arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1810.05029cond-mat.mtrl-sci
收藏

高纯Ar气氛下热处理对电弧PVD c-Al0.66 Ti 0.33 N涂层氧化行为的影响

Effect of thermal treatments in high purity Ar on the oxidation behavior of arc-PVD c-Al0.66Ti0.33N coatings

G. C. Mondragon Rodriguez, Y. Chipatecua-Godoy, N. Camacho, D. G. Espinosa-Arbelaez, J. Gonzalez-Hernandez, J. M. Alvarado-Orozco

摘要:

研究了在高纯Ar(低氧分压)气氛中温度对c-Al 0. 66 Ti 0. 33 N电弧-PVD涂层氧化及晶相演变的影响。研究了氩气射流中的高温摩擦学特性和氧化膜的结合性能。Ar的使用保护涂层免受氧化反应的影响,并允许揭示氮化物氧化过程的细节和路径。c-Al_(0. 66)Ti_(0. 33)N氮化物在Ar气氛中即使在高温下也有轻微的氧化。表面化学评价显示在Ar中700 C后形成非常薄的Al基和Ti基氧化物层。然而,仅在900 ℃后检测到金红石型TiO 2氧化物的开始形成,并且在1000 ℃后通过低角XRD衍射清楚地发现。XPS分析表明,在800 ℃下氧化后,形成了主要由a-Al_2 O_3、g-Al_2 O_3和r-TiO_2组成的极薄氧化层。在900 ℃下观察到的氧化涂层的化学组成的逐渐变化清楚地表明富Al和富Ti的氧氮化物层之间的梯度边界的形成。在1000 ℃以后,至少出现了四个氧化物和氧氮化物层和中间层,另外,c-TiO、c-Al_(0. 54)Ti_(2. 46)O_(0. 28)N_(4.58)、α-Al_2 TiO_5和TiOxNy等过渡氧化物相可能是导致形成高温稳定的金红石和氧化铝相的前驱体。在Ar射流中高温摩擦学后的表面检查表明,由于硬氮化物、氧氮化物和脆性氧化物颗粒的高尺寸颗粒粘附磨损和低尺寸颗粒微犁削,在磨损痕迹和磨损过程中形成拉伸裂纹。在Ar中高温摩擦学后进行的粘附力测试表明,临界载荷下降相关的内聚和粘合剂的损伤在接触点的划痕轨道。

英文摘要:

The effect of temperature in high purity Ar (low oxygen partial pressure) on the oxidation and crystal phase evolution of c-Al0.66Ti0.33N arc-PVD coatings was investigated. High temperature tribology in Ar jet and adhesion behavior of the oxidized coating were addressed. The use of Ar protects the coating from the oxidation reactions and allowed to shed light into the details and paths of the nitride oxidation process. The c-Al0.66Ti0.33N nitrides were slightly oxidized in Ar even at high temperature. The surface chemistry evaluation shows very thin Al- and Ti-based oxide layers formation after 700C in Ar. However, the onset formation of the rutile TiO2 oxide was detected only after 900C and was clearly found by low-angle XRD diffraction after 1000C. XPS analysis of the oxidized samples at 800C indicated the formation of extremely thin layers mainly composed of mixed oxides a-Al2O3 g-Al2O3 and r-TiO2. Gradual changes in the chemical composition of the oxidized coatings observed at 900C clearly demonstrate the formation of gradient boundaries between Al-rich and Ti-rich oxy-nitride layers. After 1000C at least four oxides and oxi-nitrides layers and interlayers were found. Additionally, it is suspected that the transition oxide phases such as c-TiO, c-Al0.54Ti2.46O0.28N4.58, alpha-Al2TiO5 and TiOxNy might be precursors leading to the formation of thermodynamically stable rutile and alumina phases. Surface inspection after high temperature tribology in Ar jet showed formation of tensile cracks in the wear tracks and wear processes due to high size particle adhesion-abrasion and low size particle micro-ploughing of hard nitrides, oxi-nitrides and brittle oxide particles. Adhesion tests performed after high temperature tribology in Ar showed critical load decrease related to cohesive and adhesive damages at the contact point of the scratch track.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑