Ti-Al-Ta-N涂层抗高温氧化性能的成因

Origin of High Temperature Oxidation Resistance of Ti-Al-Ta-N Coatings

R. Hollerweger, H. Riedl, J. Paulitsch, M. Arndt, R. Rachbauer, P. Polcik, S. Primig, P. H. Mayrhofer

摘要:

已经证明,用Ta合金化Ti-Al-N涂层可以提高其硬度、热稳定性和抗氧化性。然而,特别是对于电弧蒸发Ti-Al-Ta-N涂层,只有有限的信息的元素对各种性能的详细影响是可用的。因此,我们开发了具有不同Al(x = 0.50 - 0.65)和Ta(y = 0.00 - 0.15)含量的电弧蒸发Ti_(1-x-y)Al_xTayN涂层。虽然我们的涂层在惰性He气氛中退火过程中的热稳定性随着Ta含量的增加而增加,但在氧化过程中对于特定的Ta-Al比率获得了最佳结果。单相立方相Ti0.32Al0.60Ta0.08N在950 °C的合成空气中5小时后仅产生约5%的质量增益,而Ti0.35Al0.65N在15分钟后完全氧化。这部分是基于在规定的Ta-Al含量下抑制了金红石和直接金红石TiO 2的形成。因此,锐钛矿到金红石的转变,通常观察到的Ti 1-xAlxN,是不存在的。这减少了氧化皮内,特别是在氮化物-氧化物界面处的孔和裂纹的产生,导致形成保护性的金红石和金红石基氧化皮。这也反映在保护性氧化皮形成的活化能从Ti0.35Al0.65N的232 kJ/mol显著降低到Ti0.32Al0.60Ta0.08N的14.5 kJ/mol。根据我们的研究结果,我们可以得出结论,特别是相变内的氧化物规模需要加以抑制,因为连接的体积变化导致裂纹和孔隙的形成。

英文摘要:

Alloying Ti-Al-N coatings with Ta has proven to enhance their hardness, thermal stability, and oxidation resistance. However, especially for arc-evaporated Ti-Al-Ta-N coatings only limited information on the detailed influence of the elements on various properties is available. Therefore, we have developed arc-evaporated Ti1-x-yAlxTayN coatings with various Al (x = 0.50 - 0.65) and Ta (y = 0.00 - 0.15) contents. While the thermal stability of our coatings during annealing in inert He atmosphere increases with increasing Ta content, best results are obtained for specific Ta-Al ratios during oxidation. Single phase cubic Ti0.32Al0.60Ta0.08N yields a mass-gain of only ~5 % after 5 h at 950 °C in synthetic air, whereas Ti0.35Al0.65N is completely oxidized after 15 min. This is in part based on the suppressed anatase and direct rutile TiO2 formation at a defined Ta-Al content. Consequently, the anatase-to-rutile transformation, generally observed for Ti1-xAlxN, is absent. This reduces the generation of pores and cracks within the oxide scale and especially at the nitride-oxide interface, leading to the formation of a protective rutile and corundum based oxide scale. This is also reflected in the pronounced decrease in activation energy for the protective scale formation from 232 kJ/mol for Ti0.35Al0.65N down to 14.5 kJ/mol for Ti0.32Al0.60Ta0.08N. Based on our results we can conclude that especially phase transformations within the oxide scale need to be suppressed, as the connected volume changes lead to the formation of cracks and pores.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑