The transparent conducting oxide SnO2 is a wide bandgap semiconductor that is easily n-type doped and widely used in various electronic and optoelectronic applications. Experimental reports of the electron mobility of this material vary widely depending on the growth conditions and doping concentrations. In this work, we calculate the electron mobility of SnO2 from first principles to examine the temperature- and doping-concentration dependence, and to elucidate the scattering mechanisms that limit transport. We include both electron-phonon scattering and electron-ionized impurity scattering to accurately model scattering in a doped semiconductor. We find a strongly anisotropic mobility that favors transport in the direction parallel to the c-axis. At room temperature and intrinsic carrier concentrations, the low-energy polar-optical phonon modes dominate scattering, while ionized-impurity scattering dominates above 10^18 cm^-3.
Significant enhancement of hole mobility in [110] silicon nanowires compared to electrons and bulk silicon
利用sp 3d 5s * 紧束缚能带结构和电子和空穴的波函数,我们证明了在[110]生长的硅纳米线(SiNWs)中声学声子限制的空穴迁移率大于电子迁移率。所考虑的SiNW的室温声学限制的空穴迁移率可以高达2500 cm 2/Vs,这是几乎三倍大于体声学限制的硅空穴迁移率。结果还表明,[110]生长的硅纳米线的电子和空穴迁移率超过了类似直径的[100]硅纳米线,空穴迁移率相差近两个数量级。由于小直径的硅纳米线主要沿[110]方向生长,结果强烈表明这些硅纳米线可能在未来的电子学中有用。我们的研究结果也与最近的实验测量硅纳米线的流动性。
Electron and Hole Mobility of SnO2 from Full-Band Electron-Phonon and Ionized Impurity Scattering Computations
迁移率是SnO 2的关键参数,SnO 2作为实用的透明氧化物n型半导体被广泛研究。在实验中,电子在体SnO_2单晶的迁移率在室温下从70到260 cm ~ 2 V ~(-1)s ~(-1)变化。在这里,我们计算的迁移率限制的电子-声子和电离杂质散射耦合的玻尔兹曼输运方程与密度泛函理论电子结构。线性化玻尔兹曼输运方程的数值求解超出了常用的常数弛豫时间近似,考虑到所有的能量和动量的散射率的依赖性。声学变形势和极性光学声子被认为是电子-声子散射,其中极性光学声子散射被发现是决定电子和空穴在室温下的迁移率的主要因素。声子限制的电子迁移率的计算被发现是265 cm ~ 2 V ~(-1)s ~(-1),而被发现的空穴是7.6 cm ~ 2 V ~(-1)s ~(-1)。我们提出的迁移率作为载流子浓度的函数,这表明了上限的迁移率。n型和p型SnO 2的迁移率之间的巨大差异是电子和空穴之间的不同有效质量的结果。
Electron Mobility in Monoclinic β-Ga2O3 - Effect of Plasmon-phonon Coupling, Anisotropy, and Confinement
采用基于密度泛函微扰理论的晶格动力学计算、晶格模与集体等离子体激元振荡的耦合计算和基于玻尔兹曼理论的输运计算相结合的方法,研究了单斜β-Ga 2 O 3中的电子输运.等离子体激元与不同的纵向光学(LO)模式的强纠缠使得LO-等离子体激元耦合的作用对于传输至关重要。研究了体材料和二维电子气形式下β-Ga_2 O_3中电子迁移率与电子密度的关系。在高电子密度下,预测体迁移率为182 cm 2/ V.s,而在2DEG形式中,当远程杂质存在于界面处时,相应的迁移率为约418 cm 2/V.s,并且随着远程杂质中心远离界面而进一步提高。电子迁移率的变化趋势表明,在掺杂隔离电子沟道中实现高电子迁移率是有希望的。通过瞬态蒙特卡罗模拟跟踪实验观察到的迁移率的小各向异性。研究发现,红外活性声子模的各向异性是导致低场电子迁移率各向异性的原因。
Giant modulation of the electron mobility in semiconductor Bi$_2$O$_2$Se via incipient ferroelectric phase transition
高迁移率层状半导体具有实现下一代电子和计算的潜力。本文证明了在层状半导体Bi $_2$ O $_2$ Se中观察到的电子迁移率源于初始的铁电转变,该铁电转变赋予材料以针对库仑散射引起的迁移率退化的鲁棒保护。基于电子-声子相互作用和离子化杂质散射的第一性原理计算表明,Bi $_2$ O $_2$ Se的电子迁移率在较宽的掺杂浓度范围内可达到10 $^4$到10 $^6$ cm $^2$ V $^{-1}$ s $^{-1}$.此外,1.7%的小弹性应变可以驱动材料朝向独特的层间铁电转变,导致介电常数的大幅增加和低温电子迁移率的巨大增强超过一个数量级。这些结果为通过相位和介电工程实现高迁移率层状半导体开辟了一条新的途径。
First-principles study of electron transport in ScN
基于密度泛函理论研究了岩盐SCN的导能带结构和电子迁移率.第一性原理能带结构使我们能够获得能带速度和有效质量作为能量的函数。电子-声子散射的评估明确计算的$q$依赖的电子-声子矩阵元素,包括远程静电相互作用。自由载流子屏蔽对电子输运的影响进行了评估,使用无规相位近似。我们发现当载流子浓度超过10 $^{20}$ cm $^{-3}$时,电子迁移率显著增强。我们计算出在低载流子浓度下ScN中的室温电子迁移率为587 cm $^2$ /Vs。当载流子浓度增加时,电子迁移率在$n=10^{19}$ cm $^{-3}$附近开始显著降低,并且在$n=10^{21}$ cm $^{-3}$处下降到240 cm $^2$ /Vs。我们还探讨了应变在(111)和(100)取向的氮化钪薄膜中的影响。对于(111)薄膜,1.0%的外延压应变使面内迁移率增加72 cm $^2$ /Vs,面外迁移率增加50 cm $^2$ /Vs。对于(100)薄膜,1.0%的外延压应变使面外迁移率增加172 cm $^2$ /Vs,但对面内迁移率的影响很小。我们的研究揭示了电子输运在不同的电子浓度的SCN,并显示如何应变工程可以增加电子迁移率。
High-temperature-grown buffer layer boosts electron mobility in epitaxial La-doped BaSnO$_3$/SrZrO$_3$ heterostructures
通过在薄膜和衬底之间插入SrZrO $_3$缓冲层,我们证明了La:BaSnO $_3$薄膜中的穿透位错密度的显著降低以及电子迁移率的相关改善。室温迁移率为140厘米$^2$ V $^{-1}\text{s}^{-1}$实现25纳米厚的膜,没有任何后生长处理。用脉冲激光沉积法在(110)TbScO $_3$衬底上制备的缓冲膜中,穿透位错密度仅为$4.9\times 10^{9}$ cm $^{-2}$。
First-principles analysis of electron transport in BaSnO$_3$
BaSnO $_3$(BSO)是一种有前途的透明导电氧化物(TCO),据报道室温(RT)霍尔迁移率超过320 cm $^{2}$ V $^{-1}$ s $^{-1}$。在钙钛矿氧化物中,它具有最高的RT迁移率,比原型SrTiO $_3$高约30倍。使用基于混合密度泛函理论的第一性原理计算,我们阐明的物理机制,通过研究LO声子和电离杂质散射的细节,管理的迁移率。仔细的数值分析,以获得收敛的结果内的玻尔兹曼输运理论的弛豫时间近似。充分考虑了弛豫时间的${\bf k}$依赖性。我们发现,高RT流动性BSO起源不仅从一个小的有效质量,但也从显着减少的声子散射率相比,其他钙钛矿氧化物;这种减少的起源被确定。电离杂质散射影响总迁移率,即使在RT的掺杂剂密度大于$5\times10^{18}$ cm $^{-3}$,并成为可比较的LO声子散射的$1\times10^{20}$ cm $^{-3}$掺杂,降低漂移迁移率从其固有的LO声子限制值$\sim$ 594 cm $^{2}$ V $^{-1}$ s $^{-1}$小于310 cm $^{2}$ V $^{-1}$ s $^{-1}$。我们建议通过调制掺杂或极性不连续掺杂来避免杂质散射。我们还明确计算霍尔因子和霍尔迁移率,允许直接比较散装和薄膜的实验报告,并提供洞察的主要机制,限制流动性的国家的最先进的样品的性质。
On the limits to mobility in InAs quantum wells with nearly lattice-matched barriers
本文报道了一系列二维电子系统的生长和低温迁移率的密度依赖性,这些系统局限于非有意掺杂的低扩展缺陷密度的InAs量子阱中,具有Al $_{1-x}$ Ga $_{x}$ Sb势垒。利用双栅器件研究了电子迁移率与载流子密度和电场的关系,确定了电子迁移率限制散射机制。可能的散射机制的分析表明,流动性主要是有限的粗糙的界面在窄量子阱和合金无序和界面粗糙度的组合在宽井在高载流子密度内的第一个被占用的电子子带。在低载流子密度的功能依赖的载流子密度的迁移率提供证据的库仑散射带电缺陷。在2 K的样品温度下,获得了超过750,000 cm $^{2}$ /Vs的栅极调谐电子迁移率。
Electron and hole mobility of rutile GeO$_2$ from first principles: an ultrawide-band-gap semiconductor for power electronics
金红石型二氧化锗(r-GeO $_2$)是一种新型的超宽带隙半导体材料,在大功率电子器件中具有潜在的应用前景。我们应用基于密度泛函和密度泛函微扰理论的第一性原理计算来研究r-GeO $_2$中的载流子-声子耦合,并预测其声子限制的电子和空穴迁移率作为温度和晶体取向的函数。在300 K下计算的载流子迁移率为$μ_{\text{elec},\perp \vec{c}}$ =244 cm $^2$ V $^{-1}$ s $^{-1}$,$μ_{\text{elec},||\vec{c}}$ =377 cm $^2$ V $^{-1}$ s $^{-1}$,$μ_{\text{hole},\perp \vec{c}}$ =27 cm $^2$ V $^{-1}$ s $^{-1}$,和$μ_{\text{hole},||\vec{c}}$ =29 cm $^2$ V $^{-1}$ s $^{-1}$。在室温下,载流子散射由低频偏振光声子模式主导。预测的n型r-GeO $_2$的Baliga优值超过了几种现有的半导体,如Si,SiC,GAN和$β$-Ga $_2$ O $_3$,证明了其在高功率电子器件中的优越性能。
Combining Landau Zener Theory and Kinetic Monte Carlo Sampling for Small Polaron Mobility of Doped BiVO4
过渡金属氧化物如\ce{BiVO4}是在太阳能-燃料转换应用中作为光电极的有前景的材料。然而,它们的性能受到由于形成小极化子而导致的低载流子迁移率(特别是电子迁移率)的限制。最近的实验研究表明,原子掺杂提高了载流子迁移率和电导率。从第一性原理出发,结合Landau-Zener理论和动力学Monte Carlo(kMC)模拟,研究了掺杂前后\ce{BiVO4}中小极化子的跳跃迁移率,并考察了掺杂剂-极化子相互作用对迁移率的影响.我们发现在原始的和Mo/W掺杂的\ce{BiVO4}中在V处自发地形成极化子,这只能用具有Hubbard校正的密度泛函理论(DFT+U)或混合交换相关泛函来正确描述,而不能用局域或半局域泛函来描述。我们发现DFT+U和介电依赖杂化泛函(DDH)给出了类似的电子跳跃势垒,这也是类似的室温单斜相和四斜相。电子迁移率的计算值与实验值吻合较好,约为$10^{-4}$ cm $^2$ V $^{-1}$ s $^{-1}$ .我们发现\ce{BiVO4}中的电子极化子输运既不是完全绝热的,也不是非绝热的,而且第一和第二近邻跳跃具有明显不同的跳跃能力,尽管它们具有相似的跳跃势垒.我们进一步计算了极化子迁移率在不同的掺杂剂的存在下,并表明,Cr取代V是一个电子陷阱,而Mo和W的“排斥”中心,主要是由于最小化的局部晶格膨胀的掺杂剂和电子极化子。与极化子的“排斥”相互作用的掺杂…