高精细度钽(V)氧化物反射镜涂层中防止和逆转钽引起的光学损耗
Preventing and Reversing Vacuum-Induced Optical Losses in High-Finesse Tantalum (V) Oxide Mirror Coatings
摘要:
研究了具有SiO-$_2$-Ta $_{2}$ O $_{5}$介质叠层反射膜的高精细光学腔的真空诱导退化,并提出了保护这些反射膜和恢复其初始品质因数的方法。对于反射率集中在370 nm和422 nm的单独涂层,如果表面层涂层由Ta $_{2}$ O $_{5}$制成,则会出现真空诱导的光学损耗的连续增加,而如果表面层涂层由SiO $_2$制成,则不会出现这种情况。在大气压下用氧气填充真空室可以逆转所引起的光学损耗,并且通过422 nm的连续激光照射可以强烈地加速恢复速率。降解和恢复过程都强烈依赖于温度。我们发现,1 nm厚的SiO $_2$层钝化Ta $_{2}$ O $_{5}$表面层足以降低降解速率超过10倍,强烈支持表面氧耗尽作为主要降解机制。
英文摘要:
We study the vacuum-induced degradation of high-finesse optical cavities with mirror coatings composed of SiO$_2$-Ta$_{2}$O$_{5}$ dielectric stacks, and present methods to protect these coatings and to recover their initial quality factor. For separate coatings with reflectivities centered at 370 nm and 422 nm, a vacuum-induced continuous increase in optical loss occurs if the surface-layer coating is made of Ta$_{2}$O$_{5}$, while it does not occur if it is made of SiO$_2$. The incurred optical loss can be reversed by filling the vacuum chamber with oxygen at atmospheric pressure, and the recovery rate can be strongly accelerated by continuous laser illumination at 422 nm. Both the degradation and the recovery processes depend strongly on temperature. We find that a 1 nm-thick layer of SiO$_2$ passivating the Ta$_{2}$O$_{5}$ surface layer is sufficient to reduce the degradation rate by more than a factor of 10, strongly supporting surface oxygen depletion as the primary degradation mechanism.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。