arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2605.31395cond-mat.mtrl-sci
收藏

利用中子衍射直接观察CoCrNi合金中的化学短程有序

Direct Observation of Chemical Short-Range Order in CoCrNi Alloy Using Neutron Diffraction

Federal University of São Carlos (UFSCar)(圣卡洛斯联邦大学);Université Paris-Saclay, CEA(巴黎萨克雷大学,法国原子能和替代能源委员会);University of Sheffield(谢菲尔德大学);Massachusetts Institute of Technology(麻省理工学院);AF Research Laboratory, Materials and Manufacturing Directorate, Wright-Patterson AFB(空军研究实验室材料制造局赖特-帕特森空军基地)
Vinícius P. Bacurau, Camilo Salvador, Guilherme C. Stumpfa, Angelo F. Andreolli, Caroline B. Stocoa, Eric M. Mazzer, Lewis Owen, Yifan Cao, Rodrigo Freitas, Dan… 展开作者

Vinícius P. Bacurau, Camilo Salvador, Guilherme C. Stumpfa, Angelo F. Andreolli, Caroline B. Stocoa, Eric M. Mazzer, Lewis Owen, Yifan Cao, Rodrigo Freitas, Daniel Miracle, Francisco G. Coury

AI总结:

通过中子衍射实验证实了CoCrNi合金中存在化学短程有序,并利用原子模拟和散射分析揭示了其结构特征与形成机制。

摘要:

本研究提供了通过中子衍射识别的等原子CoCrNi合金中化学短程有序(CSRO)的实验证据。该现象表现为在Q = 1.85 A-1处出现明显的漫散射峰,其强度在热力学有利于CSRO发展的条件下增加,例如在748 K下长时间时效(100小时和240小时)或在稍高温度(798 K)下短时间时效(24小时)。通过积分漫散射强度测量有序度,发现气雾化样品(即CSRO最少的样品)仍显示出约70%的CSRO水平,该水平是在748 K下时效240小时的样品(即本研究中产生的CSRO最多的样品)中观察到的。预测性原子模拟再现了漫散射峰的存在和位置,而二维快速傅里叶变换(FT-2D)分析表明,<001>晶带轴内的(1 1/2 0)反射源于与D022、Pt2Mo和D1a构型相关的某些结构投影。互补的小角中子散射(SANS)测量识别出富镍的盘状区域,半径约为11 Å,厚度约为1 Å,与纳米级CSRO的特征长度尺度一致。这些发现表明,CSRO是CoCrNi体系固有的且能量上有利的特征,即使在快速凝固下也能保持稳定,并通过低温时效进一步增强。中子衍射与原子模拟的结合使用为探测多主元合金(MPEAs)中的局域有序现象提供了框架。

英文摘要:

This study provides experimental evidence of chemical short-range order (CSRO) in the equiatomic CoCrNi alloy, identified through neutron diffraction. The phenomenon manifests as a distinct diffuse peak at Q = 1.85 A-1, the intensity increases under thermodynamically favorable conditions for CSRO development such as prolonged aging (100 h and 240 h) at 748 K or shorter aging (24 h) at slightly higher temperature (798 K). The degree of ordering was measured by integrating the diffuse scattering intensity, revealing that the gas-atomized sample, i.e. the sample with the least amount of CSRO, still displays approximately 70% of the CSRO level observed in the sample subsequently aged for 240 h at 748 K, i.e. the sample with the highest amount of CSRO produced in this study. Predictive atomistic simulations reproduced both the presence and position of the diffuse peak, while two-dimensional fast Fourier transform (FT-2D) analyses indicated that reflections at (1 1/2 0) within the <001> zone axis originate from some structural projections associated with like D022, Pt2Mo and D1a motifs. Complementary small-angle neutron scattering (SANS) measurements identified Ni-rich, disk-shaped domains with radii of approximately 11 A and thicknesses of about 1 A, consistent with nanoscale CSRO characteristic length scale. These findings demonstrate that CSRO is an intrinsic and energetically favorable feature of the CoCrNi system, remaining stable even under rapid solidification and further enhanced by low-temperature aging. Combined use of neutron diffraction and atomistic modeling provides a framework for probing local ordering phenomena in multi-principal element alloys (MPEAs).

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑