arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2105.02404cond-mat.mtrl-scicond-mat.mes-hallcond-mat.other
收藏

初始SrO生长对PDKEEPAAAAD $_3$(001)上的SrRuO $_3$外延薄膜中剩余电阻率的高灵敏度

High-sensitivity of initial SrO growth on the residual resistivity in epitaxial thin films of SrRuO$_3$ on SrTiO$_3$ (001)

Uddipta Kar, Akhilesh Kr. Singh, Song Yang, Chun-Yen Lin, Bipul Das, Chia-Hung Hsu, Wei-Li Lee

摘要:

高结晶度、低剩余电阻率的SrRuO $_3$(SRO)薄膜的生长是研究其本征性质的关键。这里,利用吸附控制生长技术,发现TiO $_2$封端的SrTiO $_3$(STO)(001)衬底上的初始SrO层的生长条件对于在随后生长的所得SRO膜中实现低RR是至关重要的。优化的初始SrO层显示出$c$(2 × 2)的超结构,其特征在于通过电子衍射,然后生长一系列具有不同厚度的SRO膜($t$)。所得的SRO膜表现出优异的结晶度,正交相低至$t \approx$ 4.3 nm,这是由高分辨率X射线测量证实。通过对SRO斜方(021)反射的方位角X射线扫描,我们发现了四个以斜方SRO [001]为主的结构域,沿立方STO [010]方向。主要结构域的数量取决于$t$、STO错切角($α$)和错切方向($β$),对于$t \approx$ 26.6 nm和($α$,$β$)~(0.14 $^{\rm o}$,5 $^{\rm o}$),给出约92 $\%$的体积分数。另一方面,金属和铁磁性质在低至$t \approx$ 1.2 nm时得到很好的保持。残余电阻率比(RRR = $ρ$(300 K)/ $ρ$(5 K))从$t \approx$ 28.5 nm的77.1降低到$t \approx$ 1.2 nm的2.5,而$ρ$(5 K)从$t \approx$ 28.5 nm的2.5 $μΩ$ cm增加到$t \approx$ 1.2 nm的131.0 $μΩ$ cm。铁磁起始温度($T_c\prime$)约为151 K,在低至$t \approx$ 9.0 nm时几乎保持不变,在$t \approx$ 1.2 nm时降低至90 K。因此,我们的研究结果提供了一个实用的指导方针,以实现高结晶度和低RR超薄SRO薄膜通过简单地调整初始SrO层的生长。

英文摘要:

The growth of SrRuO$_3$ (SRO) thin film with high-crystallinity and low residual resistivity (RR) is essential to explore its intrinsic properties. Here, utilizing the adsorption-controlled growth technique, the growth condition of initial SrO layer on TiO$_2$-terminated SrTiO$_3$ (STO) (001) substrate was found to be crucial for achieving a low RR in the resulting SRO film grown afterward. The optimized initial SrO layer shows a $c$(2 x 2) superstructure that was characterized by electron diffraction, and a series of SRO films with different thicknesses ($t$s) were then grown. The resulting SRO films exhibit excellent crystallinity with orthorhombic-phase down to $t \approx$ 4.3 nm, which was confirmed by high resolution X-ray measurements. From azimuthal X-ray scan for SRO orthorhombic (021) reflection, we uncover four structural domains with a dominant domain of orthorhombic SRO [001] along cubic STO [010] direction. The dominant domain population depends on $t$, STO miscut angle ($α$), and miscut direction ($β$), giving a volume fraction of about 92 $\%$ for $t \approx$ 26.6 nm and ($α$, $β$) ~ (0.14$^{\rm o}$, 5$^{\rm o}$). On the other hand, metallic and ferromagnetic properties were well preserved down to $t \approx$ 1.2 nm. Residual resistivity ratio (RRR = $ρ$(300 K)/$ρ$(5 K)) reduces from 77.1 for $t \approx$ 28.5 nm to 2.5 for $t \approx$ 1.2 nm, while $ρ$(5 K) increases from 2.5 $μΩ$cm for $t \approx$ 28.5 nm to 131.0 $μΩ$cm for $t \approx$ 1.2 nm. The ferromagnetic onset temperature ($T_c\prime$) of around 151 K remains nearly unchanged down to $t \approx$ 9.0 nm and decreases to 90 K for $t \approx$ 1.2 nm. Our finding thus provides a practical guideline to achieve high crystallinity and low RR in ultra-thin SRO films by simply adjusting the growth of initial SrO layer.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑