arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1401.4916physics.optics
收藏

高反射Si/SiO $_2$涂层叠层在1550 nm处的光吸收测量

Optical Absorption Measurement at 1550 nm on a Highly-Reflective Si/SiO$_2$ Coating Stack

Jessica Steinlechner, Alexander Khalaidovski, Roman Schnabel

摘要:

未来的激光干涉引力波探测器(GWD)将可能采用晶体硅的测试质量镜和$1550\,\rm{nm}$的激光波长,这对应于硅带隙以下的光子能量。硅也可能是一种有吸引力的高折射率材料的介质镜涂层。然而,已经发现非晶硅(a-Si)膜在$1550\,\rm{nm}$处比晶体硅(c-Si)明显更有吸收性。在这里,我们调查的光吸收的Si/SiO $_2$电介质涂层与离子镀技术生产。离子镀技术不同于标准的现有技术的离子束溅射技术,因为它使用约250 $^\circ$ C的较高处理温度、较高粒子能量,并且通常导致沉积膜的较高折射率。我们的涂层叠层被制造用于在$1550\,\rm{nm}$下对s偏振光的$R=99.95\,\%$反射率和用于44 $^\circ$的入射角。利用光热自相位调制技术测量了薄膜在s偏振和p偏振方向的吸收。我们获得了$α^{\rm coat}_{s}=(1035 \pm 42)\,\rm{ppm}$和$α^{\rm coat}_{p}=(1428 \pm 97)\,\rm{ppm}$。这些结果对应于低于a-Si的文献值的吸收系数,a-Si的文献值从$100\,\rm{/cm}$变化到$2000\,\rm{/cm}$。然而,它仍然比c-Si的预期高几个数量级,因此对于GWD应用仍然太高。

英文摘要:

Future laser-interferometric gravitational wave detectors (GWDs) will potentially employ test mass mirrors from crystalline silicon and a laser wavelength of $1550\,\rm{nm}$, which corresponds to a photon energy below the silicon bandgap. Silicon might also be an attractive high-refractive index material for the dielectric mirror coatings. Films of amorphous silicon (a-Si), however, have been found to be significantly more absorptive at $1550\,\rm{nm}$ than crystalline silicon (c-Si). Here, we investigate the optical absorption of a Si/SiO$_2$ dielectric coating produced with the ion plating technique. The ion plating technique is distinct from the standard state-of-the-art ion beam sputtering technique since it uses a higher processing temperature of about 250$^\circ$C, higher particle energies, and generally results in higher refractive indices of the deposited films. Our coating stack was fabricated for a reflectivity of $R=99.95\,\%$ for s-polarized light at $1550\,\rm{nm}$ and for an angle of incidence of 44$^\circ$. We used the photothermal self-phase modulation technique to measure the coating absorption in s-polarization and p-polarization. We obtained $α^{\rm coat}_{s}=(1035 \pm 42)\,\rm{ppm}$ and $α^{\rm coat}_{p}=(1428 \pm 97)\,\rm{ppm}$. These results correspond to an absorption coefficient which is lower than literature values for a-Si which vary from $100\,\rm{/cm}$ up to $2000\,\rm{/cm}$. It is, however, still orders of magnitude higher than expected for c-Si and thus still too high for GWD applications.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑