arXiv 1208.2074cond-mat.mtrl-sci
收藏

ZnO衬底上生长的MgxZn1-xO薄膜中Mg浓度的精确校准

Precise calibration of Mg concentration in MgxZn1-xO thin films grown on ZnO substrates

Y. Kozuka, J. Falson, Y. Segawa, T. Makino, A. Tsukazaki, M. Kawasaki

摘要:

近年来,MgxZn 1-xO薄膜的生长技术得到了快速发展,使得这种材料能够广泛地应用于光学和电学应用。在设计结构和优化器件性能时,合金中Mg含量的可控和精确确定至关重要。在这项研究中,我们已经建立了实验室为基础的方法来确定镁含量的MgxZn 1-xO薄膜生长在ZnO衬底上,范围从x ~ 0.4的溶解度极限x < 0.01的稀释极限。对于Mg含量的绝对测定,卢瑟福背散射光谱用于高于x = 0.14的高Mg区域,而二次离子质谱用于量化低Mg含量。作为一种基于实验室的方法来确定镁含量,c轴长度是通过X射线衍射测量的,并且与镁含量有很好的关联。该插值使得能够将Mg含量测定为x = 0.023,其中来自ZnO衬底的峰与标准实验室设备中的MgxZn 1-xO峰重叠,从而能够进行定量测定。在稀释的Mg含量低于x = 0.023时,通过光致发光测量的MgxZn 1-xO薄膜的局域激子峰能量被发现显示出线性的Mg含量依赖性,这是很好地解决从ZnO衬底的自由激子峰下降到x = 0.0043。我们的研究结果表明,X射线衍射和光致发光相结合的方法来确定镁含量在一个宽的镁范围从x = 0.004至0.40在实验室环境中是适当的。

英文摘要:

The growth techniques for MgxZn1-xO thin films have advanced at a rapid pace in recent years, enabling the application of this material to a wide range of optical and electrical applications. In designing structures and optimizing device performances, it is crucial that the Mg content of the alloy be controllable and precisely determined. In this study, we have established laboratory-based methods to determine the Mg content of MgxZn1-xO thin films grown on ZnO substrates, ranging from the solubility limit of x ~ 0.4 to the dilute limit of x < 0.01. For the absolute determination of Mg content, Rutherford backscattering spectroscopy is used for the high Mg region above x = 0.14, while secondary ion mass spectroscopy is employed to quantify low Mg content. As a lab-based method to determine the Mg content, c-axis length is measured by X-ray diffraction and is well associated with Mg content. The interpolation enables the determination of Mg content to x = 0.023, where the peak from the ZnO substrate overlaps the MgxZn1-xO peak in standard laboratory equipment, and thus quantitative determination. At dilute Mg contents below x = 0.023, the localized exciton peak energy of the MgxZn1-xO films as measured by photoluminescence is found to show a linear Mg content dependence, which is well resolved from the free exciton peak of ZnO substrate down to x = 0.0043. Our results demonstrate that X-ray diffraction and photoluminescence in combination are appropriate methods to determine Mg content in a wide Mg range from x = 0.004 to 0.40 in a laboratory environment.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑