Cu/Al$_2$O$_3$多层薄膜的应变速率敏感性

Strain rate sensitivity of a Cu/Al$_2$O$_3$ multi-layered thin film

Szilvia Kalácska, László Pethő, Guillaume Kermouche, Johann Michler, Péter Dusán Ispánovity

AI总结:

本研究制备铜/Al$_2$O$_3$多层薄膜并进行热处理,通过不同尺寸微柱的宽应变速率压缩实验,结合多种表征揭示了Al$_2$O$_3$中间层的晶界钉扎、抑制剪切局部化和再结晶的作用,为极端环境用涂层提供了参考。

摘要:

为研究铜多晶微观结构的尺寸与应变速率依赖性,采用物理气相沉积与原子层沉积结合的混合沉积系统,在硅衬底上制备了铜/Al$_2$O$_3$多层薄膜。对具有超细晶结构的“沉积态”样品进行高温处理,增大平均晶粒尺寸,得到具有微晶结构的“热处理态”样品。利用聚焦离子束铣削制备两种不同尺寸的方形微柱,在0.001/s至1000/s的不同应变速率下进行压缩加载。结合微柱直径与变形样品的晶粒尺寸,讨论了低、高应变速率下表现出的应变速率敏感性行为差异。经透射电子显微镜表征,Al$_2$O$_3$中间层表现出优异的热稳定性,可通过析出相实现晶界钉扎,还能使微柱均匀变形,抑制剪切局部化。通过高角分辨率电子背散射衍射估算的几何必需位错密度显示,变形微柱内部位错分布不均匀,这归因于样品边缘的邻近效应。最后,Al$_2$O$_3$中间层成功抑制了所有可能的再结晶过程,提升了薄膜稳定性,使该涂层适用于极端环境下的工作场景。

英文摘要:

To study the size and strain rate dependency of copper polycrystalline microstructures, a multi-layered copper/Al$_2$O$_3$ thin film was deposited on a Si substrate using a hybrid deposition system (combining physical vapour and atomic layer deposition). High temperature treatment was applied on the ``As Deposited" material with ultrafine-grained structure to increase the average grain size, resulting in a ``Heat Treated" state with microcrystalline structure. Focused ion beam milling was employed to create square shaped micropillars with two different sizes, that were subjected to compressive loading at various (0.001/s -- 1000/s) strain rates. Differences in the strain rate sensitivity behavior manifesting at low and high strain rates are discussed in the context of the pillar diameters and the grain size of the deformed samples. The Al$_2$O$_3$ interlayer studied by transmission electron microscopy showed excellent thermal stability and grain boundary pinning by precipitation, also resulting in the homogeneous deformation of the pillars and preventing shear localization. Geometrically necessary dislocation densities estimated by high (angular) resolution electron backscatter diffraction presented inhomogeneous dislocation distribution within the deformed pillar volumes, that is attributed to the proximity of the sample edges. Finally, the Al$_2$O$_3$ interlayers successfully suppressed any possible recrystallization processes, contributing to the excellent film stability, that makes the proposed coating ideal to be operating under extreme conditions.