W. Paschinger, P. F. Rogl, G. Rogl, A. Grytsiv, E. Bauer, H. Michor, Ch. Eisenmenger-Sitter, E. Royanian, P. R. Heinrich, M. Zehetbauer, J. Horky, S. Puchegger,… 展开作者
W. Paschinger, P. F. Rogl, G. Rogl, A. Grytsiv, E. Bauer, H. Michor, Ch. Eisenmenger-Sitter, E. Royanian, P. R. Heinrich, M. Zehetbauer, J. Horky, S. Puchegger, M. Reinecker, G. Giester, P. Broz, A. Bismarck
采用电弧熔炼法制备了新型填充方钴矿EpyNi_4Sb_(12-x)Sn_x(Ep = Ba和La),并在250 ℃、350 ℃和450 ℃下退火30天。Ba和La填充的方钴矿分别实现了y = 0.93和y = 0.65的最大填充水平。采用具有组成Ni4Sb8.2Sn3.8、Ba0.42Ni4Sb8.2Sn3.8和Ba0.92Ni4Sb6.7Sn5.3的单相样品来测量物理性质,即温度依赖的电阻率、塞贝克系数和热导率。电阻率数据显示了从金属到半导体行为的交叉。从作为温度函数的塞贝克系数数据中的最大值提取相应的间隙宽度。温度依赖的单晶X射线结构分析(在100 K,200 K和300 K)揭示了热膨胀系数,爱因斯坦和德拜温度为两个选定的样品Ba 0.73 Ni 4Sb 8.1 Sn 3.9和Ba 0.95 Ni 4Sb 6.1 Sn 5.9。这些数据与比热测量的德拜温度(4.4 K < T < 200 K)相当。测量并评价了几种机械性能。热膨胀系数分别为11.8.10-6 K-1(Ni4Sb8.2Sn3.8)和13.8.10-6 K-1(Ba0.92Ni4Sb6.7Sn5.3)。室温维氏硬度值(高达24.5 mN的负载)在2.6 GPa至4.7 GPa的范围内变化。通过高压扭转(HPT)的剧烈塑性形变(SPD)被用于引入纳米结构化。HPT前后的物理性能进行了比较,显示对材料的热电行为没有显着影响。
英文摘要:
Novel filled skutterudites EpyNi4Sb12-xSnx (Ep = Ba and La) have been prepared by arc melting followed by annealing at 250C, 350C and 450C up to 30 days in sealed quartz vials. A maximum filling level of y = 0.93 and y = 0.65 was achieved for the Ba and La filled skutterudite, respectively. Single-phase samples with the composition Ni4Sb8.2Sn3.8, Ba0.42Ni4Sb8.2Sn3.8 and Ba0.92Ni4Sb6.7Sn5.3 were employed for measurements of the physical properties i.e. temperature dependent electrical resistivity, Seebeck coefficient and thermal conductivity.
Resistivity data showed a crossover from metallic to semiconducting behaviour. The corresponding gap width was extracted from maxima in the Seebeck coefficient data as a function of temperature. Temperature dependent single crystal X-ray structure analyses (at 100 K, 200 K and 300 K) revealed the thermal expansion coefficients, Einstein and Debye temperatures for two selected samples Ba0.73Ni4Sb8.1Sn3.9 and Ba0.95Ni4Sb6.1Sn5.9. These data compare well with Debye temperatures from measurements of specific heat (4.4 K < T < 200 K).
Several mechanical properties were measured and evaluated. Thermal expansion coefficients are 11.8.10-6 K-1 for Ni4Sb8.2Sn3.8 to 13.8.10-6 K-1 for Ba0.92Ni4Sb6.7Sn5.3. Room temperature Vicker's hardness values (up to a load of 24.5 mN) vary within the range of 2.6 GPa to 4.7 GPa. Severe plastic deformation (SPD) via high-pressure torsion (HPT) was used to introduce nanostructuring. Physical properties before and after HPT were compared, showing no significant effect on the material's thermoelectric behaviour.
Strong impact of grain boundaries on the thermoelectric properties of non-equilibrium synthesized p-type Ce1.05Fe4Sb12.04 filled skutterudites with nanostructure
Negative Differential Resistivity and Positive Temperature Coefficient of Resistivity effect in the diffusion limited current of ferroelectric thin film capacitors
Saturation and negative temperature coefficient of electrical resistivity in liquid iron-sulfur alloys at high densities from first principles calculations
Linear thermal expansion coefficient (at temperatures from 130 to 800 K) of borosilicate glasses applicable for coupling with silicon in microelectronics
The direct relation between the coefficient of the low temperature resistivity T^2 term and the superconducting transition temperature Tc
在超导转变温度Tc以上的几种超导体中,电阻率的形式为ρ = AT ^2。我们表明,存在一个经验关系Tc和A时,都与外部参数,如压力。样品的电阻越大,Tc越高。朗道理论表明,这是费米液体的一个普遍特征,因为ρ是由限制在Tc凝聚的对的散射决定的。我们发展了一种方法,可以确定的耦合常数λ,这是验证时,用于超流3He的输运性质。