梯度偏压对arc-PVD CrN薄膜微观结构的影响及其电化学和力学行为响应
Effect of Graded Bias Voltage on the Microstructure of arc-PVD CrN Films and its Response in Electrochemical & Mechanical Behavior
摘要:
研究了梯度偏压和恒定偏压(-40 V、-80 V和-40/60/80 V)对电弧PVD沉积CrN薄膜晶粒尺寸和表面缺陷的影响。使用电化学阻抗谱(EIS)和动电位曲线(塔菲尔)和机械性能评价的仪器化纳米压痕和划痕测试的耐腐蚀性进行了评估与显微结构的变化。结果发现,由于存在缺陷(即开放空隙、液滴),偏压变化会影响腐蚀行为,这也会影响失效机制并增加spectrum。由于CrN涂层的致密微观结构,高偏压(~ 80 V)增加了纳米硬度和弹性模量。
英文摘要:
The effect of graded or constant bias voltages (-40 V, -80 V and -40/60/80 V) on size grain and surface defects of arc PVD deposited CrN films was investigated. Corrosion resistance evaluated using electrochemical impedance spectroscopy (EIS) and potentiodynamic curves (Tafel) and the mechanical behavior evaluated by means of instrumented nanoindentation and scratch testing was correlated with the microstructural changes. It was found that the bias voltage variation affects corrosion behavior due to the presence of defects (i.e. open voids, droplets) which also affects the failure mechanisms and increasing spallation. High bias voltage (-80 V) increases nano-hardness and the elastic modulus due to the dense microstructure of the CrN coating.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。