通过分子动力学理解金属增材制造中的缺陷结构

Understanding defect structures in metal additive manufacturing via molecular dynamics

Gurmeet Singh, Anthony M. Waas, Veera Sundararaghavan

摘要:

采用分子动力学模拟研究了单晶金属柱的增材制造。在该模型中,熔池逐渐增加,并在等压条件下冷却到目标温度,以自下而上构建金属柱。共近邻分析(CNA)被用来观察在这个过程中的原子尺度的缺陷的演变。对于添加的熔融层,可以看到凝固沿着两个方向进行。与较冷晶格接触的熔融层具有快速凝固前沿,其与从顶层开始的较慢凝固前沿竞争。缺陷结构的形成强烈地依赖于两个竞争凝固前沿的速度。达到一个临界层厚度,获得无缺陷的单晶作为快速凝固前沿到达顶部的熔体池之前,从顶部的较慢的前端启动。较慢的冷却速率导致缺陷减少,然而,低于临界速率的益处减少。通过将粉末床的温度升高到临界温度,可以显著减少缺陷含量。该温度由两种竞争机制决定:在更高温度下较慢的冷却速率与随着接近熔点而增加的无定形相竞争。最后,研究了软夹杂(SiS2)和硬夹杂(SiC)对缺陷结构的影响。与纯金属相比,硬夹杂物导致保留的缺陷结构,而软夹杂物减少缺陷含量。

英文摘要:

Additive manufacturing of a single crystalline metallic column is studied using molecular dynamics simulations. In the model, a melt pool is incrementally added and cooled to a target temperature under isobaric conditions to build a metallic column from bottom up. Common neighbor analysis (CNA) is used to observe the evolution of atomic scale defects during this process. The solidification is seen to proceed along two directions for an added molten layer. The molten layer in contact with the cooler lattice has a fast solidification front that competes with the slower solidification front starting from the top layer. Defect structure formed strongly depends on the speeds of the two competing solidification fronts. Up to a critical layer thickness, defect free single crystals are obtained as the faster solidification front reaches the top of the melt pool before the initiation of the slower front from the top. Slower cooling rates lead to reduction in defects, however, the benefits diminish below a critical rate. Defect content can be significantly reduced by raising the temperature of the powder bed to a critical temperature. This temperature is determined by two competing mechanisms: slower cooling rates at higher temperatures competing against increase in amorphousness as one gets closer to the melting point. Finally, effect of added soft inclusion (SiS2) and a hard inclusion (SiC) on the defect structure is studied. Hard inclusions lead to retained defect structure while soft inclusions reduce defective content compared to a pure metal.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑