锗-锡(GeSn)雪崩光电二极管,截止波长达2.7微米用于扩展短波红外检测
Germanium-tin (GeSn) avalanche photodiode with up to 2.7 micro cutoff wavelength for extended SWIR detection
AI总结:
本研究开发了高锡含量的GeSn硅雪崩光电二极管,通过薄Ge缓冲层实现高灵敏度SWIR检测,突破传统工艺限制,实现2.7微米截止波长和高增益。
摘要:
分离吸收电荷倍增的锗锡硅雪崩光电二极管为实现CMOS兼容的高灵敏度SWIR或扩展SWIR检测提供了可行方案,利用Si优异的k因子作为倍增层和GeSn在SWIR或e-SWIR波段的吸收特性。然而,与传统GeSn在Si上生长不同,GeSn在Si上的APD设计需要较薄的Ge缓冲层以限制背景p掺杂缓冲层中的电场下降,并高效传输光载流子从GeSn吸收层到Si倍增层,因此高Sn含量APD在e-SWIR覆盖方面极具挑战性。本文实验展示了GeSn在Si上的APD,含锡量达12.7%,单片生长于Si基底上,中间有122 nm厚的Ge缓冲层,远比广泛使用的700-900 nm厚的Ge缓冲层薄。较薄的Ge缓冲层促进了GeSn吸收层的松弛,有利于锡的掺杂,从而实现高于8%锡含量的目标。与先前工作相比,器件检测范围显著提高,截止波长在300 K时增加至2.7微米,同时在77 K时1.55微米处的高雪崩增益达21,在2微米处达52,SWIR或e-SWIR范围内具有良好的响应率,最高达1.45 AW-1在1.55微米和0.66 AW-1在2微米。
英文摘要:
Separate absorption charge multiplication germanium tin on silicon avalanche photodiode offers a viable solution to achieve CMOS compatible, high sensitivity detection technology in SWIR or extended SWIR range, leveraging the excellent k-factor of Si as multiplication layer and SWIR or e-SWIR band absorption of GeSn. However, unlike well-established growth of GeSn on Si with thick Ge buffer in-between to reduce threading dislocation density due to lattice mismatch, GeSn on Si APD design requires relatively thin Ge buffer to limit electric field drop through the background p-doped buffer and efficiently transporting photocarrier from GeSn absorber to Si multiplication layer, therefore making growth of high Sn content APD for e-SWIR coverage very challenging. In this work, we experimentally demonstrate GeSn on Si APD up to 12.7 percent Sn, monolithically grown on Si substrate with 122-nm-thick Ge buffer in between, which is considerably thinner than widely used 700-900 nm thick Ge buffer. Stronger relaxation of GeSn absorber via thin Ge buffer favors Sn incorporation, leading to higher Sn content than the nominal target of 8 percent Sn. Device detection range is significantly improved compared to previous work - with cutoff wavelength increased up to 2.7 micro at 300 K, in parallel with high avalanche gain at 77 K up to 21 at 1.55 micro and up to 52 at 2 micro, and good responsivity in SWIR or e-SWIR range, up to 1.45 AW-1 at 1.55 micro and 0.66 AW-1 at 2 micro.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。