个步骤:i) 沿台阶根部优先发生的各向异性非自发成核;ii) 单层Bi$_2$O$_2$Se纳米片向周围区域扩展,最终覆盖整个STO衬底台阶;iii) Bi$_2$O$_2$Se单层以二维Frank-van der Merwe(FM)外延生长模式进行垂直生长;iv) 以逐层二维FM生长模式,最终产生原子级平整且外延取向一致的薄膜。此外,结晶质量、表面形貌和化学态的综合结果表明,成功以可控且快速的方式实现了高质量Bi$_2$O$_2$Se薄膜的PLD生长。

英文摘要:

As a novel and promising 2D material, bismuth oxyselenide (Bi$_2$O$_2$Se) has demonstrated significant potential to overcome existing technical barriers in various electronic device applications, due to its unique physical properties like high symmetry, adjustable electronic structure, ultra-high electron mobility. However, the rapid growth of Bi$_2$O$_2$Se films down to a few atomic layers with precise control remains a significant challenge. In this work, the growth of two-dimensional (2D) Bi$_2$O$_2$Se thin films by the pulsed laser deposition (PLD) method is systematically investigated. By controlling temperature, oxygen pressure, laser energy density and laser emission frequency, we successfully prepare atomically thin and flat Bi$_2$O$_2$Se (001) thin films on the (001) surface of SrTiO3. Importantly, we provide a fundamental and unique perspective toward understanding the growth process of atomically thin and flat Bi$_2$O$_2$Se films, and the growth process can be primarily summarized into four steps: i) anisotropic non-spontaneous nucleation preferentially along the step roots; ii) monolayer Bi$_2$O$_2$Se nanosheets expanding across the surrounding area, and eventually covering the entire STO substrate step; iii) vertical growth of Bi$_2$O$_2$Se monolayer in a 2D Frank-van der Merwe (FM) epitaxial growth, and iv) with a layer-by-layer 2D FM growth mode, ultimately producing an atomically flat and epitaxially aligned thin film. Moreover, the combined results of the crystallinity quality, surface morphology and the chemical states manifest the successful PLD-growth of high-quality Bi$_2$O$_2$Se films in a controllable and fast mode.