脉冲laser低温沉积高性能FeSe0. 5 Te 0. 5薄膜

High performance FeSe0.5Te0.5 thin films grown at low temperature by pulsed laser deposition

Pusheng Yuan, Zhongtang Xu, Haitao Zhang, Dongliang Wang, Yanwei Ma, Ming Zhang, Jianqi Li

摘要:

采用脉冲激光沉积法在CaF_2(001)衬底上低温(300°C)生长了高质量的FeSe_(0.5)Te_(0.5)(FST)薄膜。薄膜在4.2 K下的输运J_c在自场下为1.36 MA/cm ~ 2,在9 T下为0.97 MA/cm ~ 2,表明很弱的场依赖性。FST薄膜的Jc(γ= Jc(H//ab)/Jc(H//c))在9 T下接近各向同性,最低可达1.09。此外,由于生长温度低和激光重复频率低,在薄膜和衬底之间没有明显的非晶界面层,而在许多其他工作中,反应层的厚度约为5 nm。透射电子显微镜的证据表明,一些横向尺寸< 5 nm x 20 nm的晶格似乎受到干扰。这些位置缺陷被认为是导致超导性接近各向同性的原因。

英文摘要:

We report on fully epitaxial FeSe0.5Te0.5 (FST) thin films with high-quality grown on CaF2 (00l) substrate at a low temperature of 300°C by pulsed laser deposition. The transport Jc of thin films is up to 1.36 MA/cm2 in self-field and 0.97 MA/cm2 in 9 T at 4.2 K, indicating very weak field dependence. A nearly isotropy of Jc (γ= Jc(H//ab)/Jc(H//c) as low as 1.09 at 9 T is achieved in the FST thin films. Moreover, no clear amorphous interfacial layer presents between the film and the substrate probably ascribing to low temperature and low laser repetition rate grown, while the thickness of reaction layer is approximate 5 nm in many other works. The evidences of transmission electron microscopy show some lattices with lateral size of < 5 nm x 20 nm seem to be disturbed. Those location defects are thought to be responsible for nearly isotropic behavior of superconductivity.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑